SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME

To provide shaped glass laminates including glass substrates that differ from one another and exhibit a minimal shape mismatch therebetween, where the glass substrates are thinner.SOLUTION: Embodiments of a laminate are disclosed, the laminate comprising: a first curved glass substrate including a f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: MICHELE MARIE-LOUISE FREDHOLM
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MICHELE MARIE-LOUISE FREDHOLM
description To provide shaped glass laminates including glass substrates that differ from one another and exhibit a minimal shape mismatch therebetween, where the glass substrates are thinner.SOLUTION: Embodiments of a laminate are disclosed, the laminate comprising: a first curved glass substrate including a first viscosity (poises) at a temperature of 630°C; a second curved glass substrate including a second viscosity that is greater than the first viscosity at a temperature of 630°C; and an interlayer disposed between the first curved glass substrate and the second curved glass substrate. In one or more embodiments, the first curved glass substrate exhibits a first sag depth that is within 10% of a second sag depth of the second curved glass substrate. In one or more embodiments, the first glass substrate and the second glass substrate exhibit a shape deviation therebetween of about 5 mm or less as measured by an optical three-dimensional scanner, or exhibit minimal optical distortion. Embodiments of vehicles including such laminates and methods for making such laminates are also disclosed.SELECTED DRAWING: Figure 4 【課題】互いに異なり、互いの間に最小限の形状不一致を示すガラス基板を含む成形ガラス積層体であって、より薄いガラス基板を有する積層体を提供する。【解決手段】630℃の温度で第1の粘度(ポアズ)を含む第1の湾曲したガラス基板;630℃の温度で第1の粘度より大きい第2の粘度を含む第2の湾曲したガラス基板;並びに、第1の湾曲したガラス基板と第2の湾曲したガラス基板との間に配置された中間層を備えた積層体の実施形態が開示される。1つ以上の実施形態では、第1の湾曲したガラス基板は、第2の湾曲したガラス基板の第2の垂下深さの10%以内の第1の垂下深さを示す。1つ以上の実施形態では、第1のガラス基板及び第2のガラス基板は、光学三次元スキャナで測定して約5mm以下の形状偏差を示すか、若しくは最小光学歪みを示す。このような積層体を含む車両の実施形態、及びこのような積層体の製造方法についても開示される。【選択図】図4
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023103321A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023103321A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023103321A3</originalsourceid><addsrcrecordid>eNrjZDAP9nAMcHVRcPdxDA5W8HH09fRzDHENVnD0c1HwdQ3x8HcJVnDzDwJhoJS7QoiHq0Kwo68rDwNrWmJOcSovlOZmUHJzDXH20E0tyI9PLS5ITE7NSy2J9wowMjAyNjQwNjYydDQmShEAX0ooKA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME</title><source>esp@cenet</source><creator>MICHELE MARIE-LOUISE FREDHOLM</creator><creatorcontrib>MICHELE MARIE-LOUISE FREDHOLM</creatorcontrib><description>To provide shaped glass laminates including glass substrates that differ from one another and exhibit a minimal shape mismatch therebetween, where the glass substrates are thinner.SOLUTION: Embodiments of a laminate are disclosed, the laminate comprising: a first curved glass substrate including a first viscosity (poises) at a temperature of 630°C; a second curved glass substrate including a second viscosity that is greater than the first viscosity at a temperature of 630°C; and an interlayer disposed between the first curved glass substrate and the second curved glass substrate. In one or more embodiments, the first curved glass substrate exhibits a first sag depth that is within 10% of a second sag depth of the second curved glass substrate. In one or more embodiments, the first glass substrate and the second glass substrate exhibit a shape deviation therebetween of about 5 mm or less as measured by an optical three-dimensional scanner, or exhibit minimal optical distortion. Embodiments of vehicles including such laminates and methods for making such laminates are also disclosed.SELECTED DRAWING: Figure 4 【課題】互いに異なり、互いの間に最小限の形状不一致を示すガラス基板を含む成形ガラス積層体であって、より薄いガラス基板を有する積層体を提供する。【解決手段】630℃の温度で第1の粘度(ポアズ)を含む第1の湾曲したガラス基板;630℃の温度で第1の粘度より大きい第2の粘度を含む第2の湾曲したガラス基板;並びに、第1の湾曲したガラス基板と第2の湾曲したガラス基板との間に配置された中間層を備えた積層体の実施形態が開示される。1つ以上の実施形態では、第1の湾曲したガラス基板は、第2の湾曲したガラス基板の第2の垂下深さの10%以内の第1の垂下深さを示す。1つ以上の実施形態では、第1のガラス基板及び第2のガラス基板は、光学三次元スキャナで測定して約5mm以下の形状偏差を示すか、若しくは最小光学歪みを示す。このような積層体を含む車両の実施形態、及びこのような積層体の製造方法についても開示される。