CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE

To provide a cement composition having high acid tolerance, initial cracking resistance, high adhesiveness, and fluidity retention.SOLUTION: A cement composition includes calcium aluminate and pozzolan, where the calcium aluminate includes SO3, ZrO2, and P2O5 as a chemical component, the total amoun...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SASAKI TAKASHI, TAKAGI SATOSHI, YAMAGISHI TAKANORI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SASAKI TAKASHI
TAKAGI SATOSHI
YAMAGISHI TAKANORI
description To provide a cement composition having high acid tolerance, initial cracking resistance, high adhesiveness, and fluidity retention.SOLUTION: A cement composition includes calcium aluminate and pozzolan, where the calcium aluminate includes SO3, ZrO2, and P2O5 as a chemical component, the total amount of SO3, ZrO2, and P2O5 is 0.05 mass% or more and 2.0 mass% or less with respect to 100 pts.mass of the calcium aluminate, and the content of the P2O5 (P2O5/(SO3+ZrO2+P2O5)) is 10 mass% or more and 45 mass% or less.SELECTED DRAWING: None 【課題】優れた耐酸性と初期ひび割れ抵抗性、高い付着性、流動保持性を有するセメント組成物を提供する。【解決手段】アルミン酸カルシウム及びポゾランを含有してなるセメント組成物であって、前記アルミン酸カルシウムが化学成分としてSO3とZrO2とP2O5を含有し、前記アルミン酸カルシウム100質量部に対してSO3とZrO2とP2O5の合計量が0.05質量%以上2.0質量%以下であり、前記P2O5の含有量(P2O5/(SO3+ZrO2+P2O5))が10質量%以上45質量%以下である、セメント組成物である。【選択図】なし
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023049714A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023049714A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023049714A3</originalsourceid><addsrcrecordid>eNrjZPB2dvV19QtRcPb3DfAP9gzx9PfTUQhyDXD0DPL0c1fwdQ3x8HdRCA0GcUI8XBWCHX1ddRQc_VyAOvycg1xDgEIhQaHOIaFBrjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjAyNjAxNLc0MTRmChFAOKxLhQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE</title><source>esp@cenet</source><creator>SASAKI TAKASHI ; TAKAGI SATOSHI ; YAMAGISHI TAKANORI</creator><creatorcontrib>SASAKI TAKASHI ; TAKAGI SATOSHI ; YAMAGISHI TAKANORI</creatorcontrib><description>To provide a cement composition having high acid tolerance, initial cracking resistance, high adhesiveness, and fluidity retention.SOLUTION: A cement composition includes calcium aluminate and pozzolan, where the calcium aluminate includes SO3, ZrO2, and P2O5 as a chemical component, the total amount of SO3, ZrO2, and P2O5 is 0.05 mass% or more and 2.0 mass% or less with respect to 100 pts.mass of the calcium aluminate, and the content of the P2O5 (P2O5/(SO3+ZrO2+P2O5)) is 10 mass% or more and 45 mass% or less.SELECTED DRAWING: None 【課題】優れた耐酸性と初期ひび割れ抵抗性、高い付着性、流動保持性を有するセメント組成物を提供する。【解決手段】アルミン酸カルシウム及びポゾランを含有してなるセメント組成物であって、前記アルミン酸カルシウムが化学成分としてSO3とZrO2とP2O5を含有し、前記アルミン酸カルシウム100質量部に対してSO3とZrO2とP2O5の合計量が0.05質量%以上2.0質量%以下であり、前記P2O5の含有量(P2O5/(SO3+ZrO2+P2O5))が10質量%以上45質量%以下である、セメント組成物である。【選択図】なし</description><language>eng ; jpn</language><subject>ARTIFICIAL STONE ; BUILDING ; BUILDING IMPLEMENTS OR OTHER BUILDING AIDS, OR THEIRUSE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; FIXED CONSTRUCTIONS ; FORMS ; HANDLING BUILDING MATERIALS ON THE SITE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTINGBUILDINGS ; SCAFFOLDING ; SHUTTERING ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230410&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023049714A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230410&amp;DB=EPODOC&amp;CC=JP&amp;NR=2023049714A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SASAKI TAKASHI</creatorcontrib><creatorcontrib>TAKAGI SATOSHI</creatorcontrib><creatorcontrib>YAMAGISHI TAKANORI</creatorcontrib><title>CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE</title><description>To provide a cement composition having high acid tolerance, initial cracking resistance, high adhesiveness, and fluidity retention.SOLUTION: A cement composition includes calcium aluminate and pozzolan, where the calcium aluminate includes SO3, ZrO2, and P2O5 as a chemical component, the total amount of SO3, ZrO2, and P2O5 is 0.05 mass% or more and 2.0 mass% or less with respect to 100 pts.mass of the calcium aluminate, and the content of the P2O5 (P2O5/(SO3+ZrO2+P2O5)) is 10 mass% or more and 45 mass% or less.SELECTED DRAWING: None 【課題】優れた耐酸性と初期ひび割れ抵抗性、高い付着性、流動保持性を有するセメント組成物を提供する。