METHOD FOR PRODUCING COAL ASH GRANULE

To provide a method for producing coal ash granules in which a granulation step and a granulation device are simple, and the grain size distribution of the obtained granules is narrow.SOLUTION: A method for producing coal ash granules using a granulation machine with a rotary drum having openable/cl...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOBAYAKAWA MAKOTO, IZUMI KAZUSHI, IYASAKA KOICHIRO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KOBAYAKAWA MAKOTO
IZUMI KAZUSHI
IYASAKA KOICHIRO
description To provide a method for producing coal ash granules in which a granulation step and a granulation device are simple, and the grain size distribution of the obtained granules is narrow.SOLUTION: A method for producing coal ash granules using a granulation machine with a rotary drum having openable/closable cover comprises (A) a preliminary mixing step of charging powder at least including coal ash and a binder into the rotary drum oriented at a tilt angle of 0 to 45° with respect to a vertical axis, with a face having the cover of the rotary drum facing upward, thereafter, closing the cover, and rotating the rotary drum for preliminary mixing; (B) a granulation nuclei production step of rotating the rotary drum oriented at a tilt angle of 5 to 45° with respect to the vertical axis, with the cover of the rotary drum open, and with the face having the cover of the rotary drum facing upward, at 15 to 20 rpm for 25 to 30 min, while intermittently adding water into the rotary drum to produce granulation nuclei; and (C) a grain size adjustment step of adjusting grain sizes of granules while rotating the rotary drum at 1 to 5 rpm for 5 to 10 min, with the cover of the drum open or closed.SELECTED DRAWING: Figure 3 【課題】造粒工程や造粒装置が簡素で、得られた造粒物の粒度分布が狭い石炭灰造粒物を製造する方法を提供する。【解決手段】開閉自在な蓋を有する回転ドラムを有する造粒機を用いて石炭灰造粒物を製造する方法。(A)回転ドラムの蓋のある面を上面にして、垂直から0〜45°の傾斜角を有する回転ドラム内に、少なくとも石炭灰および結合材を含む粉体を投入した後、蓋を閉めて回転させて予め混合する、予備的混合工程、(B)回転ドラムの蓋を開けた状態で、回転ドラムの蓋のある面を上面にして、垂直から5〜45°の傾斜角を有する回転ドラムを15〜20rpmで25〜30分間回転させながら、回転ドラム内に断続的に加水して造粒核を作製する、造粒核作製工程、(C)回転ドラムの蓋を開けた状態、または閉めた状態で、回転ドラムを1〜5rpmで5〜10分間回転させながら、造粒物の粒径を調整する、粒径調整工程を含む。【選択図】図3
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2020037226A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2020037226A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2020037226A3</originalsourceid><addsrcrecordid>eNrjZFD1dQ3x8HdRcPMPUggI8ncJdfb0c1dw9nf0UXAM9lBwD3L0C_Vx5WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgZGBgbG5kZGZo7GRCkCAMtQI2w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING COAL ASH GRANULE</title><source>esp@cenet</source><creator>KOBAYAKAWA MAKOTO ; IZUMI KAZUSHI ; IYASAKA KOICHIRO</creator><creatorcontrib>KOBAYAKAWA MAKOTO ; IZUMI KAZUSHI ; IYASAKA KOICHIRO</creatorcontrib><description>To provide a method for producing coal ash granules in which a granulation step and a granulation device are simple, and the grain size distribution of the obtained granules is narrow.SOLUTION: A method for producing coal ash granules using a granulation machine with a rotary drum having openable/closable cover comprises (A) a preliminary mixing step of charging powder at least including coal ash and a binder into the rotary drum oriented at a tilt angle of 0 to 45° with respect to a vertical axis, with a face having the cover of the rotary drum facing upward, thereafter, closing the cover, and rotating the rotary drum for preliminary mixing; (B) a granulation nuclei production step of rotating