HIGH REFRACTIVE INDEX GLASS
PROBLEM TO BE SOLVED: To provide a high refractive index glass with a high liquid phase viscosity without containing a large amount of expensive heavy metal.SOLUTION: This high refractive index glass is characterized by containing, as a glass composition, 30-80% of SiO+AlO+BO, 0.1-20% of BO+ZnO, and...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YANASE TOMOMOTO MUSHIAKE ATSUSHI |
description | PROBLEM TO BE SOLVED: To provide a high refractive index glass with a high liquid phase viscosity without containing a large amount of expensive heavy metal.SOLUTION: This high refractive index glass is characterized by containing, as a glass composition, 30-80% of SiO+AlO+BO, 0.1-20% of BO+ZnO, and 3-20% of TiO+ZrOwith the refractive index (n) being 1.55 to 1.70.
【課題】高価な重金属を多量に含まなくても、液相粘度が高い高屈折率ガラスを創案する。【解決手段】本発明の高屈折率ガラスは、ガラス組成として、質量%で、SiO2+Al2O3+B2O330〜80%、B2O3+ZnO 0.1〜20%、TiO2+ZrO23〜20%を含有し、且つ屈折率ndが1.55〜1.70であることを特徴とする。【選択図】なし |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2015027927A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2015027927A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2015027927A3</originalsourceid><addsrcrecordid>eNrjZJD28HT3UAhydQtydA7xDHNV8PRzcY1QcPdxDA7mYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBoamBkbmlkbmjsZEKQIAgssg2Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>HIGH REFRACTIVE INDEX GLASS</title><source>esp@cenet</source><creator>YANASE TOMOMOTO ; MUSHIAKE ATSUSHI</creator><creatorcontrib>YANASE TOMOMOTO ; MUSHIAKE ATSUSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a high refractive index glass with a high liquid phase viscosity without containing a large amount of expensive heavy metal.SOLUTION: This high refractive index glass is characterized by containing, as a glass composition, 30-80% of SiO+AlO+BO, 0.1-20% of BO+ZnO, and 3-20% of TiO+ZrOwith the refractive index (n) being 1.55 to 1.70.
【課題】高価な重金属を多量に含まなくても、液相粘度が高い高屈折率ガラスを創案する。【解決手段】本発明の高屈折率ガラスは、ガラス組成として、質量%で、SiO2+Al2O3+B2O330〜80%、B2O3+ZnO 0.1〜20%、TiO2+ZrO23〜20%を含有し、且つ屈折率ndが1.55〜1.70であることを特徴とする。【選択図】なし</description><language>eng ; jpn</language><subject>BASIC ELECTRIC ELEMENTS ; CAPACITORS ; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE ; CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; ELECTRIC HEATING ; ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR ; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ; ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SEMICONDUCTOR DEVICES ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150212&DB=EPODOC&CC=JP&NR=2015027927A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150212&DB=EPODOC&CC=JP&NR=2015027927A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANASE TOMOMOTO</creatorcontrib><creatorcontrib>MUSHIAKE ATSUSHI</creatorcontrib><title>HIGH REFRACTIVE INDEX GLASS</title><description>PROBLEM TO BE SOLVED: To provide a high refractive index glass with a high liquid phase viscosity without containing a large amount of expensive heavy metal.SOLUTION: This high refractive index glass is characterized by containing, as a glass composition, 30-80% of SiO+AlO+BO, 0.1-20% of BO+ZnO, and 3-20% of TiO+ZrOwith the refractive index (n) being 1.55 to 1.70.
【課題】高価な重金属を多量に含まなくても、液相粘度が高い高屈折率ガラスを創案する。【解決手段】本発明の高屈折率ガラスは、ガラス組成として、質量%で、SiO2+Al2O3+B2O330〜80%、B2O3+ZnO 0.1〜20%、TiO2+ZrO23〜20%を含有し、且つ屈折率ndが1.55〜1.70であることを特徴とする。【選択図】なし</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CAPACITORS</subject><subject>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</subject><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>ELECTRIC HEATING</subject><subject>ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SEMICONDUCTOR DEVICES</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJD28HT3UAhydQtydA7xDHNV8PRzcY1QcPdxDA7mYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBoamBkbmlkbmjsZEKQIAgssg2Q</recordid><startdate>20150212</startdate><enddate>20150212</enddate><creator>YANASE TOMOMOTO</creator><creator>MUSHIAKE ATSUSHI</creator><scope>EVB</scope></search><sort><creationdate>20150212</creationdate><title>HIGH REFRACTIVE INDEX GLASS</title><author>YANASE TOMOMOTO ; MUSHIAKE ATSUSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2015027927A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2015</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CAPACITORS</topic><topic>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</topic><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>ELECTRIC HEATING</topic><topic>ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SEMICONDUCTOR DEVICES</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>YANASE TOMOMOTO</creatorcontrib><creatorcontrib>MUSHIAKE ATSUSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANASE TOMOMOTO</au><au>MUSHIAKE ATSUSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>HIGH REFRACTIVE INDEX GLASS</title><date>2015-02-12</date><risdate>2015</risdate><abstract>PROBLEM TO BE SOLVED: To provide a high refractive index glass with a high liquid phase viscosity without containing a large amount of expensive heavy metal.SOLUTION: This high refractive index glass is characterized by containing, as a glass composition, 30-80% of SiO+AlO+BO, 0.1-20% of BO+ZnO, and 3-20% of TiO+ZrOwith the refractive index (n) being 1.55 to 1.70.
【課題】高価な重金属を多量に含まなくても、液相粘度が高い高屈折率ガラスを創案する。【解決手段】本発明の高屈折率ガラスは、ガラス組成として、質量%で、SiO2+Al2O3+B2O330〜80%、B2O3+ZnO 0.1〜20%、TiO2+ZrO23〜20%を含有し、且つ屈折率ndが1.55〜1.70であることを特徴とする。【選択図】なし</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; jpn |
recordid | cdi_epo_espacenet_JP2015027927A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CAPACITORS CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY ELECTRIC HEATING ELECTRIC LIGHTING NOT OTHERWISE PROVIDED FOR ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR ELECTRICITY GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS METALLURGY MINERAL OR SLAG WOOL SEMICONDUCTOR DEVICES SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS |
title | HIGH REFRACTIVE INDEX GLASS |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T21%3A29%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANASE%20TOMOMOTO&rft.date=2015-02-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2015027927A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |