SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME

PROBLEM TO BE SOLVED: To provide spheroidal graphite cast iron in which a spheroidizing agent not containing rare-earth elements is used, and chilling at the thin thickness part can be restrained, and which has no internal defects.SOLUTION: In a ladle, the spheroidizing treatment is performed by con...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SATO TAKASHI, NISHIKAWA YUTAKA, KITAHARA MASAKAZU, IDEI HIROSHI, NARITA HIDEKAZU, TOKIYAMA TAKUYA, BABA TSUKASA, HORITANI TAKAO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SATO TAKASHI
NISHIKAWA YUTAKA
KITAHARA MASAKAZU
IDEI HIROSHI
NARITA HIDEKAZU
TOKIYAMA TAKUYA
BABA TSUKASA
HORITANI TAKAO
description PROBLEM TO BE SOLVED: To provide spheroidal graphite cast iron in which a spheroidizing agent not containing rare-earth elements is used, and chilling at the thin thickness part can be restrained, and which has no internal defects.SOLUTION: In a ladle, the spheroidizing treatment is performed by controlling the charging amount of the spheroidizing agent of an Fe-S-Mg-Ca based alloy which contains, by mass ratio, 3.0-6.0% Mg, 1.0-2.0% Ca, 0.5-3.5% Ba and ≤0.3% Al and which does not contain the rare-earth elements to 0.8-2.0%, by mass ratio, to molten iron, and also, an inoculation treatment is performed using an Fe-Si based inoculating agent, and thereafter, a melt-stream inoculation treatment is performed using an Fe-Si-Ca based inoculating agent to obtain the spheroidal graphite cast iron member composed of, by mass ratio, 3.0-4.5% C, 3.0-4.0% Si, 0.2-0.4% Mn, 0.006-0.020% S, 0.08-0.30% Cu, 0.020-0.040% Sn, 0.015-0.050% Mg, ≤0.03% Al, ≤0.01% Zn and the balance Fe with inevitable impurities, as the finish composition.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013133474A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013133474A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013133474A3</originalsourceid><addsrcrecordid>eNrjZHAPDvBwDfL3dHH0UXAPcgzw8AxxVXB2DA5R8Azy91PwdfV1cg1ScPRzUQgI8nd2DQ5WcPMPArFdQp09_dwVQjxcFYIdfV15GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgaGxobGxibmJozFRigAYpCy_</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME</title><source>esp@cenet</source><creator>SATO TAKASHI ; NISHIKAWA YUTAKA ; KITAHARA MASAKAZU ; IDEI HIROSHI ; NARITA HIDEKAZU ; TOKIYAMA TAKUYA ; BABA TSUKASA ; HORITANI TAKAO</creator><creatorcontrib>SATO TAKASHI ; NISHIKAWA YUTAKA ; KITAHARA MASAKAZU ; IDEI HIROSHI ; NARITA HIDEKAZU ; TOKIYAMA TAKUYA ; BABA TSUKASA ; HORITANI TAKAO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide spheroidal graphite cast iron in which a spheroidizing agent not containing rare-earth elements is used, and chilling at the thin thickness part can be restrained, and which has no internal defects.SOLUTION: In a ladle, the spheroidizing treatment is performed by controlling the charging amount of the spheroidizing agent of an Fe-S-Mg-Ca based alloy which contains, by mass ratio, 3.0-6.0% Mg, 1.0-2.0% Ca, 0.5-3.5% Ba and ≤0.3% Al and which does not contain the rare-earth elements to 0.8-2.0%, by mass ratio, to molten iron, and also, an inoculation treatment is performed using an Fe-Si based inoculating agent, and thereafter, a melt-stream inoculation treatment is performed using an Fe-Si-Ca based inoculating agent to obtain the spheroidal graphite cast iron member composed of, by mass ratio, 3.0-4.5% C, 3.0-4.0% Si, 0.2-0.4% Mn, 0.006-0.020% S, 0.08-0.30% Cu, 0.020-0.040% Sn, 0.015-0.050% Mg, ≤0.03% Al, ≤0.01% Zn and the balance Fe with inevitable impurities, as the finish composition.