RESIN MOLDING

To provide a resin molding having a high coloring density and scratch resistance with a simple production process.SOLUTION: Provided is a resin molding in which a colored protective layer colored in a second color which is a color similar to a first color is stacked on at least a part of a surface o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: INAGAKI SHUNSUKE, TSUJIMOTO KAZUHISA, TSUBOTA MASANORI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a resin molding having a high coloring density and scratch resistance with a simple production process.SOLUTION: Provided is a resin molding in which a colored protective layer colored in a second color which is a color similar to a first color is stacked on at least a part of a surface of a resin substrate colored in the first color. The colored protective layer is made of photosetting acrylic resin containing 1.0 to 11.0 mass% of a color material having a primary particle size distribution falling within a range of 20 to 170 nm, and the colored protective layer has a thickness of less than or equal to 5.0 μm.SELECTED DRAWING: Figure 1 【課題】高い着色濃度と耐擦傷性とを備えた樹脂成形品を、簡易な製造工程で提供する。【解決手段】第一の色に着色された樹脂基材の表面の少なくとも一部に、前記第一の色と同系色である第二の色に着色された着色保護層が積層されており、前記着色保護層は一次粒子径分布が20~170nmの範囲内である色材を1.0~11.0質量%含有する光硬化型アクリル樹脂からなり、前記着色保護層の厚さが5.0μm以下であることを特徴とする、樹脂成形品。【選択図】図1