METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER
To provide a method for storing a conductive polymer-containing liquid which can be stored stably even in a storage environment at about 40°C, a method for producing a conductive polymer-containing liquid, a method for producing a conductive laminate, and a conductive complex storage container.SOLUT...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MATSUBAYASHI SATOSHI |
description | To provide a method for storing a conductive polymer-containing liquid which can be stored stably even in a storage environment at about 40°C, a method for producing a conductive polymer-containing liquid, a method for producing a conductive laminate, and a conductive complex storage container.SOLUTION: A method for storing a conductive polymer-containing liquid is to store the conductive polymer-containing liquid in a sealed container, wherein the conductive polymer-containing liquid contains a conductive complex containing π-conjugated conductive polymers and polyanions, the polyanions not forming the conductive complex, and a dispersion medium. The level of oxygen included in a space left after subtracting the volume of the conductive polymer-containing liquid from the volume of the container is 9.9 vol.% or less.SELECTED DRAWING: None
【課題】40℃程度の保存環境下でも安定に保存することが可能な導電性高分子含有液の保存方法、導電性高分子含有液の製造方法、導電性積層体の製造方法、及び導電性複合体保存器を提供する。【解決手段】π共役系導電性高分子及びポリアニオンを含む導電性複合体と、前記導電性複合体を形成していない前記ポリアニオンと、分散媒とを含有する導電性高分子含有液を密閉した容器内で保存する方法であって、前記容器の容積から前記導電性高分子含有液の体積を差し引いて残った空間に含まれる酸素濃度を9.9体積%以下とする、導電性高分子含有液の保存方法。【選択図】なし |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023101147A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023101147A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023101147A3</originalsourceid><addsrcrecordid>eNrjZDjm6xri4e-i4OYfpBAc4h_k6eeu4Ozv5xLqHOIZ5qoQ4O8T6esapAsUCnH09APJ-ngGhnq66CggaQwI8gdqoJ5WH0dfTz_HEFcdBUc_F2QJZ3_fAB_XCLBLHd1BfLDZrkE8DKxpiTnFqbxQmptByc01xNlDN7UgPz61uCAxOTUvtSTeK8DIwMjY0MDQ0MTc0ZgoRQCwe1Bv</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER</title><source>esp@cenet</source><creator>MATSUBAYASHI SATOSHI</creator><creatorcontrib>MATSUBAYASHI SATOSHI</creatorcontrib><description>To provide a method for storing a conductive polymer-containing liquid which can be stored stably even in a storage environment at about 40°C, a method for producing a conductive polymer-containing liquid, a method for producing a conductive laminate, and a conductive complex storage container.SOLUTION: A method for storing a conductive polymer-containing liquid is to store the conductive polymer-containing liquid in a sealed container, wherein the conductive polymer-containing liquid contains a conductive complex containing π-conjugated conductive polymers and polyanions, the polyanions not forming the conductive complex, and a dispersion medium. The level of oxygen included in a space left after subtracting the volume of the conductive polymer-containing liquid from the volume of the container is 9.9 vol.% or less.SELECTED DRAWING: None
【課題】40℃程度の保存環境下でも安定に保存することが可能な導電性高分子含有液の保存方法、導電性高分子含有液の製造方法、導電性積層体の製造方法、及び導電性複合体保存器を提供する。【解決手段】π共役系導電性高分子及びポリアニオンを含む導電性複合体と、前記導電性複合体を形成していない前記ポリアニオンと、分散媒とを含有する導電性高分子含有液を密閉した容器内で保存する方法であって、前記容器の容積から前記導電性高分子含有液の体積を差し引いて残った空間に含まれる酸素濃度を9.9体積%以下とする、導電性高分子含有液の保存方法。【選択図】なし</description><language>eng ; jpn</language><subject>BASIC ELECTRIC ELEMENTS ; CABLES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; CONDUCTORS ; ELECTRICITY ; INSULATORS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230720&DB=EPODOC&CC=JP&NR=2023101147A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230720&DB=EPODOC&CC=JP&NR=2023101147A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MATSUBAYASHI SATOSHI</creatorcontrib><title>METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER</title><description>To provide a method for storing a conductive polymer-containing liquid which can be stored stably even in a storage environment at about 40°C, a method for producing a conductive polymer-containing liquid, a method for producing a conductive laminate, and a conductive complex storage container.SOLUTION: A method for storing a conductive polymer-containing liquid is to store the conductive polymer-containing liquid in a sealed container, wherein the conductive polymer-containing liquid contains a conductive complex containing π-conjugated conductive polymers and polyanions, the polyanions not forming the conductive complex, and a dispersion medium. The level of oxygen included in a space left after subtracting the volume of the conductive polymer-containing liquid from the volume of the container is 9.9 vol.