PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME

PROBLEM TO BE SOLVED: To provide a hollow extruded material of an Al-Mg-Si-based aluminum alloy capable of increasing strength in the vicinity of a welded part and increasing an expansion rate, and capable of achieving a workpiece with an even plate thickness distribution by preventing a constrictio...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKADA TAKESHI, WAKAKURI SATOSHI, HIBINO AKIRA, ICHITANI KOJI, SAGA MAKOTO, ATSUTA KEN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAKADA TAKESHI
WAKAKURI SATOSHI
HIBINO AKIRA
ICHITANI KOJI
SAGA MAKOTO
ATSUTA KEN
description PROBLEM TO BE SOLVED: To provide a hollow extruded material of an Al-Mg-Si-based aluminum alloy capable of increasing strength in the vicinity of a welded part and increasing an expansion rate, and capable of achieving a workpiece with an even plate thickness distribution by preventing a constriction when the hollow extruded material of the Al-Mg-Si-based aluminum alloy is subjected to hot bulging.SOLUTION: When a square area with a side length of 500 μm including 40 or more crystal grains is selected from an area demarcated by a range of 2 mm on both sides with a welding line as its middle in a direction vertical to the welding line on a surface vertical to a direction of extruding the porthole hollow extruded material of Al-Mg-Si-based aluminum alloy, and t/10 to 9t/10 of plate thickness t of the hollow extruded material from a surface of the hollow extruded material in a direction parallel to the welding line, the minimum value of an area ratio of the crystal grains in a Cube orientation is set to be 10-50%, and the difference of the maximum value and the minimum value of the area ratio of the crystal grains in the Cube orientation is set to be 60% or less.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012020326A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012020326A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012020326A3</originalsourceid><addsrcrecordid>eNrjZAgL8A8K8fD3cVVwjQgJCnVxdVHwdQxxDfJ09FFw8w9S8PAPUXAK9XF3BfF8Pf3cFRz9gEpcgXpcwAp8Hf1C3RydQ0KDQJIhHq4KwY6-rjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjA0MjAyMDYyMzRmChFAOMjMN8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME</title><source>esp@cenet</source><creator>TAKADA TAKESHI ; WAKAKURI SATOSHI ; HIBINO AKIRA ; ICHITANI KOJI ; SAGA MAKOTO ; ATSUTA KEN</creator><creatorcontrib>TAKADA TAKESHI ; WAKAKURI SATOSHI ; HIBINO AKIRA ; ICHITANI KOJI ; SAGA MAKOTO ; ATSUTA KEN</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a hollow extruded material of an Al-Mg-Si-based aluminum alloy capable of increasing strength in the vicinity of a welded part and increasing an expansion rate, and capable of achieving a workpiece with an even plate thickness distribution by preventing a constriction when the hollow extruded material of the Al-Mg-Si-based aluminum alloy is subjected to hot bulging.SOLUTION: When a square area with a side length of 500 μm including 40 or more crystal grains is selected from an area demarcated by a range of 2 mm on both sides with a welding line as its middle in a direction vertical to the welding line on a surface vertical to a direction of extruding the porthole hollow extruded material of Al-Mg-Si-based aluminum alloy, and t/10 to 9t/10 of plate thickness t of the hollow extruded material from a surface of the hollow extruded material in a direction parallel to the welding line, the minimum value of an area ratio of the crystal grains in a Cube orientation is set to be 10-50%, and the difference of the maximum value and the minimum value of the area ratio of the crystal grains in the Cube orientation is set to be 60% or less.</description><language>eng</language><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL ; MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120202&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012020326A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120202&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012020326A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKADA TAKESHI</creatorcontrib><creatorcontrib>WAKAKURI SATOSHI</creatorcontrib><creatorcontrib>HIBINO AKIRA</creatorcontrib><creatorcontrib>ICHITANI KOJI</creatorcontrib><creatorcontrib>SAGA MAKOTO</creatorcontrib><creatorcontrib>ATSUTA KEN</creatorcontrib><title>PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide