SCARF JOINING METHOD OF PLYWOOD
PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a leng...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KUDO KIMIHIKO |
description | PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a length (L) of 1,600-5,000 mm, moisture-curable type urethane resin-based hot-melt adhesives (5) are applied on scarf slopes (3f) (3r) shaved to the scarf ratio of 1:5 to 1:10 by 100-170 g/mand cold-pressed and cured for 10-20 sec. by hydraulic cold presses (6a), (6b) at a press clamping pressure of 0.8-1.0 MPa. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2011016288A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2011016288A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2011016288A3</originalsourceid><addsrcrecordid>eNrjZJAPdnYMclPw8vf08_RzV_B1DfHwd1Hwd1MI8IkM9_d34WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgaGhgaGZkYWFo7GRCkCAAsMIfU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SCARF JOINING METHOD OF PLYWOOD</title><source>esp@cenet</source><creator>KUDO KIMIHIKO</creator><creatorcontrib>KUDO KIMIHIKO</creatorcontrib><description>PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a length (L) of 1,600-5,000 mm, moisture-curable type urethane resin-based hot-melt adhesives (5) are applied on scarf slopes (3f) (3r) shaved to the scarf ratio of 1:5 to 1:10 by 100-170 g/mand cold-pressed and cured for 10-20 sec. by hydraulic cold presses (6a), (6b) at a press clamping pressure of 0.8-1.0 MPa.</description><language>eng</language><subject>MANUFACTURE OF SPECIFIC WOODEN ARTICLES ; NAILING OR STAPLING MACHINES IN GENERAL ; PERFORMING OPERATIONS ; TRANSPORTING ; WORKING OF WOOD NOT PROVIDED FOR IN SUBCLASSES B27B - B27L ; WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL ; WORKING VENEER OR PLYWOOD</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110127&DB=EPODOC&CC=JP&NR=2011016288A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110127&DB=EPODOC&CC=JP&NR=2011016288A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUDO KIMIHIKO</creatorcontrib><title>SCARF JOINING METHOD OF PLYWOOD</title><description>PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a length (L) of 1,600-5,000 mm, moisture-curable type urethane resin-based hot-melt adhesives (5) are applied on scarf slopes (3f) (3r) shaved to the scarf ratio of 1:5 to 1:10 by 100-170 g/mand cold-pressed and cured for 10-20 sec. by hydraulic cold presses (6a), (6b) at a press clamping pressure of 0.8-1.0 MPa.</description><subject>MANUFACTURE OF SPECIFIC WOODEN ARTICLES</subject><subject>NAILING OR STAPLING MACHINES IN GENERAL</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>WORKING OF WOOD NOT PROVIDED FOR IN SUBCLASSES B27B - B27L</subject><subject>WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL</subject><subject>WORKING VENEER OR PLYWOOD</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJAPdnYMclPw8vf08_RzV_B1DfHwd1Hwd1MI8IkM9_d34WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgaGhgaGZkYWFo7GRCkCAAsMIfU</recordid><startdate>20110127</startdate><enddate>20110127</enddate><creator>KUDO KIMIHIKO</creator><scope>EVB</scope></search><sort><creationdate>20110127</creationdate><title>SCARF JOINING METHOD OF PLYWOOD</title><author>KUDO KIMIHIKO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2011016288A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2011</creationdate><topic>MANUFACTURE OF SPECIFIC WOODEN ARTICLES</topic><topic>NAILING OR STAPLING MACHINES IN GENERAL</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>WORKING OF WOOD NOT PROVIDED FOR IN SUBCLASSES B27B - B27L</topic><topic>WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL</topic><topic>WORKING VENEER OR PLYWOOD</topic><toplevel>online_resources</toplevel><creatorcontrib>KUDO KIMIHIKO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUDO KIMIHIKO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SCARF JOINING METHOD OF PLYWOOD</title><date>2011-01-27</date><risdate>2011</risdate><abstract>PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a length (L) of 1,600-5,000 mm, moisture-curable type urethane resin-based hot-melt adhesives (5) are applied on scarf slopes (3f) (3r) shaved to the scarf ratio of 1:5 to 1:10 by 100-170 g/mand cold-pressed and cured for 10-20 sec. by hydraulic cold presses (6a), (6b) at a press clamping pressure of 0.8-1.0 MPa.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2011016288A |
source | esp@cenet |
subjects | MANUFACTURE OF SPECIFIC WOODEN ARTICLES NAILING OR STAPLING MACHINES IN GENERAL PERFORMING OPERATIONS TRANSPORTING WORKING OF WOOD NOT PROVIDED FOR IN SUBCLASSES B27B - B27L WORKING OR PRESERVING WOOD OR SIMILAR MATERIAL WORKING VENEER OR PLYWOOD |
title | SCARF JOINING METHOD OF PLYWOOD |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T00%3A49%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUDO%20KIMIHIKO&rft.date=2011-01-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2011016288A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |