POWDER CONTAINING GROUND CEMENT CLINKER

To provide a powder containing ground cement clinker, which is a cement material that has excellent early strength development under a low-temperature environment and shows a small degree of decrease in the early strength development when compared with the early strength development under a normal t...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TADA MASATO, UCHIDA SHUNICHIRO, HAYASHI KENSUKE
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TADA MASATO
UCHIDA SHUNICHIRO
HAYASHI KENSUKE
description To provide a powder containing ground cement clinker, which is a cement material that has excellent early strength development under a low-temperature environment and shows a small degree of decrease in the early strength development when compared with the early strength development under a normal temperature environment.SOLUTION: A powder containing ground cement clinker is a cement clinker powder or a mixture of a cement clinker powder and a quicklime powder. The powder is composed of 42-65 mass% of alite, 12-40 mass% of belite, 12-18 mass% of aluminate phase, 0.5-12 mass% of ferrite phase and 0.7-3.0 mass% of free lime as calculated by the Borg formula where a value of the percentage of CaO used in the calculation of alite is the percentage of total CaO contained in the powder containing ground cement clinker, from which the percentage of free lime is subtracted.SELECTED DRAWING: None 【課題】低温の環境下において早期強度発現性に優れ、かつ、常温の環境下における早期強度発現性と比較した場合に早期強度発現性の低下の程度が小さいセメントの材料である、セメントクリンカ粉砕物含有粉末を提供する。【解決手段】セメントクリンカ粉砕物、または、セメントクリンカ粉砕物と生石灰粉末の混合物である、セメントクリンカ粉砕物含有粉末であって、ボーグ式(ただし、エーライトの算出において用いられるCaOの割合の数値は、セメントクリンカ粉砕物含有粉末に含まれる全CaOの割合から、遊離石灰の割合を減じたものとする。)で算出される値として、エーライトの割合が42~65質量%、ビーライトの割合が12~40質量%、アルミネート相の割合が12~18質量%、および、フェライト相の割合が0.5~12質量%であり、かつ、遊離石灰の割合が0.7~3.0質量%であるセメントクリンカ粉砕物含有粉末。【選択図】なし
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2022131065A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2022131065A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2022131065A3</originalsourceid><addsrcrecordid>eNrjZFAP8A93cQ1ScPb3C3H09PP0c1dwD_IP9XNRcHb1dfULUXD28fTzdg3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBkZGhsaGBmamjsZEKQIAMUAkPA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>POWDER CONTAINING GROUND CEMENT CLINKER</title><source>esp@cenet</source><creator>TADA MASATO ; UCHIDA SHUNICHIRO ; HAYASHI KENSUKE</creator><creatorcontrib>TADA MASATO ; UCHIDA SHUNICHIRO ; HAYASHI KENSUKE</creatorcontrib><description>To provide a powder containing ground cement clinker, which is a cement material that has excellent early strength development under a low-temperature environment and shows a small degree of decrease in the early strength development when compared with the early strength development under a normal temperature environment.SOLUTION: A powder containing ground cement clinker is a cement clinker powder or a mixture of a cement clinker powder and a quicklime powder. The powder is composed of 42-65 mass% of alite, 12-40 mass% of belite, 12-18 mass% of aluminate phase, 0.5-12 mass% of ferrite phase and 0.7-3.0 mass% of free lime as calculated by the Borg formula where a value of the percentage of CaO used in the calculation of alite is the percentage of total CaO contained in the powder containing ground cement clinker, from which the percentage of free lime is subtracted.SELECTED DRAWING: None 【課題】低温の環境下において早期強度発現性に優れ、かつ、常温の環境下における早期強度発現性と比較した場合に早期強度発現性の低下の程度が小さいセメントの材料である、セメントクリンカ粉砕物含有粉末を提供する。【解決手段】セメントクリンカ粉砕物、または、セメントクリンカ粉砕物と生石灰粉末の混合物である、セメントクリンカ粉砕物含有粉末であって、ボーグ式(ただし、エーライトの算出において用いられるCaOの割合の数値は、セメントクリンカ粉砕物含有粉末に含まれる全CaOの割合から、遊離石灰の割合を減じたものとする。)で算出される値として、エーライトの割合が42~65質量%、ビーライトの割合が12~40質量%、アルミネート相の割合が12~18質量%、および、フェライト相の割合が0.5~12質量%であり、かつ、遊離石灰の割合が0.7~3.0質量%であるセメントクリンカ粉砕物含有粉末。