METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE

To provide the method for charging the coal, that can suppress overload and leveler breakage caused in a leveler device by using an existing leveler device.SOLUTION: The method for charging the coal comprises charging the coal containing 80 mass% or more of molding coal into a carbonization chamber...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KONO HIRONORI, OTSUKA KEIJI, IMANISHI DAISUKE, SHIWAKU TATSUHIRO, NANRI NARUMI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KONO HIRONORI
OTSUKA KEIJI
IMANISHI DAISUKE
SHIWAKU TATSUHIRO
NANRI NARUMI
description To provide the method for charging the coal, that can suppress overload and leveler breakage caused in a leveler device by using an existing leveler device.SOLUTION: The method for charging the coal comprises charging the coal containing 80 mass% or more of molding coal into a carbonization chamber through a plurality of coal charging holes in a chamber-type coke oven provided with a leveler that is inserted into the carbonization chamber from a machine side and moves to a coke side, in which a coal charge height under a coal charge hole provided closest to the coke side is lower than a height at which the leveler is provided, between start of operation and completion of the operation of the leveler, when the coal is charged into the carbonization chamber.SELECTED DRAWING: Figure 1 【課題】既存のレベラ装置を用いながらレベラ装置に生じる過負荷およびレベラの破損を抑制できる石炭装入方法を提供する。【解決手段】石炭の装入方法であって、マシンサイド側から炭化室に挿入され、コークスサイド側に移動するレベラが設けられた室炉型コークス炉に、成型炭を80質量%以上含む石炭を複数の装炭孔から炭化室に装入する石炭装入方法であって、レベラが動作開始した後、動作完了するまでの間において、最もコークスサイド側に設けられた装炭孔の下の石炭の装炭高さが、レベラが設けられた高さよりも低くなるように、石炭を炭化室に装入する。【選択図】図1
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2020152742A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2020152742A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2020152742A3</originalsourceid><addsrcrecordid>eNrjZDDzdQ3x8HdRcPMPUnD2cAxy9_RzV3D2d_RRcPRzUUCSDAjydwl1hsh6u_IwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDIwNDUyNzEyNHY6IUAQApCifV</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE</title><source>esp@cenet</source><creator>KONO HIRONORI ; OTSUKA KEIJI ; IMANISHI DAISUKE ; SHIWAKU TATSUHIRO ; NANRI NARUMI</creator><creatorcontrib>KONO HIRONORI ; OTSUKA KEIJI ; IMANISHI DAISUKE ; SHIWAKU TATSUHIRO ; NANRI NARUMI</creatorcontrib><description>To provide the method for charging the coal, that can suppress overload and leveler breakage caused in a leveler device by using an existing leveler device.SOLUTION: The method for charging the coal comprises charging the coal containing 80 mass% or more of molding coal into a carbonization chamber through a plurality of coal charging holes in a chamber-type coke oven provided with a leveler that is inserted into the carbonization chamber from a machine side and moves to a coke side, in which a coal charge height under a coal charge hole provided closest to the coke side is lower than a height at which the leveler is provided, between start of operation and completion of the operation of the leveler, when the coal is charged into the carbonization chamber.SELECTED DRAWING: Figure 1 【課題】既存のレベラ装置を用いながらレベラ装置に生じる過負荷およびレベラの破損を抑制できる石炭装入方法を提供する。【解決手段】石炭の装入方法であって、マシンサイド側から炭化室に挿入され、コークスサイド側に移動するレベラが設けられた室炉型コークス炉に、成型炭を80質量%以上含む石炭を複数の装炭孔から炭化室に装入する石炭装入方法であって、レベラが動作開始した後、動作完了するまでの間において、最もコークスサイド側に設けられた装炭孔の下の石炭の装炭高さが、レベラが設けられた高さよりも低くなるように、石炭を炭化室に装入する。【選択図】図1</description><language>eng ; jpn</language><subject>CHEMISTRY ; DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS ; FUELS ; LUBRICANTS ; METALLURGY ; PEAT ; PETROLEUM, GAS OR COKE INDUSTRIES ; TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200924&amp;DB=EPODOC&amp;CC=JP&amp;NR=2020152742A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200924&amp;DB=EPODOC&amp;CC=JP&amp;NR=2020152742A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONO HIRONORI</creatorcontrib><creatorcontrib>OTSUKA KEIJI</creatorcontrib><creatorcontrib>IMANISHI DAISUKE</creatorcontrib><creatorcontrib>SHIWAKU TATSUHIRO</creatorcontrib><creatorcontrib>NANRI NARUMI</creatorcontrib><title>METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE</title><description>To