INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE

To provide an injection molding method for a resin composition containing a PAS resin and a thermoplastic elastomer, the method capable of reducing molding defects and the frequency of mold maintenance.SOLUTION: An injection molding method using an injection unit 100 provided with: a cylinder 2; a s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KANDA TOMOMICHI, WATANABE KAZUHIRO, GIBO SHINYA
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KANDA TOMOMICHI
WATANABE KAZUHIRO
GIBO SHINYA
description To provide an injection molding method for a resin composition containing a PAS resin and a thermoplastic elastomer, the method capable of reducing molding defects and the frequency of mold maintenance.SOLUTION: An injection molding method using an injection unit 100 provided with: a cylinder 2; a screw 3 arranged in the cylinder 2 and capable of compressing and melting, measuring, and injecting a resin supplied from a root portion; and a vent port 20 arranged midway in a longitudinal direction of the cylinder 3 comprises: a supplying step for supplying a resin composition containing a PAS resin and a thermoplastic elastomer to the cylinder 2 of the injection unit 100; a plasticizing step for keeping the cylinder 2 at 290°C or more to plasticize the resin composition in the cylinder 2; an injection step for injecting the resin composition from the cylinder 2 with the screw 3; an exhausting step for exhausting a component vaporized from the resin composition in the plasticizing step or the injection step from the vent port 20; and a molding step for molding the resin composition injected in the injection step using a mold 9.SELECTED DRAWING: Figure 1 【課題】PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物の射出成形方法において、成形不良や金型のメンテナンス頻度を低減することのできる射出成形方法を提供する。【解決手段】シリンダ2とシリンダ2内に配置され、根本部より供給される樹脂を圧縮溶融、計量及び射出できるスクリュー3とシリンダ3の長手方向の途中に配置されたベント口20とを備えた射出ユニット100を用いた射出成形方法において、PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物を射出ユニット100のシリンダ2に供給する供給工程と、シリンダ2を290℃以上に保持してシリンダ2中で樹脂組成物を可塑化する可塑化工程と、樹脂組成物をスクリュー3でシリンダ2から射出する射出工程と、可塑化工程又は射出工程において樹脂組成物から揮発した成分をベント口20から排出する排出工程と、射出工程において射出された樹脂組成物を金型9で成形する成形工程とを含む。【選択図】図1
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023163928A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023163928A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023163928A3</originalsourceid><addsrcrecordid>eNrjZMjx9PNydQ7x9PdT8PX3cfH0c1fwdQ3x8HfRUfB19At1c3QOCQ1CiCr4u8HU6Sg4-rngVuQa4uijEOQa7Omn4OzvG-Af7BniysPAmpaYU5zKC6W5GZTcXEOcPXRTC_LjU4sLEpNT81JL4r0CjAyMjA3NjC2NLByNiVIEAFMANw0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE</title><source>esp@cenet</source><creator>KANDA TOMOMICHI ; WATANABE KAZUHIRO ; GIBO SHINYA</creator><creatorcontrib>KANDA TOMOMICHI ; WATANABE KAZUHIRO ; GIBO SHINYA</creatorcontrib><description>To provide an injection molding method for a resin composition containing a PAS resin and a thermoplastic elastomer, the method capable of reducing molding defects and the frequency of mold maintenance.SOLUTION: An injection molding method using an injection unit 100 provided with: a cylinder 2; a screw 3 arranged in the cylinder 2 and capable of compressing and melting, measuring, and injecting a resin supplied from a root portion; and a vent port 20 arranged midway in a longitudinal direction of the cylinder 3 comprises: a supplying step for supplying a resin composition containing a PAS resin and a thermoplastic elastomer to the cylinder 2 of the injection unit 100; a plasticizing step for keeping the cylinder 2 at 290°C or more to plasticize the resin composition in the cylinder 2; an injection step for injecting the resin composition from the cylinder 2 with the screw 3; an exhausting step for exhausting a component vaporized from the resin composition in the plasticizing step or the injection step from the vent port 20; and a molding step for molding the resin composition injected in the injection step using a mold 9.SELECTED DRAWING: Figure 1 【課題】PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物の射出成形方法において、成形不良や金型のメンテナンス頻度を低減することのできる射出成形方法を提供する。【解決手段】シリンダ2とシリンダ2内に配置され、根本部より供給される樹脂を圧縮溶融、計量及び射出できるスクリュー3とシリンダ3の長手方向の途中に配置されたベント口20とを備えた射出ユニット100を用いた射出成形方法において、PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物を射出ユニット100のシリンダ2に供給する供給工程と、シリンダ2を290℃以上に保持してシリンダ2中で樹脂組成物を可塑化する可塑化工程と、樹脂組成物をスクリュー3でシリンダ2から射出する射出工程と、可塑化工程又は射出工程において樹脂組成物から揮発した成分をベント口20から排出する排出工程と、射出工程において射出された樹脂組成物を金型9で成形する成形工程とを含む。