Cu-CONTAINING LOW ALLOY STEEL EXCELLENT IN STRENGTH-LOW TEMPERATURE TOUGHNESS AND MANUFACTURING METHOD THEREFOR

PROBLEM TO BE SOLVED: To provide a Cu-containing low alloy steel excellent in balance of strength and low temperature toughness.SOLUTION: A Cu-containing low alloy steel has a chemical composition containing, by mass%, C:0.01-0.08%, Si:0.10-0.40%, Mn:0.80-1.80%, Ni:0.80-2.50%, Cr:0.50-1.00%, Cu:0.80...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HONMA YUTA, SASAKI HAJIME, UNO KOKICHI, KAYANO RINZO, HASHI KUNIHIKO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a Cu-containing low alloy steel excellent in balance of strength and low temperature toughness.SOLUTION: A Cu-containing low alloy steel has a chemical composition containing, by mass%, C:0.01-0.08%, Si:0.10-0.40%, Mn:0.80-1.80%, Ni:0.80-2.50%, Cr:0.50-1.00%, Cu:0.80-1.50%, Mo:0.20-0.60%, Al:0.010-0.050%, Nb:0.030-0.080%, N:0.005-0.020% and further if desired, Ca:0.010% or less and the balance Fe with inevitable impurities, 0.2% bearing force of 525 MPa or more and a fracture appearance transition temperature (FATT) measured by 2 mmV notch Charpy impact test of -70°C or less.SELECTED DRAWING: Figure 1 【課題】強度と低温靱性のバランスに優れたCu含有低合金鋼を提供する。【解決手段】Cu含有低合金鋼は、質量%で、C:0.01〜0.08%、Si:0.10〜0.40%、Mn:0.80〜1.80%、Ni:0.80〜2.50%、Cr:0.50〜1.00%、Cu:0.80〜1.50%、Mo:0.20〜0.60%、Al:0.010〜0.050%、Nb:0.030〜0.080%、N:0.005〜0.020%を含有し、さらに、所望によりCa:0.010%以下を含有し、残部がFe及び不可避不純物からなる化学組成を有し、0.2%耐力が525MPa以上で、かつ2mmVノッチシャルピー衝撃試験にて測定された延性脆性破面遷移温度(FATT)が−70℃以下を有する。【選択図】図1