METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL
PROBLEM TO BE SOLVED: To provide a method for conversion of waste plastic to oil that has a sufficiently high rate of conversion to oil.SOLUTION: A method for conversion of waste plastic to oil according to the present invention includes the steps of: feeding crushed waste plastic as a raw material...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YUKIMOTO MASAO TANI HARUKI |
description | PROBLEM TO BE SOLVED: To provide a method for conversion of waste plastic to oil that has a sufficiently high rate of conversion to oil.SOLUTION: A method for conversion of waste plastic to oil according to the present invention includes the steps of: feeding crushed waste plastic as a raw material into iron pyroligneous acid 7 as a heat medium preheated to a temperature range of 350-500°C in a reactor 1; mixing the waste plastic into the iron pyroligneous acid 7 by stirring means 3 and decomposing the waste plastic by the high-temperature iron pyroligneous acid 7 on a contact surface with the iron pyroligneous acid 7 to produce cracked gas; and cooling the cracked gas to produce cracked oil.SELECTED DRAWING: Figure 1
【課題】油化率が十分に高い廃プラスチックの油化方法を提供すること。【解決手段】本発明の廃プラスチックの油化方法は、反応器1内で350℃〜500℃の温度域に予め加熱した熱媒体としての木酢酸鉄液7に破砕した廃プラスチックを原料として投入する工程と、撹拌手段3によって木酢酸鉄液7中に前記廃プラスチックを混合し、前記廃プラスチックを木酢酸鉄液7との接触面において高温の木酢酸鉄液7によって分解させて分解ガスを生成する工程と、前記分解ガスを冷却し分解油を生成する工程と、を備えることを特徴とする方法である。【選択図】図1 |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2016023240A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2016023240A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2016023240A3</originalsourceid><addsrcrecordid>eNrjZND1dQ3x8HdRcPMPUnD29wtzDQr29PdT8HdTCHcMDnFVCPABUp7OCiH-Cv6ePjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjA0MzAyNjIxMDRmChFAPjkJa4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL</title><source>esp@cenet</source><creator>YUKIMOTO MASAO ; TANI HARUKI</creator><creatorcontrib>YUKIMOTO MASAO ; TANI HARUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for conversion of waste plastic to oil that has a sufficiently high rate of conversion to oil.SOLUTION: A method for conversion of waste plastic to oil according to the present invention includes the steps of: feeding crushed waste plastic as a raw material into iron pyroligneous acid 7 as a heat medium preheated to a temperature range of 350-500°C in a reactor 1; mixing the waste plastic into the iron pyroligneous acid 7 by stirring means 3 and decomposing the waste plastic by the high-temperature iron pyroligneous acid 7 on a contact surface with the iron pyroligneous acid 7 to produce cracked gas; and cooling the cracked gas to produce cracked oil.SELECTED DRAWING: Figure 1
【課題】油化率が十分に高い廃プラスチックの油化方法を提供すること。【解決手段】本発明の廃プラスチックの油化方法は、反応器1内で350℃〜500℃の温度域に予め加熱した熱媒体としての木酢酸鉄液7に破砕した廃プラスチックを原料として投入する工程と、撹拌手段3によって木酢酸鉄液7中に前記廃プラスチックを混合し、前記廃プラスチックを木酢酸鉄液7との接触面において高温の木酢酸鉄液7によって分解させて分解ガスを生成する工程と、前記分解ガスを冷却し分解油を生成する工程と、を備えることを特徴とする方法である。【選択図】図1</description><language>eng ; jpn</language><subject>CHEMISTRY ; CRACKING HYDROCARBON OILS ; FUELS ; LUBRICANTS ; METALLURGY ; MINERAL WAXES ; PEAT ; PETROLEUM, GAS OR COKE INDUSTRIES ; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION ; RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES ; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS ; REFORMING OF NAPHTHA ; TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160208&DB=EPODOC&CC=JP&NR=2016023240A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160208&DB=EPODOC&CC=JP&NR=2016023240A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YUKIMOTO MASAO</creatorcontrib><creatorcontrib>TANI HARUKI</creatorcontrib><title>METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL</title><description>PROBLEM TO BE SOLVED: To provide a method for conversion of waste plastic to oil that has a sufficiently high rate of conversion to oil.SOLUTION: A method for conversion of waste plastic to oil according to the present invention includes the steps of: feeding crushed waste plastic as a raw material into iron pyroligneous acid 7 as a heat medium preheated to a temperature range of 350-500°C in a reactor 1; mixing the waste plastic into the iron pyroligneous acid 7 by stirring means 3 and decomposing the waste plastic by the high-temperature iron pyroligneous acid 7 on a contact surface with the iron pyroligneous acid 7 to produce cracked gas; and cooling the cracked gas to produce cracked oil.SELECTED DRAWING: Figure 1