a hollow extruded material of an Al-Mg-Si-based aluminum alloy capable of increasing strength in the vicinity of a welded part and increasing an expansion rate, and capable of achieving a workpiece with an even plate thickness distribution by preventing a constriction when the hollow extruded material of the Al-Mg-Si-based aluminum alloy is subjected to hot bulging.SOLUTION: When a square area with a side length of 500 μm including 40 or more crystal grains is selected from an area demarcated by a range of 2 mm on both sides with a welding line as its middle in a direction vertical to the welding line on a surface vertical to a direction of extruding the porthole hollow extruded material of Al-Mg-Si-based aluminum alloy, and t/10 to 9t/10 of plate thickness t of the hollow extruded material from a surface of the hollow extruded material in a direction parallel to the welding line, the minimum value of an area ratio of the crystal grains in a Cube orientation is set to be 10-50%, and the difference of the maximum value and the minimum value of the area ratio of the crystal grains in the Cube orientation is set to be 60% or less.</description><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</subject><subject>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAgL8A8K8fD3cVVwjQgJCnVxdVHwdQxxDfJ09FFw8w9S8PAPUXAK9XF3BfF8Pf3cFRz9gEpcgXpcwAp8Hf1C3RydQ0KDQJIhHq4KwY6-rjwMrGmJOcWpvFCam0HJzTXE2UM3tSA_PrW4IDE5NS-1JN4rwMjA0MjAyMDYyMzRmChFAOMjMN8</recordid><startdate>20120202</startdate><enddate>20120202</enddate><creator>TAKADA TAKESHI</creator><creator>WAKAKURI SATOSHI</creator><creator>HIBINO AKIRA</creator><creator>ICHITANI KOJI</creator><creator>SAGA MAKOTO</creator><creator>ATSUTA KEN</creator><scope>EVB</scope></search><sort><creationdate>20120202</creationdate><title>PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME</title><author>TAKADA TAKESHI ; WAKAKURI SATOSHI ; HIBINO AKIRA ; ICHITANI KOJI ; SAGA MAKOTO ; ATSUTA KEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012020326A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</topic><topic>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKADA TAKESHI</creatorcontrib><creatorcontrib>WAKAKURI SATOSHI</creatorcontrib><creatorcontrib>HIBINO AKIRA</creatorcontrib><creatorcontrib>ICHITANI KOJI</creatorcontrib><creatorcontrib>SAGA MAKOTO</creatorcontrib><creatorcontrib>ATSUTA KEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKADA TAKESHI</au><au>WAKAKURI SATOSHI</au><au>HIBINO AKIRA</au><au>ICHITANI KOJI</au><au>SAGA MAKOTO</au><au>ATSUTA KEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME</title><date>2012-02-02</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To provide a hollow extruded material of an Al-Mg-Si-based aluminum alloy capable of increasing strength in the vicinity of a welded part and increasing an expansion rate, and capable of achieving a workpiece with an even plate thickness distribution by preventing a constriction when the hollow extruded material of the Al-Mg-Si-based aluminum alloy is subjected to hot bulging.SOLUTION: When a square area with a side length of 500 μm including 40 or more crystal grains is selected from an area demarcated by a range of 2 mm on both sides with a welding line as its middle in a direction vertical to the welding line on a surface vertical to a direction of extruding the porthole hollow extruded material of Al-Mg-Si-based aluminum alloy, and t/10 to 9t/10 of plate thickness t of the hollow extruded material from a surface of the hollow extruded material in a direction parallel to the welding line, the minimum value of an area ratio of the crystal grains in a Cube orientation is set to be 10-50%, and the difference of the maximum value and the minimum value of the area ratio of the crystal grains in the Cube orientation is set to be 60% or less.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2012020326A
source esp@cenet
subjects AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL
MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL
title PORTHOLE EXTRUDED MATERIAL FOR HOT BULGE FORMING AND METHOD FOR MANUFACTURING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T19%3A01%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKADA%20TAKESHI&rft.date=2012-02-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012020326A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true