the rotary drum oriented at a tilt angle of 5 to 45° with respect to the vertical axis, with the cover of the rotary drum open, and with the face having the cover of the rotary drum facing upward, at 15 to 20 rpm for 25 to 30 min, while intermittently adding water into the rotary drum to produce granulation nuclei; and (C) a grain size adjustment step of adjusting grain sizes of granules while rotating the rotary drum at 1 to 5 rpm for 5 to 10 min, with the cover of the drum open or closed.SELECTED DRAWING: Figure 3 【課題】造粒工程や造粒装置が簡素で、得られた造粒物の粒度分布が狭い石炭灰造粒物を製造する方法を提供する。【解決手段】開閉自在な蓋を有する回転ドラムを有する造粒機を用いて石炭灰造粒物を製造する方法。(A)回転ドラムの蓋のある面を上面にして、垂直から0〜45°の傾斜角を有する回転ドラム内に、少なくとも石炭灰および結合材を含む粉体を投入した後、蓋を閉めて回転させて予め混合する、予備的混合工程、(B)回転ドラムの蓋を開けた状態で、回転ドラムの蓋のある面を上面にして、垂直から5〜45°の傾斜角を有する回転ドラムを15〜20rpmで25〜30分間回転させながら、回転ドラム内に断続的に加水して造粒核を作製する、造粒核作製工程、(C)回転ドラムの蓋を開けた状態、または閉めた状態で、回転ドラムを1〜5rpmで5〜10分間回転させながら、造粒物の粒径を調整する、粒径調整工程を含む。【選択図】図3</description><language>eng ; jpn</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; PREPARING CLAY ; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL,e.g. PLASTER ; REFRACTORIES ; SLAG ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF NATURAL STONE ; WORKING CEMENT, CLAY, OR STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200312&amp;DB=EPODOC&amp;CC=JP&amp;NR=2020037226A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200312&amp;DB=EPODOC&amp;CC=JP&amp;NR=2020037226A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KOBAYAKAWA MAKOTO</creatorcontrib><creatorcontrib>IZUMI KAZUSHI</creatorcontrib><creatorcontrib>IYASAKA KOICHIRO</creatorcontrib><title>METHOD FOR PRODUCING COAL ASH GRANULE</title><description>To provide a method for producing coal ash granules in which a granulation step and a granulation device are simple, and the grain size distribution of the obtained granules is narrow.SOLUTION: A method for producing coal ash granules using a granulation machine with a rotary drum having openable/closable cover comprises (A) a preliminary mixing step of charging powder at least including coal ash and a binder into the rotary drum oriented at a tilt angle of 0 to 45° with respect to a vertical axis, with a face having the cover of the rotary drum facing upward, thereafter, closing the cover, and rotating the rotary drum for preliminary mixing; (B) a granulation nuclei production step of rotating the rotary drum oriented at a tilt angle of 5 to 45° with respect to the vertical axis, with the cover of the rotary drum open, and with the face having the cover of the rotary drum facing upward, at 15 to 20 rpm for 25 to 30 min, while intermittently adding water into the rotary drum to produce granulation nuclei; and (C) a grain size adjustment step of adjusting grain sizes of granules while rotating the rotary drum at 1 to 5 rpm for 5 to 10 min, with the cover of the drum open or closed.SELECTED DRAWING: Figure 3 【課題】造粒工程や造粒装置が簡素で、得られた造粒物の粒度分布が狭い石炭灰造粒物を製造する方法を提供する。【解決手段】開閉自在な蓋を有する回転ドラムを有する造粒機を用いて石炭灰造粒物を製造する方法。(A)回転ドラムの蓋のある面を上面にして、垂直から0〜45°の傾斜角を有する回転ドラム内に、少なくとも石炭灰および結合材を含む粉体を投入した後、蓋を閉めて回転させて予め混合する、予備的混合工程、(B)回転ドラムの蓋を開けた状態で、回転ドラムの蓋のある面を上面にして、垂直から5〜45°の傾斜角を有する回転ドラムを15〜20rpmで25〜30分間回転させながら、回転ドラム内に断続的に加水して造粒核を作製する、造粒核作製工程、(C)回転ドラムの蓋を開けた状態、または閉めた状態で、回転ドラムを1〜5rpmで5〜10分間回転させながら、造粒物の粒径を調整する、粒径調整工程を含む。