【解決手段】アルミン酸カルシウム及びポゾランを含有してなるセメント組成物であって、前記アルミン酸カルシウムが化学成分としてSO3とZrO2とP2O5を含有し、前記アルミン酸カルシウム100質量部に対してSO3とZrO2とP2O5の合計量が0.05質量%以上2.0質量%以下であり、前記P2O5の含有量(P2O5/(SO3+ZrO2+P2O5))が10質量%以上45質量%以下である、セメント組成物である。【選択図】なし</description><subject>ARTIFICIAL STONE</subject><subject>BUILDING</subject><subject>BUILDING IMPLEMENTS OR OTHER BUILDING AIDS, OR THEIRUSE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>FIXED CONSTRUCTIONS</subject><subject>FORMS</subject><subject>HANDLING BUILDING MATERIALS ON THE SITE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTINGBUILDINGS</subject><subject>SCAFFOLDING</subject><subject>SHUTTERING</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPB2dvV19QtRcPb3DfAP9gzx9PfTUQhyDXD0DPL0c1fwdQ3x8HdRCA0GcUI8XBWCHX1ddRQc_VyAOvycg1xDgEIhQaHOIaFBrjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjAyNjAxNLc0MTRmChFAOKxLhQ</recordid><startdate>20230410</startdate><enddate>20230410</enddate><creator>SASAKI TAKASHI</creator><creator>TAKAGI SATOSHI</creator><creator>YAMAGISHI TAKANORI</creator><scope>EVB</scope></search><sort><creationdate>20230410</creationdate><title>CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE</title><author>SASAKI TAKASHI ; TAKAGI SATOSHI ; YAMAGISHI TAKANORI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023049714A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>ARTIFICIAL STONE</topic><topic>BUILDING</topic><topic>BUILDING IMPLEMENTS OR OTHER BUILDING AIDS, OR THEIRUSE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>FIXED CONSTRUCTIONS</topic><topic>FORMS</topic><topic>HANDLING BUILDING MATERIALS ON THE SITE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTINGBUILDINGS</topic><topic>SCAFFOLDING</topic><topic>SHUTTERING</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SASAKI TAKASHI</creatorcontrib><creatorcontrib>TAKAGI SATOSHI</creatorcontrib><creatorcontrib>YAMAGISHI TAKANORI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SASAKI TAKASHI</au><au>TAKAGI SATOSHI</au><au>YAMAGISHI TAKANORI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE</title><date>2023-04-10</date><risdate>2023</risdate><abstract>To provide a cement composition having high acid tolerance, initial cracking resistance, high adhesiveness, and fluidity retention.SOLUTION: A cement composition includes calcium aluminate and pozzolan, where the calcium aluminate includes SO3, ZrO2, and P2O5 as a chemical component, the total amount of SO3, ZrO2, and P2O5 is 0.05 mass% or more and 2.0 mass% or less with respect to 100 pts.mass of the calcium aluminate, and the content of the P2O5 (P2O5/(SO3+ZrO2+P2O5)) is 10 mass% or more and 45 mass% or less.SELECTED DRAWING: None 【課題】優れた耐酸性と初期ひび割れ抵抗性、高い付着性、流動保持性を有するセメント組成物を提供する。【解決手段】アルミン酸カルシウム及びポゾランを含有してなるセメント組成物であって、前記アルミン酸カルシウムが化学成分としてSO3とZrO2とP2O5を含有し、前記アルミン酸カルシウム100質量部に対してSO3とZrO2とP2O5の合計量が0.05質量%以上2.0質量%以下であり、前記P2O5の含有量(P2O5/(SO3+ZrO2+P2O5))が10質量%以上45質量%以下である、セメント組成物である。【選択図】なし</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2023049714A
source esp@cenet
subjects ARTIFICIAL STONE
BUILDING
BUILDING IMPLEMENTS OR OTHER BUILDING AIDS, OR THEIRUSE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
FIXED CONSTRUCTIONS
FORMS
HANDLING BUILDING MATERIALS ON THE SITE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTINGBUILDINGS
SCAFFOLDING
SHUTTERING
SLAG
TREATMENT OF NATURAL STONE
title CEMENT COMPOSITION, REPAIRING METHOD USING THE SAME, AND CONCRETE STRUCTURE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T15%3A43%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SASAKI%20TAKASHI&rft.date=2023-04-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023049714A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true