% or less.SELECTED DRAWING: None
【課題】40℃程度の保存環境下でも安定に保存することが可能な導電性高分子含有液の保存方法、導電性高分子含有液の製造方法、導電性積層体の製造方法、及び導電性複合体保存器を提供する。【解決手段】π共役系導電性高分子及びポリアニオンを含む導電性複合体と、前記導電性複合体を形成していない前記ポリアニオンと、分散媒とを含有する導電性高分子含有液を密閉した容器内で保存する方法であって、前記容器の容積から前記導電性高分子含有液の体積を差し引いて残った空間に含まれる酸素濃度を9.9体積%以下とする、導電性高分子含有液の保存方法。【選択図】なし</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CABLES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>CONDUCTORS</subject><subject>ELECTRICITY</subject><subject>INSULATORS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDjm6xri4e-i4OYfpBAc4h_k6eeu4Ozv5xLqHOIZ5qoQ4O8T6esapAsUCnH09APJ-ngGhnq66CggaQwI8gdqoJ5WH0dfTz_HEFcdBUc_F2QJZ3_fAB_XCLBLHd1BfLDZrkE8DKxpiTnFqbxQmptByc01xNlDN7UgPz61uCAxOTUvtSTeK8DIwMjY0MDQ0MTc0ZgoRQCwe1Bv</recordid><startdate>20230720</startdate><enddate>20230720</enddate><creator>MATSUBAYASHI SATOSHI</creator><scope>EVB</scope></search><sort><creationdate>20230720</creationdate><title>METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER</title><author>MATSUBAYASHI SATOSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023101147A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CABLES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>CONDUCTORS</topic><topic>ELECTRICITY</topic><topic>INSULATORS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>MATSUBAYASHI SATOSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MATSUBAYASHI SATOSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER</title><date>2023-07-20</date><risdate>2023</risdate><abstract>To provide a method for storing a conductive polymer-containing liquid which can be stored stably even in a storage environment at about 40°C, a method for producing a conductive polymer-containing liquid, a method for producing a conductive laminate, and a conductive complex storage container.SOLUTION: A method for storing a conductive polymer-containing liquid is to store the conductive polymer-containing liquid in a sealed container, wherein the conductive polymer-containing liquid contains a conductive complex containing π-conjugated conductive polymers and polyanions, the polyanions not forming the conductive complex, and a dispersion medium. The level of oxygen included in a space left after subtracting the volume of the conductive polymer-containing liquid from the volume of the container is 9.9 vol.% or less.SELECTED DRAWING: None
【課題】40℃程度の保存環境下でも安定に保存することが可能な導電性高分子含有液の保存方法、導電性高分子含有液の製造方法、導電性積層体の製造方法、及び導電性複合体保存器を提供する。【解決手段】π共役系導電性高分子及びポリアニオンを含む導電性複合体と、前記導電性複合体を形成していない前記ポリアニオンと、分散媒とを含有する導電性高分子含有液を密閉した容器内で保存する方法であって、前記容器の容積から前記導電性高分子含有液の体積を差し引いて残った空間に含まれる酸素濃度を9.9体積%以下とする、導電性高分子含有液の保存方法。【選択図】なし</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; jpn |
recordid | cdi_epo_espacenet_JP2023101147A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CABLES CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS CONDUCTORS ELECTRICITY INSULATORS MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES THEIR PREPARATION OR CHEMICAL WORKING-UP |
title | METHOD FOR STORING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE POLYMER-CONTAINING LIQUID, METHOD FOR PRODUCING CONDUCTIVE LAMINATE, AND CONDUCTIVE COMPLEX STORAGE CONTAINER |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T06%3A24%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MATSUBAYASHI%20SATOSHI&rft.date=2023-07-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023101147A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |