METHOD FOR PRODUCING MOLTEN STEEL

PROBLEM TO BE SOLVED: To provide a method for producing molten steel, by which the use amount of a temperature increasing agent can be decreased to a small amount in blowing in a converter even when the molten steel having a low P concentration is produced.SOLUTION: In a process of delivering molten...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NISHIGUCHI NORITAKA, TAKESHITA HIROAKI, OSHIMA KENJI, TAKAHASHI DAISUKE
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NISHIGUCHI NORITAKA
TAKESHITA HIROAKI
OSHIMA KENJI
TAKAHASHI DAISUKE
description PROBLEM TO BE SOLVED: To provide a method for producing molten steel, by which the use amount of a temperature increasing agent can be decreased to a small amount in blowing in a converter even when the molten steel having a low P concentration is produced.SOLUTION: In a process of delivering molten pig iron tapped from a blast furnace into a charging ladle from a blast furnace ladle or a torpedo car, a dephosphorization treated molten pig iron obtained by subjecting the molten pig iron to dephosphorization treatment and normal pig iron not subjected to dephosphorization treatment are mixed to obtain mixed pig iron having an Si concentration of 0.10 mass% or more and 0.50 mass% or less and a P concentration of 0.030 mass% or more and 0.100 mass% or less. The molten steel is produced in a condition where a use amount of a temperature increasing agent is small, by charging the mixed pig iron into a converter and adding the temperature increasing agent to perform blowing.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013133536A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013133536A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013133536A3</originalsourceid><addsrcrecordid>eNrjZFD0dQ3x8HdRcPMPUggI8ncJdfb0c1fw9fcJcfVTCA5xdfXhYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBobGhsbGpsZmjsZEKQIAV8YikQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING MOLTEN STEEL</title><source>esp@cenet</source><creator>NISHIGUCHI NORITAKA ; TAKESHITA HIROAKI ; OSHIMA KENJI ; TAKAHASHI DAISUKE</creator><creatorcontrib>NISHIGUCHI NORITAKA ; TAKESHITA HIROAKI ; OSHIMA KENJI ; TAKAHASHI DAISUKE</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for producing molten steel, by which the use amount of a temperature increasing agent can be decreased to a small amount in blowing in a converter even when the molten steel having a low P concentration is produced.SOLUTION: In a process of delivering molten pig iron tapped from a blast furnace into a charging ladle from a blast furnace ladle or a torpedo car, a dephosphorization treated molten pig iron obtained by subjecting the molten pig iron to dephosphorization treatment and normal pig iron not subjected to dephosphorization treatment are mixed to obtain mixed pig iron having an Si concentration of 0.10 mass% or more and 0.50 mass% or less and a P concentration of 0.030 mass% or more and 0.100 mass% or less. The molten steel is produced in a condition where a use amount of a temperature increasing agent is small, by charging the mixed pig iron into a converter and adding the temperature increasing agent to perform blowing.</description><language>eng</language><subject>CHEMISTRY ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130708&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013133536A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130708&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013133536A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NISHIGUCHI NORITAKA</creatorcontrib><creatorcontrib>TAKESHITA HIROAKI</creatorcontrib><creatorcontrib>OSHIMA KENJI</creatorcontrib><creatorcontrib>TAKAHASHI DAISUKE</creatorcontrib><title>METHOD FOR PRODUCING MOLTEN STEEL</title><description>PROBLEM TO BE SOLVED: To provide a method for producing molten steel, by which the use amount of a temperature increasing agent can be decreased to a small amount in blowing in a converter even when the molten steel having a low P concentration is produced.SOLUTION: In a process of delivering molten pig iron tapped from a blast furnace into a charging ladle from a blast furnace ladle or a torpedo car, a dephosphorization treated molten pig iron obtained by subjecting the molten pig iron to dephosphorization treatment and normal pig iron not subjected to dephosphorization treatment are mixed to obtain mixed pig iron having an Si concentration of 0.10 mass% or more and 0.50 mass% or less and a P concentration of 0.030 mass% or more and 0.100 mass% or less. The molten steel is produced in a condition where a use amount of a temperature increasing agent is small, by charging the mixed pig iron into a converter and adding the temperature increasing agent to perform blowing.</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD0dQ3x8HdRcPMPUggI8ncJdfb0c1fw9fcJcfVTCA5xdfXhYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBobGhsbGpsZmjsZEKQIAV8YikQ</recordid><startdate>20130708</startdate><enddate>20130708</enddate><creator>NISHIGUCHI NORITAKA</creator><creator>TAKESHITA HIROAKI</creator><creator>OSHIMA KENJI</creator><creator>TAKAHASHI DAISUKE</creator><scope>EVB</scope></search><sort><creationdate>20130708</creationdate><title>METHOD FOR PRODUCING MOLTEN STEEL</title><author>NISHIGUCHI NORITAKA ; TAKESHITA HIROAKI ; OSHIMA KENJI ; TAKAHASHI DAISUKE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013133536A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><toplevel>online_resources</toplevel><creatorcontrib>NISHIGUCHI NORITAKA</creatorcontrib><creatorcontrib>TAKESHITA HIROAKI</creatorcontrib><creatorcontrib>OSHIMA KENJI</creatorcontrib><creatorcontrib>TAKAHASHI DAISUKE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NISHIGUCHI NORITAKA</au><au>TAKESHITA HIROAKI</au><au>OSHIMA KENJI</au><au>TAKAHASHI DAISUKE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING MOLTEN STEEL</title><date>2013-07-08</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for producing molten steel, by which the use amount of a temperature increasing agent can be decreased to a small amount in blowing in a converter even when the molten steel having a low P concentration is produced.SOLUTION: In a process of delivering molten pig iron tapped from a blast furnace into a charging ladle from a blast furnace ladle or a torpedo car, a dephosphorization treated molten pig iron obtained by subjecting the molten pig iron to dephosphorization treatment and normal pig iron not subjected to dephosphorization treatment are mixed to obtain mixed pig iron having an Si concentration of 0.10 mass% or more and 0.50 mass% or less and a P concentration of 0.030 mass% or more and 0.100 mass% or less. The molten steel is produced in a condition where a use amount of a temperature increasing agent is small, by charging the mixed pig iron into a converter and adding the temperature increasing agent to perform blowing.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2013133536A
source esp@cenet
subjects CHEMISTRY
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
title METHOD FOR PRODUCING MOLTEN STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T09%3A20%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NISHIGUCHI%20NORITAKA&rft.date=2013-07-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013133536A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true