provide the method for charging the coal, that can suppress overload and leveler breakage caused in a leveler device by using an existing leveler device.SOLUTION: The method for charging the coal comprises charging the coal containing 80 mass% or more of molding coal into a carbonization chamber through a plurality of coal charging holes in a chamber-type coke oven provided with a leveler that is inserted into the carbonization chamber from a machine side and moves to a coke side, in which a coal charge height under a coal charge hole provided closest to the coke side is lower than a height at which the leveler is provided, between start of operation and completion of the operation of the leveler, when the coal is charged into the carbonization chamber.SELECTED DRAWING: Figure 1 【課題】既存のレベラ装置を用いながらレベラ装置に生じる過負荷およびレベラの破損を抑制できる石炭装入方法を提供する。【解決手段】石炭の装入方法であって、マシンサイド側から炭化室に挿入され、コークスサイド側に移動するレベラが設けられた室炉型コークス炉に、成型炭を80質量%以上含む石炭を複数の装炭孔から炭化室に装入する石炭装入方法であって、レベラが動作開始した後、動作完了するまでの間において、最もコークスサイド側に設けられた装炭孔の下の石炭の装炭高さが、レベラが設けられた高さよりも低くなるように、石炭を炭化室に装入する。【選択図】図1</description><subject>CHEMISTRY</subject><subject>DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>PEAT</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDzdQ3x8HdRcPMPUnD2cAxy9_RzV3D2d_RRcPRzUUCSDAjydwl1hsh6u_IwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDIwNDUyNzEyNHY6IUAQApCifV</recordid><startdate>20200924</startdate><enddate>20200924</enddate><creator>KONO HIRONORI</creator><creator>OTSUKA KEIJI</creator><creator>IMANISHI DAISUKE</creator><creator>SHIWAKU TATSUHIRO</creator><creator>NANRI NARUMI</creator><scope>EVB</scope></search><sort><creationdate>20200924</creationdate><title>METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE</title><author>KONO HIRONORI ; OTSUKA KEIJI ; IMANISHI DAISUKE ; SHIWAKU TATSUHIRO ; NANRI NARUMI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2020152742A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>PEAT</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><toplevel>online_resources</toplevel><creatorcontrib>KONO HIRONORI</creatorcontrib><creatorcontrib>OTSUKA KEIJI</creatorcontrib><creatorcontrib>IMANISHI DAISUKE</creatorcontrib><creatorcontrib>SHIWAKU TATSUHIRO</creatorcontrib><creatorcontrib>NANRI NARUMI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONO HIRONORI</au><au>OTSUKA KEIJI</au><au>IMANISHI DAISUKE</au><au>SHIWAKU TATSUHIRO</au><au>NANRI NARUMI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE</title><date>2020-09-24</date><risdate>2020</risdate><abstract>To provide the method for charging the coal, that can suppress overload and leveler breakage caused in a leveler device by using an existing leveler device.SOLUTION: The method for charging the coal comprises charging the coal containing 80 mass% or more of molding coal into a carbonization chamber through a plurality of coal charging holes in a chamber-type coke oven provided with a leveler that is inserted into the carbonization chamber from a machine side and moves to a coke side, in which a coal charge height under a coal charge hole provided closest to the coke side is lower than a height at which the leveler is provided, between start of operation and completion of the operation of the leveler, when the coal is charged into the carbonization chamber.SELECTED DRAWING: Figure 1 【課題】既存のレベラ装置を用いながらレベラ装置に生じる過負荷およびレベラの破損を抑制できる石炭装入方法を提供する。【解決手段】石炭の装入方法であって、マシンサイド側から炭化室に挿入され、コークスサイド側に移動するレベラが設けられた室炉型コークス炉に、成型炭を80質量%以上含む石炭を複数の装炭孔から炭化室に装入する石炭装入方法であって、レベラが動作開始した後、動作完了するまでの間において、最もコークスサイド側に設けられた装炭孔の下の石炭の装炭高さが、レベラが設けられた高さよりも低くなるように、石炭を炭化室に装入する。【選択図】図1</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2020152742A
source esp@cenet
subjects CHEMISTRY
DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS
FUELS
LUBRICANTS
METALLURGY
PEAT
PETROLEUM, GAS OR COKE INDUSTRIES
TECHNICAL GASES CONTAINING CARBON MONOXIDE
title METHOD FOR CHARGING COAL AND METHOD FOR PRODUCING COKE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-21T15%3A08%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONO%20HIRONORI&rft.date=2020-09-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2020152742A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true