PORTLAND CEMENT CLINKER

PROBLEM TO BE SOLVED: To provide a cement and a hydraulic composition which can be fired at low temperature, can increase an amount of an AlO-containing waste to be used, has better fluidity than conventional one, and has good strength development property.SOLUTION: There are provided a cement and a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: SABAYASHI TAKASHI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SABAYASHI TAKASHI
description PROBLEM TO BE SOLVED: To provide a cement and a hydraulic composition which can be fired at low temperature, can increase an amount of an AlO-containing waste to be used, has better fluidity than conventional one, and has good strength development property.SOLUTION: There are provided a cement and a hydraulic composition in which the total amount of CA and CAF which are obtained by calculating a mineral composition of a clinker by Bogue equation is 24% or more, a CS amount is 60-63%, a CS amount is 8-11%, and an iron ratio (I.M) is 1.3 or less, and fluidity and strength development property are excellent. The hydraulic composition desirably has gypsum added thereto, and preferably contains 1-25% of limestone in the total composition.SELECTED DRAWING: None 【課題】低温で焼成することが可能で、Al2O3含有廃棄物の使用量も多くでき、かつ、従来よりもいっそう流動性が良好で、さらには強度発現性が良好なセメントや水硬性組成物の提供。【解決手段】クリンカーの鉱物組成をボーグ式により算出されたC3AおよびC4AFの合計量が24%以上、C3S量が60〜63%、C2S量が8〜11%であり、かつ鉄率(I.M)が1.3以下とする流動性および強度発現性が良好なセメントや水硬性組成物。望ましくは、石こうが加られ、さらには、石灰石を全組成物あたり、1〜25%含むことが好ましい、水硬性組成物。【選択図】なし
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2018158861A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2018158861A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2018158861A3</originalsourceid><addsrcrecordid>eNrjZBAP8A8K8XH0c1FwdvV19QtRcPbx9PN2DeJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhhaGphYWZoaOxkQpAgASsh_q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PORTLAND CEMENT CLINKER</title><source>esp@cenet</source><creator>SABAYASHI TAKASHI</creator><creatorcontrib>SABAYASHI TAKASHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a cement and a hydraulic composition which can be fired at low temperature, can increase an amount of an AlO-containing waste to be used, has better fluidity than conventional one, and has good strength development property.SOLUTION: There are provided a cement and a hydraulic composition in which the total amount of CA and CAF which are obtained by calculating a mineral composition of a clinker by Bogue equation is 24% or more, a CS amount is 60-63%, a CS amount is 8-11%, and an iron ratio (I.M) is 1.3 or less, and fluidity and strength development property are excellent. The hydraulic composition desirably has gypsum added thereto, and preferably contains 1-25% of limestone in the total composition.SELECTED DRAWING: None 【課題】低温で焼成することが可能で、Al2O3含有廃棄物の使用量も多くでき、かつ、従来よりもいっそう流動性が良好で、さらには強度発現性が良好なセメントや水硬性組成物の提供。【解決手段】クリンカーの鉱物組成をボーグ式により算出されたC3AおよびC4AFの合計量が24%以上、C3S量が60〜63%、C2S量が8〜11%であり、かつ鉄率(I.M)が1.3以下とする流動性および強度発現性が良好なセメントや水硬性組成物。望ましくは、石こうが加られ、さらには、石灰石を全組成物あたり、1〜25%含むことが好ましい、水硬性組成物。【選択図】なし</description><language>eng ; jpn</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181011&amp;DB=EPODOC&amp;CC=JP&amp;NR=2018158861A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181011&amp;DB=EPODOC&amp;CC=JP&amp;NR=2018158861A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SABAYASHI TAKASHI</creatorcontrib><title>PORTLAND CEMENT CLINKER</title><description>PROBLEM TO BE SOLVED: To provide a cement and a hydraulic composition which can be fired at low temperature, can increase an amount of an AlO-containing waste to be used, has better fluidity than conventional one, and has good strength development property.SOLUTION: There are provided a cement and a hydraulic composition in which the total amount of CA and CAF which are obtained by calculating a mineral composition of a clinker by Bogue equation is 24% or more, a CS amount is 60-63%, a CS amount is 8-11%, and an iron ratio (I.M) is 1.3 or less, and fluidity and strength development property are excellent. The hydraulic composition desirably has gypsum added thereto, and preferably contains 1-25% of limestone in the total composition.SELECTED DRAWING: None 【課題】低温で焼成することが可能で、Al2O3含有廃棄物の使用量も多くでき、かつ、従来よりもいっそう流動性が良好で、さらには強度発現性が良好なセメントや水硬性組成物の提供。【解決手段】クリンカーの鉱物組成をボーグ式により算出されたC3AおよびC4AFの合計量が24%以上、C3S量が60〜63%、C2S量が8〜11%であり、かつ鉄率(I.M)が1.3以下とする流動性および強度発現性が良好なセメントや水硬性組成物。望ましくは、石こうが加られ、さらには、石灰石を全組成物あたり、1〜25%含むことが好ましい、水硬性組成物。【選択図】なし</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBAP8A8K8XH0c1FwdvV19QtRcPbx9PN2DeJhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhhaGphYWZoaOxkQpAgASsh_q</recordid><startdate>20181011</startdate><enddate>20181011</enddate><creator>SABAYASHI TAKASHI</creator><scope>EVB</scope></search><sort><creationdate>20181011</creationdate><title>PORTLAND CEMENT CLINKER</title><author>SABAYASHI TAKASHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2018158861A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2018</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>SABAYASHI TAKASHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SABAYASHI TAKASHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PORTLAND CEMENT CLINKER</title><date>2018-10-11</date><risdate>2018</risdate><abstract>PROBLEM TO BE SOLVED: To provide a cement and a hydraulic composition which can be fired at low temperature, can increase an amount of an AlO-containing waste to be used, has better fluidity than conventional one, and has good strength development property.SOLUTION: There are provided a cement and a hydraulic composition in which the total amount of CA and CAF which are obtained by calculating a mineral composition of a clinker by Bogue equation is 24% or more, a CS amount is 60-63%, a CS amount is 8-11%, and an iron ratio (I.M) is 1.3 or less, and fluidity and strength development property are excellent. The hydraulic composition desirably has gypsum added thereto, and preferably contains 1-25% of limestone in the total composition.SELECTED DRAWING: None 【課題】低温で焼成することが可能で、Al2O3含有廃棄物の使用量も多くでき、かつ、従来よりもいっそう流動性が良好で、さらには強度発現性が良好なセメントや水硬性組成物の提供。【解決手段】クリンカーの鉱物組成をボーグ式により算出されたC3AおよびC4AFの合計量が24%以上、C3S量が60〜63%、C2S量が8〜11%であり、かつ鉄率(I.M)が1.3以下とする流動性および強度発現性が良好なセメントや水硬性組成物。望ましくは、石こうが加られ、さらには、石灰石を全組成物あたり、1〜25%含むことが好ましい、水硬性組成物。【選択図】なし</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2018158861A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title PORTLAND CEMENT CLINKER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T01%3A54%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SABAYASHI%20TAKASHI&rft.date=2018-10-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2018158861A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true