METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY

PROBLEM TO BE SOLVED: To provide a method for manufacturing a secondary battery which can be charged/discharged at high rate.SOLUTION: In the method for manufacturing a secondary battery, negative electrode slurry including a negative electrode active material, carboxymethyl cellulose (CMC) and styr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: AKITA HIROYUKI, MIO TAKUMI, ANDO KENSUKE, SUMI TOMOHIDE
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator AKITA HIROYUKI
MIO TAKUMI
ANDO KENSUKE
SUMI TOMOHIDE
description PROBLEM TO BE SOLVED: To provide a method for manufacturing a secondary battery which can be charged/discharged at high rate.SOLUTION: In the method for manufacturing a secondary battery, negative electrode slurry including a negative electrode active material, carboxymethyl cellulose (CMC) and styrene-butadiene rubber is imparted on a negative electrode collector and dried to form a negative electrode active material layer. The CMC has a weight average molecular weight of 30×10or more and 40×10or less. An amount of the CMC included in the negative electrode active material layer is in a range of 0.6-0.8 mass%. The negative electrode active material has an O/C value of 1.0 or less, the O/C value being a value of a ratio between an oxygen element and a carbon element and obtained by means of an X-ray photoelectron spectroscopy on a surface of a particle thereof.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013045714A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013045714A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013045714A3</originalsourceid><addsrcrecordid>eNrjZDD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8PP3cwwMdfUPDVYIdnX293NxDIpUcHIMCXENiuRhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhsYGJqbmhiaOxkQpAgBlOShz</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY</title><source>esp@cenet</source><creator>AKITA HIROYUKI ; MIO TAKUMI ; ANDO KENSUKE ; SUMI TOMOHIDE</creator><creatorcontrib>AKITA HIROYUKI ; MIO TAKUMI ; ANDO KENSUKE ; SUMI TOMOHIDE</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a secondary battery which can be charged/discharged at high rate.SOLUTION: In the method for manufacturing a secondary battery, negative electrode slurry including a negative electrode active material, carboxymethyl cellulose (CMC) and styrene-butadiene rubber is imparted on a negative electrode collector and dried to form a negative electrode active material layer. The CMC has a weight average molecular weight of 30×10or more and 40×10or less. An amount of the CMC included in the negative electrode active material layer is in a range of 0.6-0.8 mass%. The negative electrode active material has an O/C value of 1.0 or less, the O/C value being a value of a ratio between an oxygen element and a carbon element and obtained by means of an X-ray photoelectron spectroscopy on a surface of a particle thereof.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130304&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013045714A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130304&amp;DB=EPODOC&amp;CC=JP&amp;NR=2013045714A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>AKITA HIROYUKI</creatorcontrib><creatorcontrib>MIO TAKUMI</creatorcontrib><creatorcontrib>ANDO KENSUKE</creatorcontrib><creatorcontrib>SUMI TOMOHIDE</creatorcontrib><title>METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a secondary battery which can be charged/discharged at high rate.SOLUTION: In the method for manufacturing a secondary battery, negative electrode slurry including a negative electrode active material, carboxymethyl cellulose (CMC) and styrene-butadiene rubber is imparted on a negative electrode collector and dried to form a negative electrode active material layer. The CMC has a weight average molecular weight of 30×10or more and 40×10or less. An amount of the CMC included in the negative electrode active material layer is in a range of 0.6-0.8 mass%. The negative electrode active material has an O/C value of 1.0 or less, the O/C value being a value of a ratio between an oxygen element and a carbon element and obtained by means of an X-ray photoelectron spectroscopy on a surface of a particle thereof.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8PP3cwwMdfUPDVYIdnX293NxDIpUcHIMCXENiuRhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhsYGJqbmhiaOxkQpAgBlOShz</recordid><startdate>20130304</startdate><enddate>20130304</enddate><creator>AKITA HIROYUKI</creator><creator>MIO TAKUMI</creator><creator>ANDO KENSUKE</creator><creator>SUMI TOMOHIDE</creator><scope>EVB</scope></search><sort><creationdate>20130304</creationdate><title>METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY</title><author>AKITA HIROYUKI ; MIO TAKUMI ; ANDO KENSUKE ; SUMI TOMOHIDE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013045714A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>AKITA HIROYUKI</creatorcontrib><creatorcontrib>MIO TAKUMI</creatorcontrib><creatorcontrib>ANDO KENSUKE</creatorcontrib><creatorcontrib>SUMI TOMOHIDE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>AKITA HIROYUKI</au><au>MIO TAKUMI</au><au>ANDO KENSUKE</au><au>SUMI TOMOHIDE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY</title><date>2013-03-04</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing a secondary battery which can be charged/discharged at high rate.SOLUTION: In the method for manufacturing a secondary battery, negative electrode slurry including a negative electrode active material, carboxymethyl cellulose (CMC) and styrene-butadiene rubber is imparted on a negative electrode collector and dried to form a negative electrode active material layer. The CMC has a weight average molecular weight of 30×10or more and 40×10or less. An amount of the CMC included in the negative electrode active material layer is in a range of 0.6-0.8 mass%. The negative electrode active material has an O/C value of 1.0 or less, the O/C value being a value of a ratio between an oxygen element and a carbon element and obtained by means of an X-ray photoelectron spectroscopy on a surface of a particle thereof.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2013045714A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title METHOD FOR MANUFACTURING NONAQUEOUS SECONDARY BATTERY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T02%3A21%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=AKITA%20HIROYUKI&rft.date=2013-03-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013045714A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true