SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB

PROBLEM TO BE SOLVED: To provide a secondary cooling method of a continuous casting slab, in which occurrence of a surface crack (a corner crack) and an inner crack (a horizontal crack) is prevented by the cooling method of the slab only, without sacrificing productivity of a continuous casting appa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KAWANAMI SHUNICHI, MATSUBA TORU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KAWANAMI SHUNICHI
MATSUBA TORU
description PROBLEM TO BE SOLVED: To provide a secondary cooling method of a continuous casting slab, in which occurrence of a surface crack (a corner crack) and an inner crack (a horizontal crack) is prevented by the cooling method of the slab only, without sacrificing productivity of a continuous casting apparatus and without modifying a component system of the slab.SOLUTION: In a secondary cooling method of a continuous casting slab, width cutting not spraying secondary cooling water 25 is performed at both end parts of a long side 21a of an upper surface side of a cast slab 5 in at least a part of a casting segment from immediately after a bent part 13 to a solidification completion position in a continuous casting apparatus, whereas a total width including both end parts of the long side 21a of a lower surface side of the cast slab 5 is sprayed with the secondary cooling water 25 in the casting segment from immediately after the bent part 13 to the solidification completion position.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2014061527A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2014061527A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2014061527A3</originalsourceid><addsrcrecordid>eNrjZDAOdnX293NxDIpUcPb39_H0c1fwdQ3x8HdR8HcDiviFePqF-ocGKzg7BoeAJIN9HJ14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgaGJgZmhqZG5ozFRigD0FSeR</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB</title><source>esp@cenet</source><creator>KAWANAMI SHUNICHI ; MATSUBA TORU</creator><creatorcontrib>KAWANAMI SHUNICHI ; MATSUBA TORU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a secondary cooling method of a continuous casting slab, in which occurrence of a surface crack (a corner crack) and an inner crack (a horizontal crack) is prevented by the cooling method of the slab only, without sacrificing productivity of a continuous casting apparatus and without modifying a component system of the slab.SOLUTION: In a secondary cooling method of a continuous casting slab, width cutting not spraying secondary cooling water 25 is performed at both end parts of a long side 21a of an upper surface side of a cast slab 5 in at least a part of a casting segment from immediately after a bent part 13 to a solidification completion position in a continuous casting apparatus, whereas a total width including both end parts of the long side 21a of a lower surface side of the cast slab 5 is sprayed with the secondary cooling water 25 in the casting segment from immediately after the bent part 13 to the solidification completion position.</description><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140410&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014061527A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25546,76297</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140410&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014061527A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KAWANAMI SHUNICHI</creatorcontrib><creatorcontrib>MATSUBA TORU</creatorcontrib><title>SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB</title><description>PROBLEM TO BE SOLVED: To provide a secondary cooling method of a continuous casting slab, in which occurrence of a surface crack (a corner crack) and an inner crack (a horizontal crack) is prevented by the cooling method of the slab only, without sacrificing productivity of a continuous casting apparatus and without modifying a component system of the slab.SOLUTION: In a secondary cooling method of a continuous casting slab, width cutting not spraying secondary cooling water 25 is performed at both end parts of a long side 21a of an upper surface side of a cast slab 5 in at least a part of a casting segment from immediately after a bent part 13 to a solidification completion position in a continuous casting apparatus, whereas a total width including both end parts of the long side 21a of a lower surface side of the cast slab 5 is sprayed with the secondary cooling water 25 in the casting segment from immediately after the bent part 13 to the solidification completion position.</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAOdnX293NxDIpUcPb39_H0c1fwdQ3x8HdR8HcDiviFePqF-ocGKzg7BoeAJIN9HJ14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgaGJgZmhqZG5ozFRigD0FSeR</recordid><startdate>20140410</startdate><enddate>20140410</enddate><creator>KAWANAMI SHUNICHI</creator><creator>MATSUBA TORU</creator><scope>EVB</scope></search><sort><creationdate>20140410</creationdate><title>SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB</title><author>KAWANAMI SHUNICHI ; MATSUBA TORU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2014061527A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2014</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KAWANAMI SHUNICHI</creatorcontrib><creatorcontrib>MATSUBA TORU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KAWANAMI SHUNICHI</au><au>MATSUBA TORU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB</title><date>2014-04-10</date><risdate>2014</risdate><abstract>PROBLEM TO BE SOLVED: To provide a secondary cooling method of a continuous casting slab, in which occurrence of a surface crack (a corner crack) and an inner crack (a horizontal crack) is prevented by the cooling method of the slab only, without sacrificing productivity of a continuous casting apparatus and without modifying a component system of the slab.SOLUTION: In a secondary cooling method of a continuous casting slab, width cutting not spraying secondary cooling water 25 is performed at both end parts of a long side 21a of an upper surface side of a cast slab 5 in at least a part of a casting segment from immediately after a bent part 13 to a solidification completion position in a continuous casting apparatus, whereas a total width including both end parts of the long side 21a of a lower surface side of the cast slab 5 is sprayed with the secondary cooling water 25 in the casting segment from immediately after the bent part 13 to the solidification completion position.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2014061527A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title SECONDARY COOLING METHOD OF CONTINUOUS CASTING SLAB
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-17T09%3A39%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KAWANAMI%20SHUNICHI&rft.date=2014-04-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2014061527A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true