MOLD STEEL AND METAL MOLD

To provide a mold steel excellent in wear resistance and thermal shock resistance, and a metal mold.SOLUTION: A mold steel comprises, in mass%, 0.55%≤C≤0.70%, 0.30%≤Si≤0.60%, 0.55%≤Mn≤1.2%, 5.7%≤Cr≤6.9%, 1.2%≤Mo+1/2W≤1.6%, 0.55%≤V≤0.79%, and 0.005%≤N≤0.1%, with the remainder being Fe and unavoidable...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NEMOTO TAKESHI, UMEMORI NAOKI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NEMOTO TAKESHI
UMEMORI NAOKI
description To provide a mold steel excellent in wear resistance and thermal shock resistance, and a metal mold.SOLUTION: A mold steel comprises, in mass%, 0.55%≤C≤0.70%, 0.30%≤Si≤0.60%, 0.55%≤Mn≤1.2%, 5.7%≤Cr≤6.9%, 1.2%≤Mo+1/2W≤1.6%, 0.55%≤V≤0.79%, and 0.005%≤N≤0.1%, with the remainder being Fe and unavoidable impurities, a content of Al, Ni, S, and Cu as inevitable impurities is, in mass%, Al≤0.020%, Ni≤0.20%, S≤0.0015%, and Cu≤0.10%, a value of P1 determined by the following formula (1) is P1≥24, and the value of P2 determined by the following formula (2) is 4.9≤P2≤7.3. P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1) P2=7.4V+15.8N+38.6Al (2).SELECTED DRAWING: Figure 1 【課題】耐摩耗性と耐熱衝撃性に優れた金型用鋼、および金型を提供する。【解決手段】質量%で、0.55%≦C≦0.70%、0.30%≦Si≦0.60%、0.55%≦Mn≦1.2%、5.7%≦Cr≦6.9%、1.2%≦Mo+1/2W≦1.6%、0.55%≦V≦0.79%、および0.005%≦N≦0.1%を含有し、残部がFeおよび不可避的不純物よりなり、不可避的不純物としてのAl、Ni、S、Cuの含有量が、質量%で、Al≦0.020%、Ni≦0.20%、S≦0.0015%、およびCu≦0.10%であり、下記の式(1)によって求められるP1の値が、P1≧24であり、下記の式(2)によって求められるP2の値が、4.9≦P2≦7.3である、金型用鋼とする。P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1)P2=7.4V+15.8N+38.6Al (2)【選択図】図1
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023122766A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023122766A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023122766A3</originalsourceid><addsrcrecordid>eNrjZJD09fdxUQgOcXX1UXD0c1HwdQ1x9FEACfIwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDI2NDIyNzMzNHY6IUAQAsoyAN</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MOLD STEEL AND METAL MOLD</title><source>esp@cenet</source><creator>NEMOTO TAKESHI ; UMEMORI NAOKI</creator><creatorcontrib>NEMOTO TAKESHI ; UMEMORI NAOKI</creatorcontrib><description>To provide a mold steel excellent in wear resistance and thermal shock resistance, and a metal mold.SOLUTION: A mold steel comprises, in mass%, 0.55%≤C≤0.70%, 0.30%≤Si≤0.60%, 0.55%≤Mn≤1.2%, 5.7%≤Cr≤6.9%, 1.2%≤Mo+1/2W≤1.6%, 0.55%≤V≤0.79%, and 0.005%≤N≤0.1%, with the remainder being Fe and unavoidable impurities, a content of Al, Ni, S, and Cu as inevitable impurities is, in mass%, Al≤0.020%, Ni≤0.20%, S≤0.0015%, and Cu≤0.10%, a value of P1 determined by the following formula (1) is P1≥24, and the value of P2 determined by the following formula (2) is 4.9≤P2≤7.3. P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1) P2=7.4V+15.8N+38.6Al (2).SELECTED DRAWING: Figure 1 【課題】耐摩耗性と耐熱衝撃性に優れた金型用鋼、および金型を提供する。【解決手段】質量%で、0.55%≦C≦0.70%、0.30%≦Si≦0.60%、0.55%≦Mn≦1.2%、5.7%≦Cr≦6.9%、1.2%≦Mo+1/2W≦1.6%、0.55%≦V≦0.79%、および0.005%≦N≦0.1%を含有し、残部がFeおよび不可避的不純物よりなり、不可避的不純物としてのAl、Ni、S、Cuの含有量が、質量%で、Al≦0.020%、Ni≦0.20%、S≦0.0015%、およびCu≦0.10%であり、下記の式(1)によって求められるP1の値が、P1≧24であり、下記の式(2)によって求められるP2の値が、4.9≦P2≦7.3である、金型用鋼とする。