SCARF JOINING METHOD OF PLYWOOD

PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a leng...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: KUDO KIMIHIKO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To largely shorten a cycle time required for the scarf joining of plywood, and to improve productivity by employing a moisture-curable type urethane resin-based hot-melt adhesive.SOLUTION: The plywood (1) has a thickness (T) of 7.5-35 mm, a width (W) of 900-1,250 mm, and a length (L) of 1,600-5,000 mm, moisture-curable type urethane resin-based hot-melt adhesives (5) are applied on scarf slopes (3f) (3r) shaved to the scarf ratio of 1:5 to 1:10 by 100-170 g/mand cold-pressed and cured for 10-20 sec. by hydraulic cold presses (6a), (6b) at a press clamping pressure of 0.8-1.0 MPa.