ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME

PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a battery case excellent in pressure resistance and laser weldability and a suitable method for producing the same.SOLUTION: The aluminum alloy sheet for a battery case comprises 0.10-0.60 mass% of Si, 0.05-0.60 mass% of Fe, more than 0.70...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ISHII HIDEHIKO, ZHAO PIZHI, FUJII TAKANORI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ISHII HIDEHIKO
ZHAO PIZHI
FUJII TAKANORI
description PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a battery case excellent in pressure resistance and laser weldability and a suitable method for producing the same.SOLUTION: The aluminum alloy sheet for a battery case comprises 0.10-0.60 mass% of Si, 0.05-0.60 mass% of Fe, more than 0.70 mass% and less than 1.0 mass% of Cu, 0.10-1.80 mass% of Mn, more than 0.70 mass% and not more than 1.5 mass% of Mg, more than 0.10 mass% and less than 0.20 mass% of Zr, and 0.03-0.25 mass% of Ti, with the balance of Al and unavoidable impurities, wherein artificial aging treatment is not performed prior to case molding. Further, 0.02 mass% or less of B and 0.35 mass% or less of Cr can be contained. A battery case is produced from the aluminum alloy sheet by performing aging treatment after the aluminum alloy sheet is molded into a case. The battery case is excellent in pressure resistance because a sufficient intermediate phase of AlCuMg is developed due to the aging treatment, and is capable of high-speed laser welding because the Cu content achieves the specific amount above.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012255214A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012255214A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012255214A3</originalsourceid><addsrcrecordid>eNrjZHB39An19fQL9VVw9PHxj1QI9nB1DVFw8w9ScHIMCXENilRwdgx2VXD0c1HwdQ3x8HcBywUE-buEOnv6uSuEeLgqBDv6uvIwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDQyMjU1MjQxNHY6IUAQANQyyf</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME</title><source>esp@cenet</source><creator>ISHII HIDEHIKO ; ZHAO PIZHI ; FUJII TAKANORI</creator><creatorcontrib>ISHII HIDEHIKO ; ZHAO PIZHI ; FUJII TAKANORI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a battery case excellent in pressure resistance and laser weldability and a suitable method for producing the same.SOLUTION: The aluminum alloy sheet for a battery case comprises 0.10-0.60 mass% of Si, 0.05-0.60 mass% of Fe, more than 0.70 mass% and less than 1.0 mass% of Cu, 0.10-1.80 mass% of Mn, more than 0.70 mass% and not more than 1.5 mass% of Mg, more than 0.10 mass% and less than 0.20 mass% of Zr, and 0.03-0.25 mass% of Ti, with the balance of Al and unavoidable impurities, wherein artificial aging treatment is not performed prior to case molding. Further, 0.02 mass% or less of B and 0.35 mass% or less of Cr can be contained. A battery case is produced from the aluminum alloy sheet by performing aging treatment after the aluminum alloy sheet is molded into a case. The battery case is excellent in pressure resistance because a sufficient intermediate phase of AlCuMg is developed due to the aging treatment, and is capable of high-speed laser welding because the Cu content achieves the specific amount above.</description><language>eng</language><subject>ALLOYS ; BASIC ELECTRIC ELEMENTS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; ELECTRICITY ; FERROUS OR NON-FERROUS ALLOYS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121227&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012255214A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121227&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012255214A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ISHII HIDEHIKO</creatorcontrib><creatorcontrib>ZHAO PIZHI</creatorcontrib><creatorcontrib>FUJII TAKANORI</creatorcontrib><title>ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a battery case excellent in pressure resistance and laser weldability and a suitable method for producing the same.SOLUTION: The aluminum alloy sheet for a battery case comprises 0.10-0.60 mass% of Si, 0.05-0.60 mass% of Fe, more than 0.70 mass% and less than 1.0 mass% of Cu, 0.10-1.80 mass% of Mn, more than 0.70 mass% and not more than 1.5 mass% of Mg, more than 0.10 mass% and less than 0.20 mass% of Zr, and 0.03-0.25 mass% of Ti, with the balance of Al and unavoidable impurities, wherein artificial aging treatment is not performed prior to case molding. Further, 0.02 mass% or less of B and 0.35 mass% or less of Cr can be contained. A battery case is produced from the aluminum alloy sheet by performing aging treatment after the aluminum alloy sheet is molded into a case. The battery case is excellent in pressure resistance because a sufficient intermediate phase of AlCuMg is developed due to the aging treatment, and is capable of high-speed laser welding because the Cu content achieves the specific amount above.</description><subject>ALLOYS</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHB39An19fQL9VVw9PHxj1QI9nB1DVFw8w9ScHIMCXENilRwdgx2VXD0c1HwdQ3x8HcBywUE-buEOnv6uSuEeLgqBDv6uvIwsKYl5hSn8kJpbgYlN9cQZw_d1IL8-NTigsTk1LzUknivACMDQyMjU1MjQxNHY6IUAQANQyyf</recordid><startdate>20121227</startdate><enddate>20121227</enddate><creator>ISHII HIDEHIKO</creator><creator>ZHAO PIZHI</creator><creator>FUJII TAKANORI</creator><scope>EVB</scope></search><sort><creationdate>20121227</creationdate><title>ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME</title><author>ISHII HIDEHIKO ; ZHAO PIZHI ; FUJII TAKANORI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012255214A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>ALLOYS</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>ISHII HIDEHIKO</creatorcontrib><creatorcontrib>ZHAO PIZHI</creatorcontrib><creatorcontrib>FUJII TAKANORI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ISHII HIDEHIKO</au><au>ZHAO PIZHI</au><au>FUJII TAKANORI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME</title><date>2012-12-27</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To provide an aluminum alloy sheet for a battery case excellent in pressure resistance and laser weldability and a suitable method for producing the same.SOLUTION: The aluminum alloy sheet for a battery case comprises 0.10-0.60 mass% of Si, 0.05-0.60 mass% of Fe, more than 0.70 mass% and less than 1.0 mass% of Cu, 0.10-1.80 mass% of Mn, more than 0.70 mass% and not more than 1.5 mass% of Mg, more than 0.10 mass% and less than 0.20 mass% of Zr, and 0.03-0.25 mass% of Ti, with the balance of Al and unavoidable impurities, wherein artificial aging treatment is not performed prior to case molding. Further, 0.02 mass% or less of B and 0.35 mass% or less of Cr can be contained. A battery case is produced from the aluminum alloy sheet by performing aging treatment after the aluminum alloy sheet is molded into a case. The battery case is excellent in pressure resistance because a sufficient intermediate phase of AlCuMg is developed due to the aging treatment, and is capable of high-speed laser welding because the Cu content achieves the specific amount above.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2012255214A
source esp@cenet
subjects ALLOYS
BASIC ELECTRIC ELEMENTS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
ELECTRICITY
FERROUS OR NON-FERROUS ALLOYS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title ALUMINUM ALLOY SHEET FOR BATTERY CASE AND METHOD FOR PRODUCING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T11%3A52%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ISHII%20HIDEHIKO&rft.date=2012-12-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012255214A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true