P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1)P2=7.4V+15.8N+38.6Al (2)【選択図】図1</description><language>eng ; jpn</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230905&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023122766A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230905&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023122766A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NEMOTO TAKESHI</creatorcontrib><creatorcontrib>UMEMORI NAOKI</creatorcontrib><title>MOLD STEEL AND METAL MOLD</title><description>To provide a mold steel excellent in wear resistance and thermal shock resistance, and a metal mold.SOLUTION: A mold steel comprises, in mass%, 0.55%≤C≤0.70%, 0.30%≤Si≤0.60%, 0.55%≤Mn≤1.2%, 5.7%≤Cr≤6.9%, 1.2%≤Mo+1/2W≤1.6%, 0.55%≤V≤0.79%, and 0.005%≤N≤0.1%, with the remainder being Fe and unavoidable impurities, a content of Al, Ni, S, and Cu as inevitable impurities is, in mass%, Al≤0.020%, Ni≤0.20%, S≤0.0015%, and Cu≤0.10%, a value of P1 determined by the following formula (1) is P1≥24, and the value of P2 determined by the following formula (2) is 4.9≤P2≤7.3. P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1) P2=7.4V+15.8N+38.6Al (2).SELECTED DRAWING: Figure 1 【課題】耐摩耗性と耐熱衝撃性に優れた金型用鋼、および金型を提供する。【解決手段】質量%で、0.55%≦C≦0.70%、0.30%≦Si≦0.60%、0.55%≦Mn≦1.2%、5.7%≦Cr≦6.9%、1.2%≦Mo+1/2W≦1.6%、0.55%≦V≦0.79%、および0.005%≦N≦0.1%を含有し、残部がFeおよび不可避的不純物よりなり、不可避的不純物としてのAl、Ni、S、Cuの含有量が、質量%で、Al≦0.020%、Ni≦0.20%、S≦0.0015%、およびCu≦0.10%であり、下記の式(1)によって求められるP1の値が、P1≧24であり、下記の式(2)によって求められるP2の値が、4.9≦P2≦7.3である、金型用鋼とする。P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1)P2=7.4V+15.8N+38.6Al (2)【選択図】図1</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJD09fdxUQgOcXX1UXD0c1HwdQ1x9FEACfIwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDI2NDIyNzMzNHY6IUAQAsoyAN</recordid><startdate>20230905</startdate><enddate>20230905</enddate><creator>NEMOTO TAKESHI</creator><creator>UMEMORI NAOKI</creator><scope>EVB</scope></search><sort><creationdate>20230905</creationdate><title>MOLD STEEL AND METAL MOLD</title><author>NEMOTO TAKESHI ; UMEMORI NAOKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023122766A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>NEMOTO TAKESHI</creatorcontrib><creatorcontrib>UMEMORI NAOKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NEMOTO TAKESHI</au><au>UMEMORI NAOKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MOLD STEEL AND METAL MOLD</title><date>2023-09-05</date><risdate>2023</risdate><abstract>To provide a mold steel excellent in wear resistance and thermal shock resistance, and a metal mold.SOLUTION: A mold steel comprises, in mass%, 0.55%≤C≤0.70%, 0.30%≤Si≤0.60%, 0.55%≤Mn≤1.2%, 5.7%≤Cr≤6.9%, 1.2%≤Mo+1/2W≤1.6%, 0.55%≤V≤0.79%, and 0.005%≤N≤0.1%, with the remainder being Fe and unavoidable impurities, a content of Al, Ni, S, and Cu as inevitable impurities is, in mass%, Al≤0.020%, Ni≤0.20%, S≤0.0015%, and Cu≤0.10%, a value of P1 determined by the following formula (1) is P1≥24, and the value of P2 determined by the following formula (2) is 4.9≤P2≤7.3. P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1) P2=7.4V+15.8N+38.6Al (2).SELECTED DRAWING: Figure 1 【課題】耐摩耗性と耐熱衝撃性に優れた金型用鋼、および金型を提供する。【解決手段】質量%で、0.55%≦C≦0.70%、0.30%≦Si≦0.60%、0.55%≦Mn≦1.2%、5.7%≦Cr≦6.9%、1.2%≦Mo+1/2W≦1.6%、0.55%≦V≦0.79%、および0.005%≦N≦0.1%を含有し、残部がFeおよび不可避的不純物よりなり、不可避的不純物としてのAl、Ni、S、Cuの含有量が、質量%で、Al≦0.020%、Ni≦0.20%、S≦0.0015%、およびCu≦0.10%であり、下記の式(1)によって求められるP1の値が、P1≧24であり、下記の式(2)によって求められるP2の値が、4.9≦P2≦7.3である、金型用鋼とする。P1=45-13.6Si-7.0(Mo+1/2W)-12.9Ni (1)P2=7.4V+15.8N+38.6Al (2)【選択図】図1</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2023122766A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title MOLD STEEL AND METAL MOLD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T18%3A13%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NEMOTO%20TAKESHI&rft.date=2023-09-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023122766A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true