【選択図】図1</description><language>eng ; jpn</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231110&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023163928A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231110&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023163928A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KANDA TOMOMICHI</creatorcontrib><creatorcontrib>WATANABE KAZUHIRO</creatorcontrib><creatorcontrib>GIBO SHINYA</creatorcontrib><title>INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE</title><description>To provide an injection molding method for a resin composition containing a PAS resin and a thermoplastic elastomer, the method capable of reducing molding defects and the frequency of mold maintenance.SOLUTION: An injection molding method using an injection unit 100 provided with: a cylinder 2; a screw 3 arranged in the cylinder 2 and capable of compressing and melting, measuring, and injecting a resin supplied from a root portion; and a vent port 20 arranged midway in a longitudinal direction of the cylinder 3 comprises: a supplying step for supplying a resin composition containing a PAS resin and a thermoplastic elastomer to the cylinder 2 of the injection unit 100; a plasticizing step for keeping the cylinder 2 at 290°C or more to plasticize the resin composition in the cylinder 2; an injection step for injecting the resin composition from the cylinder 2 with the screw 3; an exhausting step for exhausting a component vaporized from the resin composition in the plasticizing step or the injection step from the vent port 20; and a molding step for molding the resin composition injected in the injection step using a mold 9.SELECTED DRAWING: Figure 1 【課題】PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物の射出成形方法において、成形不良や金型のメンテナンス頻度を低減することのできる射出成形方法を提供する。【解決手段】シリンダ2とシリンダ2内に配置され、根本部より供給される樹脂を圧縮溶融、計量及び射出できるスクリュー3とシリンダ3の長手方向の途中に配置されたベント口20とを備えた射出ユニット100を用いた射出成形方法において、PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物を射出ユニット100のシリンダ2に供給する供給工程と、シリンダ2を290℃以上に保持してシリンダ2中で樹脂組成物を可塑化する可塑化工程と、樹脂組成物をスクリュー3でシリンダ2から射出する射出工程と、可塑化工程又は射出工程において樹脂組成物から揮発した成分をベント口20から排出する排出工程と、射出工程において射出された樹脂組成物を金型9で成形する成形工程とを含む。【選択図】図1</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZMjx9PNydQ7x9PdT8PX3cfH0c1fwdQ3x8HfRUfB19At1c3QOCQ1CiCr4u8HU6Sg4-rngVuQa4uijEOQa7Omn4OzvG-Af7BniysPAmpaYU5zKC6W5GZTcXEOcPXRTC_LjU4sLEpNT81JL4r0CjAyMjA3NjC2NLByNiVIEAFMANw0</recordid><startdate>20231110</startdate><enddate>20231110</enddate><creator>KANDA TOMOMICHI</creator><creator>WATANABE KAZUHIRO</creator><creator>GIBO SHINYA</creator><scope>EVB</scope></search><sort><creationdate>20231110</creationdate><title>INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE</title><author>KANDA TOMOMICHI ; WATANABE KAZUHIRO ; GIBO SHINYA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023163928A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>KANDA TOMOMICHI</creatorcontrib><creatorcontrib>WATANABE KAZUHIRO</creatorcontrib><creatorcontrib>GIBO SHINYA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KANDA TOMOMICHI</au><au>WATANABE KAZUHIRO</au><au>GIBO SHINYA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE</title><date>2023-11-10</date><risdate>2023</risdate><abstract>To provide an injection molding method for a resin composition containing a PAS resin and a thermoplastic elastomer, the method capable of reducing molding defects and the frequency of mold maintenance.SOLUTION: An injection molding method using an injection unit 100 provided with: a cylinder 2; a screw 3 arranged in the cylinder 2 and capable of compressing and melting, measuring, and injecting a resin supplied from a root portion; and a vent port 20 arranged midway in a longitudinal direction of the cylinder 3 comprises: a supplying step for supplying a resin composition containing a PAS resin and a thermoplastic elastomer to the cylinder 2 of the injection unit 100; a plasticizing step for keeping the cylinder 2 at 290°C or more to plasticize the resin composition in the cylinder 2; an injection step for injecting the resin composition from the cylinder 2 with the screw 3; an exhausting step for exhausting a component vaporized from the resin composition in the plasticizing step or the injection step from the vent port 20; and a molding step for molding the resin composition injected in the injection step using a mold 9.SELECTED DRAWING: Figure 1 【課題】PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物の射出成形方法において、成形不良や金型のメンテナンス頻度を低減することのできる射出成形方法を提供する。【解決手段】シリンダ2とシリンダ2内に配置され、根本部より供給される樹脂を圧縮溶融、計量及び射出できるスクリュー3とシリンダ3の長手方向の途中に配置されたベント口20とを備えた射出ユニット100を用いた射出成形方法において、PAS樹脂と熱可塑性エラストマーとを含む樹脂組成物を射出ユニット100のシリンダ2に供給する供給工程と、シリンダ2を290℃以上に保持してシリンダ2中で樹脂組成物を可塑化する可塑化工程と、樹脂組成物をスクリュー3でシリンダ2から射出する射出工程と、可塑化工程又は射出工程において樹脂組成物から揮発した成分をベント口20から排出する排出工程と、射出工程において射出された樹脂組成物を金型9で成形する成形工程とを含む。【選択図】図1</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2023163928A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
LAYERED PRODUCTS
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title INJECTION MOLDING METHOD, MANUFACTURING METHOD OF MOLDING, AND MANUFACTURING METHOD OF METAL RESIN COMPOSITE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T00%3A25%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KANDA%20TOMOMICHI&rft.date=2023-11-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023163928A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true