METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY

PROBLEM TO BE SOLVED: To provide a method for reducing the diameter of a metallic tube by spinning, by which flaring at the tube end which is actualized by thinning and higher reduction rate of the metallic tube to be a base stock and a shape defect phenomenon such as folded wrinkles and cracks, or...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KANO HIROTAKA, OZAKI YOSHIHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KANO HIROTAKA
OZAKI YOSHIHIRO
description PROBLEM TO BE SOLVED: To provide a method for reducing the diameter of a metallic tube by spinning, by which flaring at the tube end which is actualized by thinning and higher reduction rate of the metallic tube to be a base stock and a shape defect phenomenon such as folded wrinkles and cracks, or the like due to the flaring is prevented advantageously and simultaneously productivity is improved, in the method for reducing the diameter of the metallic tube by spinning, by which the diameter of the metallic tube is reduced by pushing a roll-shaped tool performing reciprocating movement in the axial direction of the metallic tube while revolving around the center axis of a metallic tube to be the base stock.SOLUTION: After reducing only the center part 10c in the axial direction of a metallic tube 10, by cutting the diameter reduced part 10c on a cutting line 10b and dividing it into two, two parts 11, 12 with the tube ends reduced in diameters are obtained without causing defects in a shape.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013244523A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013244523A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013244523A3</originalsourceid><addsrcrecordid>eNrjZHD1dQ3x8HdRcPMPUghydQl19vRzV3DxdAQKuwYpOEUqBAd4-vmBBMM9PJ09FDyDFdz9geo9_RTC_YO8HZ08fTxDInkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBobGRiYmpkbGjMVGKALwnLDk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY</title><source>esp@cenet</source><creator>KANO HIROTAKA ; OZAKI YOSHIHIRO</creator><creatorcontrib>KANO HIROTAKA ; OZAKI YOSHIHIRO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for reducing the diameter of a metallic tube by spinning, by which flaring at the tube end which is actualized by thinning and higher reduction rate of the metallic tube to be a base stock and a shape defect phenomenon such as folded wrinkles and cracks, or the like due to the flaring is prevented advantageously and simultaneously productivity is improved, in the method for reducing the diameter of the metallic tube by spinning, by which the diameter of the metallic tube is reduced by pushing a roll-shaped tool performing reciprocating movement in the axial direction of the metallic tube while revolving around the center axis of a metallic tube to be the base stock.SOLUTION: After reducing only the center part 10c in the axial direction of a metallic tube 10, by cutting the diameter reduced part 10c on a cutting line 10b and dividing it into two, two parts 11, 12 with the tube ends reduced in diameters are obtained without causing defects in a shape.</description><language>eng</language><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131209&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013244523A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25569,76552</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20131209&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013244523A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KANO HIROTAKA</creatorcontrib><creatorcontrib>OZAKI YOSHIHIRO</creatorcontrib><title>METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY</title><description>PROBLEM TO BE SOLVED: To provide a method for reducing the diameter of a metallic tube by spinning, by which flaring at the tube end which is actualized by thinning and higher reduction rate of the metallic tube to be a base stock and a shape defect phenomenon such as folded wrinkles and cracks, or the like due to the flaring is prevented advantageously and simultaneously productivity is improved, in the method for reducing the diameter of the metallic tube by spinning, by which the diameter of the metallic tube is reduced by pushing a roll-shaped tool performing reciprocating movement in the axial direction of the metallic tube while revolving around the center axis of a metallic tube to be the base stock.SOLUTION: After reducing only the center part 10c in the axial direction of a metallic tube 10, by cutting the diameter reduced part 10c on a cutting line 10b and dividing it into two, two parts 11, 12 with the tube ends reduced in diameters are obtained without causing defects in a shape.</description><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD1dQ3x8HdRcPMPUghydQl19vRzV3DxdAQKuwYpOEUqBAd4-vmBBMM9PJ09FDyDFdz9geo9_RTC_YO8HZ08fTxDInkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBobGRiYmpkbGjMVGKALwnLDk</recordid><startdate>20131209</startdate><enddate>20131209</enddate><creator>KANO HIROTAKA</creator><creator>OZAKI YOSHIHIRO</creator><scope>EVB</scope></search><sort><creationdate>20131209</creationdate><title>METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY</title><author>KANO HIROTAKA ; OZAKI YOSHIHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013244523A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>KANO HIROTAKA</creatorcontrib><creatorcontrib>OZAKI YOSHIHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KANO HIROTAKA</au><au>OZAKI YOSHIHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY</title><date>2013-12-09</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for reducing the diameter of a metallic tube by spinning, by which flaring at the tube end which is actualized by thinning and higher reduction rate of the metallic tube to be a base stock and a shape defect phenomenon such as folded wrinkles and cracks, or the like due to the flaring is prevented advantageously and simultaneously productivity is improved, in the method for reducing the diameter of the metallic tube by spinning, by which the diameter of the metallic tube is reduced by pushing a roll-shaped tool performing reciprocating movement in the axial direction of the metallic tube while revolving around the center axis of a metallic tube to be the base stock.SOLUTION: After reducing only the center part 10c in the axial direction of a metallic tube 10, by cutting the diameter reduced part 10c on a cutting line 10b and dividing it into two, two parts 11, 12 with the tube ends reduced in diameters are obtained without causing defects in a shape.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2013244523A
source esp@cenet
subjects MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL
title METHOD FOR REDUCING DIAMETER BY SPINNING WHICH IS GOOD IN WORKABILITY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-14T16%3A44%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KANO%20HIROTAKA&rft.date=2013-12-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013244523A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true