【選択図】図3</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>PREPARING CLAY</subject><subject>PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL,e.g. PLASTER</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><subject>WORKING CEMENT, CLAY, OR STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD1dQ3x8HdRcPMPUggI8ncJdfb0c1dw9nf0UXAM9lBwD3L0C_Vx5WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgZGBgbG5kZGZo7GRCkCAMtQI2w</recordid><startdate>20200312</startdate><enddate>20200312</enddate><creator>KOBAYAKAWA MAKOTO</creator><creator>IZUMI KAZUSHI</creator><creator>IYASAKA KOICHIRO</creator><scope>EVB</scope></search><sort><creationdate>20200312</creationdate><title>METHOD FOR PRODUCING COAL ASH GRANULE</title><author>KOBAYAKAWA MAKOTO ; IZUMI KAZUSHI ; IYASAKA KOICHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2020037226A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>PREPARING CLAY</topic><topic>PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL,e.g. PLASTER</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><topic>WORKING CEMENT, CLAY, OR STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>KOBAYAKAWA MAKOTO</creatorcontrib><creatorcontrib>IZUMI KAZUSHI</creatorcontrib><creatorcontrib>IYASAKA KOICHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KOBAYAKAWA MAKOTO</au><au>IZUMI KAZUSHI</au><au>IYASAKA KOICHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING COAL ASH GRANULE</title><date>2020-03-12</date><risdate>2020</risdate><abstract>To provide a method for producing coal ash granules in which a granulation step and a granulation device are simple, and the grain size distribution of the obtained granules is narrow.SOLUTION: A method for producing coal ash granules using a granulation machine with a rotary drum having openable/closable cover comprises (A) a preliminary mixing step of charging powder at least including coal ash and a binder into the rotary drum oriented at a tilt angle of 0 to 45° with respect to a vertical axis, with a face having the cover of the rotary drum facing upward, thereafter, closing the cover, and rotating the rotary drum for preliminary mixing; (B) a granulation nuclei production step of rotating the rotary drum oriented at a tilt angle of 5 to 45° with respect to the vertical axis, with the cover of the rotary drum open, and with the face having the cover of the rotary drum facing upward, at 15 to 20 rpm for 25 to 30 min, while intermittently adding water into the rotary drum to produce granulation nuclei; and (C) a grain size adjustment step of adjusting grain sizes of granules while rotating the rotary drum at 1 to 5 rpm for 5 to 10 min, with the cover of the drum open or closed.SELECTED DRAWING: Figure 3 【課題】造粒工程や造粒装置が簡素で、得られた造粒物の粒度分布が狭い石炭灰造粒物を製造する方法を提供する。【解決手段】開閉自在な蓋を有する回転ドラムを有する造粒機を用いて石炭灰造粒物を製造する方法。(A)回転ドラムの蓋のある面を上面にして、垂直から0〜45°の傾斜角を有する回転ドラム内に、少なくとも石炭灰および結合材を含む粉体を投入した後、蓋を閉めて回転させて予め混合する、予備的混合工程、(B)回転ドラムの蓋を開けた状態で、回転ドラムの蓋のある面を上面にして、垂直から5〜45°の傾斜角を有する回転ドラムを15〜20rpmで25〜30分間回転させながら、回転ドラム内に断続的に加水して造粒核を作製する、造粒核作製工程、(C)回転ドラムの蓋を開けた状態、または閉めた状態で、回転ドラムを1〜5rpmで5〜10分間回転させながら、造粒物の粒径を調整する、粒径調整工程を含む。【選択図】図3</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2020037226A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
PREPARING CLAY
PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL,e.g. PLASTER
REFRACTORIES
SLAG
THEIR RELEVANT APPARATUS
TRANSPORTING
TREATMENT OF NATURAL STONE
WORKING CEMENT, CLAY, OR STONE
title METHOD FOR PRODUCING COAL ASH GRANULE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T10%3A56%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KOBAYAKAWA%20MAKOTO&rft.date=2020-03-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2020037226A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true