【選択図】図4</description><language>eng ; jpn</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230726&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023103321A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230726&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023103321A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MICHELE MARIE-LOUISE FREDHOLM</creatorcontrib><title>SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME</title><description>To provide shaped glass laminates including glass substrates that differ from one another and exhibit a minimal shape mismatch therebetween, where the glass substrates are thinner.SOLUTION: Embodiments of a laminate are disclosed, the laminate comprising: a first curved glass substrate including a first viscosity (poises) at a temperature of 630°C; a second curved glass substrate including a second viscosity that is greater than the first viscosity at a temperature of 630°C; and an interlayer disposed between the first curved glass substrate and the second curved glass substrate. In one or more embodiments, the first curved glass substrate exhibits a first sag depth that is within 10% of a second sag depth of the second curved glass substrate. In one or more embodiments, the first glass substrate and the second glass substrate exhibit a shape deviation therebetween of about 5 mm or less as measured by an optical three-dimensional scanner, or exhibit minimal optical distortion. Embodiments of vehicles including such laminates and methods for making such laminates are also disclosed.SELECTED DRAWING: Figure 4 【課題】互いに異なり、互いの間に最小限の形状不一致を示すガラス基板を含む成形ガラス積層体であって、より薄いガラス基板を有する積層体を提供する。【解決手段】630℃の温度で第1の粘度(ポアズ)を含む第1の湾曲したガラス基板;630℃の温度で第1の粘度より大きい第2の粘度を含む第2の湾曲したガラス基板;並びに、第1の湾曲したガラス基板と第2の湾曲したガラス基板との間に配置された中間層を備えた積層体の実施形態が開示される。1つ以上の実施形態では、第1の湾曲したガラス基板は、第2の湾曲したガラス基板の第2の垂下深さの10%以内の第1の垂下深さを示す。1つ以上の実施形態では、第1のガラス基板及び第2のガラス基板は、光学三次元スキャナで測定して約5mm以下の形状偏差を示すか、若しくは最小光学歪みを示す。このような積層体を含む車両の実施形態、及びこのような積層体の製造方法についても開示される。【選択図】図4</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAP9nAMcHVRcPdxDA5W8HH09fRzDHENVnD0c1HwdQ3x8HcJVnDzDwJhoJS7QoiHq0Kwo68rDwNrWmJOcSovlOZmUHJzDXH20E0tyI9PLS5ITE7NSy2J9wowMjAyNjQwNjYydDQmShEAX0ooKA</recordid><startdate>20230726</startdate><enddate>20230726</enddate><creator>MICHELE MARIE-LOUISE FREDHOLM</creator><scope>EVB</scope></search><sort><creationdate>20230726</creationdate><title>SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME</title><author>MICHELE MARIE-LOUISE FREDHOLM</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023103321A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>MICHELE MARIE-LOUISE FREDHOLM</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MICHELE MARIE-LOUISE FREDHOLM</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME</title><date>2023-07-26</date><risdate>2023</risdate><abstract>To provide shaped glass laminates including glass substrates that differ from one another and exhibit a minimal shape mismatch therebetween, where the glass substrates are thinner.SOLUTION: Embodiments of a laminate are disclosed, the laminate comprising: a first curved glass substrate including a first viscosity (poises) at a temperature of 630°C; a second curved glass substrate including a second viscosity that is greater than the first viscosity at a temperature of 630°C; and an interlayer disposed between the first curved glass substrate and the second curved glass substrate. In one or more embodiments, the first curved glass substrate exhibits a first sag depth that is within 10% of a second sag depth of the second curved glass substrate. In one or more embodiments, the first glass substrate and the second glass substrate exhibit a shape deviation therebetween of about 5 mm or less as measured by an optical three-dimensional scanner, or exhibit minimal optical distortion. Embodiments of vehicles including such laminates and methods for making such laminates are also disclosed.SELECTED DRAWING: Figure 4 【課題】互いに異なり、互いの間に最小限の形状不一致を示すガラス基板を含む成形ガラス積層体であって、より薄いガラス基板を有する積層体を提供する。【解決手段】630℃の温度で第1の粘度(ポアズ)を含む第1の湾曲したガラス基板;630℃の温度で第1の粘度より大きい第2の粘度を含む第2の湾曲したガラス基板;並びに、第1の湾曲したガラス基板と第2の湾曲したガラス基板との間に配置された中間層を備えた積層体の実施形態が開示される。1つ以上の実施形態では、第1の湾曲したガラス基板は、第2の湾曲したガラス基板の第2の垂下深さの10%以内の第1の垂下深さを示す。1つ以上の実施形態では、第1のガラス基板及び第2のガラス基板は、光学三次元スキャナで測定して約5mm以下の形状偏差を示すか、若しくは最小光学歪みを示す。このような積層体を含む車両の実施形態、及びこのような積層体の製造方法についても開示される。【選択図】図4</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2023103321A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title SHAPED GLASS LAMINATES AND METHODS FOR FORMING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T08%3A19%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MICHELE%20MARIE-LOUISE%20FREDHOLM&rft.date=2023-07-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023103321A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true