GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL

PROBLEM TO BE SOLVED: To provide a graphite negative electrode material for lithium secondary battery use which is high in tap density and less in fine powder amount, a manufacturing method thereof, and a negative electrode for lithium secondary battery use and a lithium secondary battery that are a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: UONO HIROYUKI, KAMATA TOMIYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator UONO HIROYUKI
KAMATA TOMIYUKI
description PROBLEM TO BE SOLVED: To provide a graphite negative electrode material for lithium secondary battery use which is high in tap density and less in fine powder amount, a manufacturing method thereof, and a negative electrode for lithium secondary battery use and a lithium secondary battery that are arranged by use of the graphite negative electrode material.SOLUTION: A method for manufacturing a graphite negative electrode material for lithium secondary battery use comprises the steps of: using a pitch material including 20 mass% or less of quinoline insoluble as a material to perform a thermal treatment of the material; conglobating the material subjected to the thermal treatment; baking the material subjected to the conglobation; and graphitizing the material subjected to the baking according to circumstances. In the graphite negative electrode material for lithium secondary battery use, the average circularity is 0.90 or larger; the average total number of particles is 3×10/g or less; the ratio (d/d) of a 90%-particle diameter to a 10%-particle diameter in a volume-based particle size distribution is 1.5-2.8; and the minimum particle diameter (d) is 3.5 μm or larger.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2014060168A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2014060168A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2014060168A3</originalsourceid><addsrcrecordid>eNqNjr0KwkAQhNNYiPoOi7VC_CHYbu72cifJXVg3glUQOStRQZ_XZzGopYLVMPB9w_STR8FYWycEngoUtyWgkpRw0AQVCrHDEtDrrvjGoJKGnS-gIrFBg1hiCmbyIr4smMBQOrGuqWBDKniNvIMcpRveQbOhl_ibEIsCyB3GjL4gDflbCwb-eT5Mesf96RZHnxwkY0Oi7DReL228XfeHeI73dl3P09kyzdJZtsLFX9ATxChWGA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL</title><source>esp@cenet</source><creator>UONO HIROYUKI ; KAMATA TOMIYUKI</creator><creatorcontrib>UONO HIROYUKI ; KAMATA TOMIYUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a graphite negative electrode material for lithium secondary battery use which is high in tap density and less in fine powder amount, a manufacturing method thereof, and a negative electrode for lithium secondary battery use and a lithium secondary battery that are arranged by use of the graphite negative electrode material.SOLUTION: A method for manufacturing a graphite negative electrode material for lithium secondary battery use comprises the steps of: using a pitch material including 20 mass% or less of quinoline insoluble as a material to perform a thermal treatment of the material; conglobating the material subjected to the thermal treatment; baking the material subjected to the conglobation; and graphitizing the material subjected to the baking according to circumstances. In the graphite negative electrode material for lithium secondary battery use, the average circularity is 0.90 or larger; the average total number of particles is 3×10/g or less; the ratio (d/d) of a 90%-particle diameter to a 10%-particle diameter in a volume-based particle size distribution is 1.5-2.8; and the minimum particle diameter (d) is 3.5 μm or larger.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS THEREOF ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140403&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014060168A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140403&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014060168A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>UONO HIROYUKI</creatorcontrib><creatorcontrib>KAMATA TOMIYUKI</creatorcontrib><title>GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL</title><description>PROBLEM TO BE SOLVED: To provide a graphite negative electrode material for lithium secondary battery use which is high in tap density and less in fine powder amount, a manufacturing method thereof, and a negative electrode for lithium secondary battery use and a lithium secondary battery that are arranged by use of the graphite negative electrode material.SOLUTION: A method for manufacturing a graphite negative electrode material for lithium secondary battery use comprises the steps of: using a pitch material including 20 mass% or less of quinoline insoluble as a material to perform a thermal treatment of the material; conglobating the material subjected to the thermal treatment; baking the material subjected to the conglobation; and graphitizing the material subjected to the baking according to circumstances. In the graphite negative electrode material for lithium secondary battery use, the average circularity is 0.90 or larger; the average total number of particles is 3×10/g or less; the ratio (d/d) of a 90%-particle diameter to a 10%-particle diameter in a volume-based particle size distribution is 1.5-2.8; and the minimum particle diameter (d) is 3.5 μm or larger.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjr0KwkAQhNNYiPoOi7VC_CHYbu72cifJXVg3glUQOStRQZ_XZzGopYLVMPB9w_STR8FYWycEngoUtyWgkpRw0AQVCrHDEtDrrvjGoJKGnS-gIrFBg1hiCmbyIr4smMBQOrGuqWBDKniNvIMcpRveQbOhl_ibEIsCyB3GjL4gDflbCwb-eT5Mesf96RZHnxwkY0Oi7DReL228XfeHeI73dl3P09kyzdJZtsLFX9ATxChWGA</recordid><startdate>20140403</startdate><enddate>20140403</enddate><creator>UONO HIROYUKI</creator><creator>KAMATA TOMIYUKI</creator><scope>EVB</scope></search><sort><creationdate>20140403</creationdate><title>GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL</title><author>UONO HIROYUKI ; KAMATA TOMIYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2014060168A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2014</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>UONO HIROYUKI</creatorcontrib><creatorcontrib>KAMATA TOMIYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>UONO HIROYUKI</au><au>KAMATA TOMIYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL</title><date>2014-04-03</date><risdate>2014</risdate><abstract>PROBLEM TO BE SOLVED: To provide a graphite negative electrode material for lithium secondary battery use which is high in tap density and less in fine powder amount, a manufacturing method thereof, and a negative electrode for lithium secondary battery use and a lithium secondary battery that are arranged by use of the graphite negative electrode material.SOLUTION: A method for manufacturing a graphite negative electrode material for lithium secondary battery use comprises the steps of: using a pitch material including 20 mass% or less of quinoline insoluble as a material to perform a thermal treatment of the material; conglobating the material subjected to the thermal treatment; baking the material subjected to the conglobation; and graphitizing the material subjected to the baking according to circumstances. In the graphite negative electrode material for lithium secondary battery use, the average circularity is 0.90 or larger; the average total number of particles is 3×10/g or less; the ratio (d/d) of a 90%-particle diameter to a 10%-particle diameter in a volume-based particle size distribution is 1.5-2.8; and the minimum particle diameter (d) is 3.5 μm or larger.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2014060168A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CHEMISTRY
COMPOUNDS THEREOF
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title GRAPHITE NEGATIVE ELECTRODE MATERIAL AND MANUFACTURING METHOD THEREOF, AND NEGATIVE ELECTRODE FOR LITHIUM SECONDARY BATTERY USE AND LITHIUM SECONDARY BATTERY THAT ARE ARRANGED BY USE OF GRAPHITE NEGATIVE ELECTRODE MATERIAL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T09%3A03%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=UONO%20HIROYUKI&rft.date=2014-04-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2014060168A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true