【選択図】なし</description><language>eng ; jpn</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220907&amp;DB=EPODOC&amp;CC=JP&amp;NR=2022131065A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,782,887,25571,76555</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20220907&amp;DB=EPODOC&amp;CC=JP&amp;NR=2022131065A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TADA MASATO</creatorcontrib><creatorcontrib>UCHIDA SHUNICHIRO</creatorcontrib><creatorcontrib>HAYASHI KENSUKE</creatorcontrib><title>POWDER CONTAINING GROUND CEMENT CLINKER</title><description>To provide a powder containing ground cement clinker, which is a cement material that has excellent early strength development under a low-temperature environment and shows a small degree of decrease in the early strength development when compared with the early strength development under a normal temperature environment.SOLUTION: A powder containing ground cement clinker is a cement clinker powder or a mixture of a cement clinker powder and a quicklime powder. The powder is composed of 42-65 mass% of alite, 12-40 mass% of belite, 12-18 mass% of aluminate phase, 0.5-12 mass% of ferrite phase and 0.7-3.0 mass% of free lime as calculated by the Borg formula where a value of the percentage of CaO used in the calculation of alite is the percentage of total CaO contained in the powder containing ground cement clinker, from which the percentage of free lime is subtracted.SELECTED DRAWING: None 【課題】低温の環境下において早期強度発現性に優れ、かつ、常温の環境下における早期強度発現性と比較した場合に早期強度発現性の低下の程度が小さいセメントの材料である、セメントクリンカ粉砕物含有粉末を提供する。【解決手段】セメントクリンカ粉砕物、または、セメントクリンカ粉砕物と生石灰粉末の混合物である、セメントクリンカ粉砕物含有粉末であって、ボーグ式(ただし、エーライトの算出において用いられるCaOの割合の数値は、セメントクリンカ粉砕物含有粉末に含まれる全CaOの割合から、遊離石灰の割合を減じたものとする。)で算出される値として、エーライトの割合が42~65質量%、ビーライトの割合が12~40質量%、アルミネート相の割合が12~18質量%、および、フェライト相の割合が0.5~12質量%であり、かつ、遊離石灰の割合が0.7~3.0質量%であるセメントクリンカ粉砕物含有粉末。【選択図】なし</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFAP8A93cQ1ScPb3C3H09PP0c1dwD_IP9XNRcHb1dfULUXD28fTzdg3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBkZGhsaGBmamjsZEKQIAMUAkPA</recordid><startdate>20220907</startdate><enddate>20220907</enddate><creator>TADA MASATO</creator><creator>UCHIDA SHUNICHIRO</creator><creator>HAYASHI KENSUKE</creator><scope>EVB</scope></search><sort><creationdate>20220907</creationdate><title>POWDER CONTAINING GROUND CEMENT CLINKER</title><author>TADA MASATO ; UCHIDA SHUNICHIRO ; HAYASHI KENSUKE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2022131065A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2022</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>TADA MASATO</creatorcontrib><creatorcontrib>UCHIDA SHUNICHIRO</creatorcontrib><creatorcontrib>HAYASHI KENSUKE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TADA MASATO</au><au>UCHIDA SHUNICHIRO</au><au>HAYASHI KENSUKE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>POWDER CONTAINING GROUND CEMENT CLINKER</title><date>2022-09-07</date><risdate>2022</risdate><abstract>To provide a powder containing ground cement clinker, which is a cement material that has excellent early strength development under a low-temperature environment and shows a small degree of decrease in the early strength development when compared with the early strength development under a normal temperature environment.SOLUTION: A powder containing ground cement clinker is a cement clinker powder or a mixture of a cement clinker powder and a quicklime powder. The powder is composed of 42-65 mass% of alite, 12-40 mass% of belite, 12-18 mass% of aluminate phase, 0.5-12 mass% of ferrite phase and 0.7-3.0 mass% of free lime as calculated by the Borg formula where a value of the percentage of CaO used in the calculation of alite is the percentage of total CaO contained in the powder containing ground cement clinker, from which the percentage of free lime is subtracted.SELECTED DRAWING: None 【課題】低温の環境下において早期強度発現性に優れ、かつ、常温の環境下における早期強度発現性と比較した場合に早期強度発現性の低下の程度が小さいセメントの材料である、セメントクリンカ粉砕物含有粉末を提供する。【解決手段】セメントクリンカ粉砕物、または、セメントクリンカ粉砕物と生石灰粉末の混合物である、セメントクリンカ粉砕物含有粉末であって、ボーグ式(ただし、エーライトの算出において用いられるCaOの割合の数値は、セメントクリンカ粉砕物含有粉末に含まれる全CaOの割合から、遊離石灰の割合を減じたものとする。)で算出される値として、エーライトの割合が42~65質量%、ビーライトの割合が12~40質量%、アルミネート相の割合が12~18質量%、および、フェライト相の割合が0.5~12質量%であり、かつ、遊離石灰の割合が0.7~3.0質量%であるセメントクリンカ粉砕物含有粉末。【選択図】なし</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2022131065A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title POWDER CONTAINING GROUND CEMENT CLINKER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-04T08%3A27%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TADA%20MASATO&rft.date=2022-09-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2022131065A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true