METHOD FOR MANUFACTURING RETARDATION FILM

PROBLEM TO BE SOLVED: To provide a method for manufacturing a polypropylene-based resin retardation film having high axis accuracy and uniform phase difference value.SOLUTION: The method for manufacturing the polypropylene-based resin retardation film includes: (A) longitudinally stretching a rolled...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUROIWA HIDEO, NAKATANI AKIHIKO, ARIKAWA NAOKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUROIWA HIDEO
NAKATANI AKIHIKO
ARIKAWA NAOKI
description PROBLEM TO BE SOLVED: To provide a method for manufacturing a polypropylene-based resin retardation film having high axis accuracy and uniform phase difference value.SOLUTION: The method for manufacturing the polypropylene-based resin retardation film includes: (A) longitudinally stretching a rolled film made of a polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of T°C between 0-40°C; and (C) laterally stretching the cured rolled film, in this order. The curing step (B) is conducted so as to satisfy the expression: D≥-0.4T+20 on the basis of a curing period as D day. Typically, the method includes: (A) longitudinally stretching the rolled film made of the polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of between 20-30°C for 10 days or more; and (C) laterally stretching the cured rolled film, in this order.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012037597A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012037597A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012037597A3</originalsourceid><addsrcrecordid>eNrjZND0dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCHINcQxycQzx9PdTcPP08eVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhkYGxuamluaOxkQpAgB9wiTt</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING RETARDATION FILM</title><source>esp@cenet</source><creator>KUROIWA HIDEO ; NAKATANI AKIHIKO ; ARIKAWA NAOKI</creator><creatorcontrib>KUROIWA HIDEO ; NAKATANI AKIHIKO ; ARIKAWA NAOKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a polypropylene-based resin retardation film having high axis accuracy and uniform phase difference value.SOLUTION: The method for manufacturing the polypropylene-based resin retardation film includes: (A) longitudinally stretching a rolled film made of a polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of T°C between 0-40°C; and (C) laterally stretching the cured rolled film, in this order. The curing step (B) is conducted so as to satisfy the expression: D≥-0.4T+20 on the basis of a curing period as D day. Typically, the method includes: (A) longitudinally stretching the rolled film made of the polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of between 20-30°C for 10 days or more; and (C) laterally stretching the cured rolled film, in this order.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES ; INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PERFORMING OPERATIONS ; PHYSICS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120223&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012037597A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120223&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012037597A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUROIWA HIDEO</creatorcontrib><creatorcontrib>NAKATANI AKIHIKO</creatorcontrib><creatorcontrib>ARIKAWA NAOKI</creatorcontrib><title>METHOD FOR MANUFACTURING RETARDATION FILM</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a polypropylene-based resin retardation film having high axis accuracy and uniform phase difference value.SOLUTION: The method for manufacturing the polypropylene-based resin retardation film includes: (A) longitudinally stretching a rolled film made of a polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of T°C between 0-40°C; and (C) laterally stretching the cured rolled film, in this order. The curing step (B) is conducted so as to satisfy the expression: D≥-0.4T+20 on the basis of a curing period as D day. Typically, the method includes: (A) longitudinally stretching the rolled film made of the polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of between 20-30°C for 10 days or more; and (C) laterally stretching the cured rolled film, in this order.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND0dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCHINcQxycQzx9PdTcPP08eVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhkYGxuamluaOxkQpAgB9wiTt</recordid><startdate>20120223</startdate><enddate>20120223</enddate><creator>KUROIWA HIDEO</creator><creator>NAKATANI AKIHIKO</creator><creator>ARIKAWA NAOKI</creator><scope>EVB</scope></search><sort><creationdate>20120223</creationdate><title>METHOD FOR MANUFACTURING RETARDATION FILM</title><author>KUROIWA HIDEO ; NAKATANI AKIHIKO ; ARIKAWA NAOKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012037597A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>KUROIWA HIDEO</creatorcontrib><creatorcontrib>NAKATANI AKIHIKO</creatorcontrib><creatorcontrib>ARIKAWA NAOKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUROIWA HIDEO</au><au>NAKATANI AKIHIKO</au><au>ARIKAWA NAOKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING RETARDATION FILM</title><date>2012-02-23</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing a polypropylene-based resin retardation film having high axis accuracy and uniform phase difference value.SOLUTION: The method for manufacturing the polypropylene-based resin retardation film includes: (A) longitudinally stretching a rolled film made of a polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of T°C between 0-40°C; and (C) laterally stretching the cured rolled film, in this order. The curing step (B) is conducted so as to satisfy the expression: D≥-0.4T+20 on the basis of a curing period as D day. Typically, the method includes: (A) longitudinally stretching the rolled film made of the polypropylene-based resin; (B) curing the longitudinally stretched rolled film under the environment of a temperature of between 20-30°C for 10 days or more; and (C) laterally stretching the cured rolled film, in this order.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2012037597A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES
INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
PERFORMING OPERATIONS
PHYSICS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title METHOD FOR MANUFACTURING RETARDATION FILM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T22%3A34%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUROIWA%20HIDEO&rft.date=2012-02-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012037597A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true