AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN

PROBLEM TO BE SOLVED: To provide an aqueous polyurethane resin composition for a glass fiber sizing agent having excellent glass fiber sizing property, a glass fiber sizing agent using the same, glass fibers for a reinforced resin obtained by treatment with the glass fiber sizing agent, and a glass...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIMAMURA NOBUYUKI, KOSAKA TATSUMI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHIMAMURA NOBUYUKI
KOSAKA TATSUMI
description PROBLEM TO BE SOLVED: To provide an aqueous polyurethane resin composition for a glass fiber sizing agent having excellent glass fiber sizing property, a glass fiber sizing agent using the same, glass fibers for a reinforced resin obtained by treatment with the glass fiber sizing agent, and a glass fiber-reinforced resin having excellent mechanical strength.SOLUTION: The aqueous polyurethane resin composition is produced by dispersing an urethane resin, obtained by reacting an epoxy ester compound and polyisocyanate, in water with the use of an emulsifier. The epoxy ester compound includes a ricinoleic acid epoxy ester compound represented by general formula (1) as an essential component, where in formula, R is each independently H or 1-3C alkyl, and n is a number of 0-3.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013100194A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013100194A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013100194A3</originalsourceid><addsrcrecordid>eNqNjr0OgkAMx1kcjPoOjTMkoC6OBQqcgR7eHYMuhJhzMkqCT-iTCeqixsSp7f_jl46dG24rkpWGUua7SpHJkAkUacEQyaKUWhghGRKpIM1Ra0hESAq02AtOAVNi4wJy_NMFGRoUTDFUehBNRqCxIPetMfAfm6dIcH9FfeH5xgf8KzB1Rsfm1NnZa06ceUImyjzbXmrbtc3Bnu213pQLP1gGvh-sV7j8K3QHpUxOEg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN</title><source>esp@cenet</source><creator>SHIMAMURA NOBUYUKI ; KOSAKA TATSUMI</creator><creatorcontrib>SHIMAMURA NOBUYUKI ; KOSAKA TATSUMI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide an aqueous polyurethane resin composition for a glass fiber sizing agent having excellent glass fiber sizing property, a glass fiber sizing agent using the same, glass fibers for a reinforced resin obtained by treatment with the glass fiber sizing agent, and a glass fiber-reinforced resin having excellent mechanical strength.SOLUTION: The aqueous polyurethane resin composition is produced by dispersing an urethane resin, obtained by reacting an epoxy ester compound and polyisocyanate, in water with the use of an emulsifier. The epoxy ester compound includes a ricinoleic acid epoxy ester compound represented by general formula (1) as an essential component, where in formula, R is each independently H or 1-3C alkyl, and n is a number of 0-3.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; LAUNDERING ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; MINERAL OR SLAG WOOL ; ORGANIC MACROMOLECULAR COMPOUNDS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS ; TEXTILES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130523&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013100194A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130523&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013100194A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHIMAMURA NOBUYUKI</creatorcontrib><creatorcontrib>KOSAKA TATSUMI</creatorcontrib><title>AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN</title><description>PROBLEM TO BE SOLVED: To provide an aqueous polyurethane resin composition for a glass fiber sizing agent having excellent glass fiber sizing property, a glass fiber sizing agent using the same, glass fibers for a reinforced resin obtained by treatment with the glass fiber sizing agent, and a glass fiber-reinforced resin having excellent mechanical strength.SOLUTION: The aqueous polyurethane resin composition is produced by dispersing an urethane resin, obtained by reacting an epoxy ester compound and polyisocyanate, in water with the use of an emulsifier. The epoxy ester compound includes a ricinoleic acid epoxy ester compound represented by general formula (1) as an essential component, where in formula, R is each independently H or 1-3C alkyl, and n is a number of 0-3.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>LAUNDERING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><subject>TEXTILES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjr0OgkAMx1kcjPoOjTMkoC6OBQqcgR7eHYMuhJhzMkqCT-iTCeqixsSp7f_jl46dG24rkpWGUua7SpHJkAkUacEQyaKUWhghGRKpIM1Ra0hESAq02AtOAVNi4wJy_NMFGRoUTDFUehBNRqCxIPetMfAfm6dIcH9FfeH5xgf8KzB1Rsfm1NnZa06ceUImyjzbXmrbtc3Bnu213pQLP1gGvh-sV7j8K3QHpUxOEg</recordid><startdate>20130523</startdate><enddate>20130523</enddate><creator>SHIMAMURA NOBUYUKI</creator><creator>KOSAKA TATSUMI</creator><scope>EVB</scope></search><sort><creationdate>20130523</creationdate><title>AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN</title><author>SHIMAMURA NOBUYUKI ; KOSAKA TATSUMI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013100194A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>LAUNDERING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><topic>TEXTILES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SHIMAMURA NOBUYUKI</creatorcontrib><creatorcontrib>KOSAKA TATSUMI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHIMAMURA NOBUYUKI</au><au>KOSAKA TATSUMI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN</title><date>2013-05-23</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide an aqueous polyurethane resin composition for a glass fiber sizing agent having excellent glass fiber sizing property, a glass fiber sizing agent using the same, glass fibers for a reinforced resin obtained by treatment with the glass fiber sizing agent, and a glass fiber-reinforced resin having excellent mechanical strength.SOLUTION: The aqueous polyurethane resin composition is produced by dispersing an urethane resin, obtained by reacting an epoxy ester compound and polyisocyanate, in water with the use of an emulsifier. The epoxy ester compound includes a ricinoleic acid epoxy ester compound represented by general formula (1) as an essential component, where in formula, R is each independently H or 1-3C alkyl, and n is a number of 0-3.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2013100194A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
COMPOSITIONS BASED THEREON
FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
LAUNDERING
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
MINERAL OR SLAG WOOL
ORGANIC MACROMOLECULAR COMPOUNDS
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
TEXTILES
THEIR PREPARATION OR CHEMICAL WORKING-UP
TREATMENT OF TEXTILES OR THE LIKE
TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS
title AQUEOUS POLYURETHANE RESIN COMPOSITION FOR GLASS FIBER SIZING AGENT, AND GLASS FIBER SIZING AGENT OBTAINED USING THE SAME, GLASS FIBER FOR FIBER-REINFORCED RESIN AND GLASS FIBER-REINFORCED RESIN
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-10T12%3A26%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHIMAMURA%20NOBUYUKI&rft.date=2013-05-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013100194A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true