【課題】油化率が十分に高い廃プラスチックの油化方法を提供すること。【解決手段】本発明の廃プラスチックの油化方法は、反応器1内で350℃〜500℃の温度域に予め加熱した熱媒体としての木酢酸鉄液7に破砕した廃プラスチックを原料として投入する工程と、撹拌手段3によって木酢酸鉄液7中に前記廃プラスチックを混合し、前記廃プラスチックを木酢酸鉄液7との接触面において高温の木酢酸鉄液7によって分解させて分解ガスを生成する工程と、前記分解ガスを冷却し分解油を生成する工程と、を備えることを特徴とする方法である。【選択図】図1</description><subject>CHEMISTRY</subject><subject>CRACKING HYDROCARBON OILS</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>MINERAL WAXES</subject><subject>PEAT</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION</subject><subject>RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES</subject><subject>REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS</subject><subject>REFORMING OF NAPHTHA</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND1dQ3x8HdRcPMPUnD29wtzDQr29PdT8HdTCHcMDnFVCPABUp7OCiH-Cv6ePjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjA0MzAyNjIxMDRmChFAPjkJa4</recordid><startdate>20160208</startdate><enddate>20160208</enddate><creator>YUKIMOTO MASAO</creator><creator>TANI HARUKI</creator><scope>EVB</scope></search><sort><creationdate>20160208</creationdate><title>METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL</title><author>YUKIMOTO MASAO ; TANI HARUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2016023240A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2016</creationdate><topic>CHEMISTRY</topic><topic>CRACKING HYDROCARBON OILS</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>MINERAL WAXES</topic><topic>PEAT</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION</topic><topic>RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES</topic><topic>REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS</topic><topic>REFORMING OF NAPHTHA</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><toplevel>online_resources</toplevel><creatorcontrib>YUKIMOTO MASAO</creatorcontrib><creatorcontrib>TANI HARUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YUKIMOTO MASAO</au><au>TANI HARUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL</title><date>2016-02-08</date><risdate>2016</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for conversion of waste plastic to oil that has a sufficiently high rate of conversion to oil.SOLUTION: A method for conversion of waste plastic to oil according to the present invention includes the steps of: feeding crushed waste plastic as a raw material into iron pyroligneous acid 7 as a heat medium preheated to a temperature range of 350-500°C in a reactor 1; mixing the waste plastic into the iron pyroligneous acid 7 by stirring means 3 and decomposing the waste plastic by the high-temperature iron pyroligneous acid 7 on a contact surface with the iron pyroligneous acid 7 to produce cracked gas; and cooling the cracked gas to produce cracked oil.SELECTED DRAWING: Figure 1
【課題】油化率が十分に高い廃プラスチックの油化方法を提供すること。【解決手段】本発明の廃プラスチックの油化方法は、反応器1内で350℃〜500℃の温度域に予め加熱した熱媒体としての木酢酸鉄液7に破砕した廃プラスチックを原料として投入する工程と、撹拌手段3によって木酢酸鉄液7中に前記廃プラスチックを混合し、前記廃プラスチックを木酢酸鉄液7との接触面において高温の木酢酸鉄液7によって分解させて分解ガスを生成する工程と、前記分解ガスを冷却し分解油を生成する工程と、を備えることを特徴とする方法である。【選択図】図1</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; jpn |
recordid | cdi_epo_espacenet_JP2016023240A |
source | esp@cenet |
subjects | CHEMISTRY CRACKING HYDROCARBON OILS FUELS LUBRICANTS METALLURGY MINERAL WAXES PEAT PETROLEUM, GAS OR COKE INDUSTRIES PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVEHYDROGENATION, OLIGOMERISATION, POLYMERISATION RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, ORGASES REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS REFORMING OF NAPHTHA TECHNICAL GASES CONTAINING CARBON MONOXIDE |
title | METHOD FOR CONVERSION OF WASTE PLASTIC TO OIL |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T00%3A26%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YUKIMOTO%20MASAO&rft.date=2016-02-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2016023240A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |