ROAD REPAIRING MATERIAL

To provide a road repairing material which has rapid hardening property, excellent strength development in a short period of time, and good long-term stability.SOLUTION: (1) The road repairing material includes a cement, calcium aluminate having a vitrification rate of 70% or more, a CaO/AlOmolar ra...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SASAKI TAKASHI, TERAJIMA ISAO, KASAHARA MISATO, TERASAKI SEIICHI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SASAKI TAKASHI
TERAJIMA ISAO
KASAHARA MISATO
TERASAKI SEIICHI
description To provide a road repairing material which has rapid hardening property, excellent strength development in a short period of time, and good long-term stability.SOLUTION: (1) The road repairing material includes a cement, calcium aluminate having a vitrification rate of 70% or more, a CaO/AlOmolar ratio of 1.5 to 2.3, and a Blaine specific surface area of 3000 cm/g or more, gypsum, alkaline earth metal hydroxide, a plasticizer, a premixed material comprising inorganic fine powder and an aggregate, and a polymer latex. (2) A repairing method is characterized in providing a partition in one bag in which the premixed material and the polymer latex of (1) are separately filled, mixing the premixed material and the polymer latex by removing the partition immediately before using, and filling the material in a repair spot of a road.SELECTED DRAWING: None 【課題】 速硬性で短時間の強度発現性に優れ、長期安定性の良好な道路補修材を提供する。【解決手段】(1)セメント、ガラス化率が70%以上、CaO/Al2O3モル比が1.5〜2.3、ブレーン比表面積が3000cm2/g以上であるカルシウムアルミネート、石膏、アルカリ土類金属水酸化物、可塑剤、無機微粉末及び骨材を含有してなるプレミックス材料、並びに、ポリマーラテックスからなる道路補修材(2)さらに、一つの袋の中に仕切りを設けて、(1)のプレミックス材料とポリマーラテックスを別々に詰め、使用する直前に前記仕切りを外して混合し、道路の補修箇所に充填することを特徴とする補修方法。【選択図】 なし
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2019011231A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2019011231A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2019011231A3</originalsourceid><addsrcrecordid>eNrjZBAP8nd0UQhyDXD0DPL0c1fwdQxxDfJ09OFhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhpYGhoZGxoaOxkQpAgAGsR-w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ROAD REPAIRING MATERIAL</title><source>esp@cenet</source><creator>SASAKI TAKASHI ; TERAJIMA ISAO ; KASAHARA MISATO ; TERASAKI SEIICHI</creator><creatorcontrib>SASAKI TAKASHI ; TERAJIMA ISAO ; KASAHARA MISATO ; TERASAKI SEIICHI</creatorcontrib><description>To provide a road repairing material which has rapid hardening property, excellent strength development in a short period of time, and good long-term stability.SOLUTION: (1) The road repairing material includes a cement, calcium aluminate having a vitrification rate of 70% or more, a CaO/AlOmolar ratio of 1.5 to 2.3, and a Blaine specific surface area of 3000 cm/g or more, gypsum, alkaline earth metal hydroxide, a plasticizer, a premixed material comprising inorganic fine powder and an aggregate, and a polymer latex. (2) A repairing method is characterized in providing a partition in one bag in which the premixed material and the polymer latex of (1) are separately filled, mixing the premixed material and the polymer latex by removing the partition immediately before using, and filling the material in a repair spot of a road.SELECTED DRAWING: None 【課題】 速硬性で短時間の強度発現性に優れ、長期安定性の良好な道路補修材を提供する。【解決手段】(1)セメント、ガラス化率が70%以上、CaO/Al2O3モル比が1.5〜2.3、ブレーン比表面積が3000cm2/g以上であるカルシウムアルミネート、石膏、アルカリ土類金属水酸化物、可塑剤、無機微粉末及び骨材を含有してなるプレミックス材料、並びに、ポリマーラテックスからなる道路補修材(2)さらに、一つの袋の中に仕切りを設けて、(1)のプレミックス材料とポリマーラテックスを別々に詰め、使用する直前に前記仕切りを外して混合し、道路の補修箇所に充填することを特徴とする補修方法。【選択図】 なし</description><language>eng ; jpn</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES ; CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE ; FIXED CONSTRUCTIONS ; LIME, MAGNESIA ; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190124&amp;DB=EPODOC&amp;CC=JP&amp;NR=2019011231A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190124&amp;DB=EPODOC&amp;CC=JP&amp;NR=2019011231A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SASAKI TAKASHI</creatorcontrib><creatorcontrib>TERAJIMA ISAO</creatorcontrib><creatorcontrib>KASAHARA MISATO</creatorcontrib><creatorcontrib>TERASAKI SEIICHI</creatorcontrib><title>ROAD REPAIRING MATERIAL</title><description>To provide a road repairing material which has rapid hardening property, excellent strength development in a short period of time, and good long-term stability.SOLUTION: (1) The road repairing material includes a cement, calcium aluminate having a vitrification rate of 70% or more, a CaO/AlOmolar ratio of 1.5 to 2.3, and a Blaine specific surface area of 3000 cm/g or more, gypsum, alkaline earth metal hydroxide, a plasticizer, a premixed material comprising inorganic fine powder and an aggregate, and a polymer latex. (2) A repairing method is characterized in providing a partition in one bag in which the premixed material and the polymer latex of (1) are separately filled, mixing the premixed material and the polymer latex by removing the partition immediately before using, and filling the material in a repair spot of a road.SELECTED DRAWING: None 【課題】 速硬性で短時間の強度発現性に優れ、長期安定性の良好な道路補修材を提供する。【解決手段】(1)セメント、ガラス化率が70%以上、CaO/Al2O3モル比が1.5〜2.3、ブレーン比表面積が3000cm2/g以上であるカルシウムアルミネート、石膏、アルカリ土類金属水酸化物、可塑剤、無機微粉末及び骨材を含有してなるプレミックス材料、並びに、ポリマーラテックスからなる道路補修材(2)さらに、一つの袋の中に仕切りを設けて、(1)のプレミックス材料とポリマーラテックスを別々に詰め、使用する直前に前記仕切りを外して混合し、道路の補修箇所に充填することを特徴とする補修方法。【選択図】 なし</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</subject><subject>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</subject><subject>FIXED CONSTRUCTIONS</subject><subject>LIME, MAGNESIA</subject><subject>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBAP8nd0UQhyDXD0DPL0c1fwdQxxDfJ09OFhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhpYGhoZGxoaOxkQpAgAGsR-w</recordid><startdate>20190124</startdate><enddate>20190124</enddate><creator>SASAKI TAKASHI</creator><creator>TERAJIMA ISAO</creator><creator>KASAHARA MISATO</creator><creator>TERASAKI SEIICHI</creator><scope>EVB</scope></search><sort><creationdate>20190124</creationdate><title>ROAD REPAIRING MATERIAL</title><author>SASAKI TAKASHI ; TERAJIMA ISAO ; KASAHARA MISATO ; TERASAKI SEIICHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2019011231A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2019</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</topic><topic>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</topic><topic>FIXED CONSTRUCTIONS</topic><topic>LIME, MAGNESIA</topic><topic>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SASAKI TAKASHI</creatorcontrib><creatorcontrib>TERAJIMA ISAO</creatorcontrib><creatorcontrib>KASAHARA MISATO</creatorcontrib><creatorcontrib>TERASAKI SEIICHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SASAKI TAKASHI</au><au>TERAJIMA ISAO</au><au>KASAHARA MISATO</au><au>TERASAKI SEIICHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ROAD REPAIRING MATERIAL</title><date>2019-01-24</date><risdate>2019</risdate><abstract>To provide a road repairing material which has rapid hardening property, excellent strength development in a short period of time, and good long-term stability.SOLUTION: (1) The road repairing material includes a cement, calcium aluminate having a vitrification rate of 70% or more, a CaO/AlOmolar ratio of 1.5 to 2.3, and a Blaine specific surface area of 3000 cm/g or more, gypsum, alkaline earth metal hydroxide, a plasticizer, a premixed material comprising inorganic fine powder and an aggregate, and a polymer latex. (2) A repairing method is characterized in providing a partition in one bag in which the premixed material and the polymer latex of (1) are separately filled, mixing the premixed material and the polymer latex by removing the partition immediately before using, and filling the material in a repair spot of a road.SELECTED DRAWING: None 【課題】 速硬性で短時間の強度発現性に優れ、長期安定性の良好な道路補修材を提供する。【解決手段】(1)セメント、ガラス化率が70%以上、CaO/Al2O3モル比が1.5〜2.3、ブレーン比表面積が3000cm2/g以上であるカルシウムアルミネート、石膏、アルカリ土類金属水酸化物、可塑剤、無機微粉末及び骨材を含有してなるプレミックス材料、並びに、ポリマーラテックスからなる道路補修材(2)さらに、一つの袋の中に仕切りを設けて、(1)のプレミックス材料とポリマーラテックスを別々に詰め、使用する直前に前記仕切りを外して混合し、道路の補修箇所に充填することを特徴とする補修方法。【選択図】 なし</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2019011231A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE
FIXED CONSTRUCTIONS
LIME, MAGNESIA
MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title ROAD REPAIRING MATERIAL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T13%3A55%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SASAKI%20TAKASHI&rft.date=2019-01-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2019011231A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true