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130708&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013133474A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130708&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013133474A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SATO TAKASHI</creatorcontrib><creatorcontrib>NISHIKAWA YUTAKA</creatorcontrib><creatorcontrib>KITAHARA MASAKAZU</creatorcontrib><creatorcontrib>IDEI HIROSHI</creatorcontrib><creatorcontrib>NARITA HIDEKAZU</creatorcontrib><creatorcontrib>TOKIYAMA TAKUYA</creatorcontrib><creatorcontrib>BABA TSUKASA</creatorcontrib><creatorcontrib>HORITANI TAKAO</creatorcontrib><title>SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide spheroidal graphite cast iron in which a spheroidizing agent not containing rare-earth elements is used, and chilling at the thin thickness part can be restrained, and which has no internal defects.SOLUTION: In a ladle, the spheroidizing treatment is performed by controlling the charging amount of the spheroidizing agent of an Fe-S-Mg-Ca based alloy which contains, by mass ratio, 3.0-6.0% Mg, 1.0-2.0% Ca, 0.5-3.5% Ba and ≤0.3% Al and which does not contain the rare-earth elements to 0.8-2.0%, by mass ratio, to molten iron, and also, an inoculation treatment is performed using an Fe-Si based inoculating agent, and thereafter, a melt-stream inoculation treatment is performed using an Fe-Si-Ca based inoculating agent to obtain the spheroidal graphite cast iron member composed of, by mass ratio, 3.0-4.5% C, 3.0-4.0% Si, 0.2-0.4% Mn, 0.006-0.020% S, 0.08-0.30% Cu, 0.020-0.040% Sn, 0.015-0.050% Mg, ≤0.03% Al, ≤0.01% Zn and the balance Fe with inevitable impurities, as the finish composition.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAPDvBwDfL3dHH0UXAPcgzw8AxxVXB2DA5R8Azy91PwdfV1cg1ScPRzUQgI8nd2DQ5WcPMPArFdQp09_dwVQjxcFYIdfV15GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgaGxobGxibmJozFRigAYpCy_</recordid><startdate>20130708</startdate><enddate>20130708</enddate><creator>SATO TAKASHI</creator><creator>NISHIKAWA YUTAKA</creator><creator>KITAHARA MASAKAZU</creator><creator>IDEI HIROSHI</creator><creator>NARITA HIDEKAZU</creator><creator>TOKIYAMA TAKUYA</creator><creator>BABA TSUKASA</creator><creator>HORITANI TAKAO</creator><scope>EVB</scope></search><sort><creationdate>20130708</creationdate><title>SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME</title><author>SATO TAKASHI ; NISHIKAWA YUTAKA ; KITAHARA MASAKAZU ; IDEI HIROSHI ; NARITA HIDEKAZU ; TOKIYAMA TAKUYA ; BABA TSUKASA ; HORITANI TAKAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013133474A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SATO TAKASHI</creatorcontrib><creatorcontrib>NISHIKAWA YUTAKA</creatorcontrib><creatorcontrib>KITAHARA MASAKAZU</creatorcontrib><creatorcontrib>IDEI HIROSHI</creatorcontrib><creatorcontrib>NARITA HIDEKAZU</creatorcontrib><creatorcontrib>TOKIYAMA TAKUYA</creatorcontrib><creatorcontrib>BABA TSUKASA</creatorcontrib><creatorcontrib>HORITANI TAKAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SATO TAKASHI</au><au>NISHIKAWA YUTAKA</au><au>KITAHARA MASAKAZU</au><au>IDEI HIROSHI</au><au>NARITA HIDEKAZU</au><au>TOKIYAMA TAKUYA</au><au>BABA TSUKASA</au><au>HORITANI TAKAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME</title><date>2013-07-08</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide spheroidal graphite cast iron in which a spheroidizing agent not containing rare-earth elements is used, and chilling at the thin thickness part can be restrained, and which has no internal defects.SOLUTION: In a ladle, the spheroidizing treatment is performed by controlling the charging amount of the spheroidizing agent of an Fe-S-Mg-Ca based alloy which contains, by mass ratio, 3.0-6.0% Mg, 1.0-2.0% Ca, 0.5-3.5% Ba and ≤0.3% Al and which does not contain the rare-earth elements to 0.8-2.0%, by mass ratio, to molten iron, and also, an inoculation treatment is performed using an Fe-Si based inoculating agent, and thereafter, a melt-stream inoculation treatment is performed using an Fe-Si-Ca based inoculating agent to obtain the spheroidal graphite cast iron member composed of, by mass ratio, 3.0-4.5% C, 3.0-4.0% Si, 0.2-0.4% Mn, 0.006-0.020% S, 0.08-0.30% Cu, 0.020-0.040% Sn, 0.015-0.050% Mg, ≤0.03% Al, ≤0.01% Zn and the balance Fe with inevitable impurities, as the finish composition.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2013133474A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title SPHEROIDAL GRAPHITE CAST IRON MEMBER AND PROCESS FOR PRODUCING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T23%3A01%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SATO%20TAKASHI&rft.date=2013-07-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013133474A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true