CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT
PROBLEM TO BE SOLVED: To provide a concrete composition, while suppressing the exhaust amount of carbon dioxide, which can secure satisfactory applicability in a state where the reduction in the fluidity and the reduction in an air amount with the lapse of time in the prepared concrete composition a...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YONEZAWA TOSHIO IKEO YOSAKU HASUMI TAKASHI KINOSHITA MITSUO TAMAKI SHINJI INOUE KAZUMASA SAITO KAZUHIDE KURODA MOE WACHI MASAHIRO MITSUI TATEO |
description | PROBLEM TO BE SOLVED: To provide a concrete composition, while suppressing the exhaust amount of carbon dioxide, which can secure satisfactory applicability in a state where the reduction in the fluidity and the reduction in an air amount with the lapse of time in the prepared concrete composition are suppressed, further can suppress the drying shrinkage of the obtained hardened body, and can make the required strength appear in the obtained hardened body as well. SOLUTION: The concrete composition at least comprises cement, water, fine aggregate, coarse aggregate and an admixture. As the cement, the following blast-furnace cement is used, also, the ratio of the water/the blast-furnace cement is regulated to 20 to 60%, and further, per 100 pts.mass of the blast-furnace cement, as at least a part of the admixture, a specified cement dispersant, a specified drying shrinkage reducer and a specified setting accelerator are comprised by prescribed amounts. The blast-furnace cement comprises blast-furnace slag fine powder having fineness of 3,000 to 13,000 cm2/g and portland cement, and also, the blast-furnace slag fine powder is comprised by 60 to 80 mass% and the portland cement is comprised by 20 to 40 mass% (total 100 mass%). COPYRIGHT: (C)2011,JPO&INPIT |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2010285292A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2010285292A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2010285292A3</originalsourceid><addsrcrecordid>eNrjZNB39vdzDnINcVVw9vcN8A_2DPH091MIDfb0c1dw8nEMDtF1Cw3yc3QGyrv6uvqF8DCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwNDAyMLUyNLI0djohQBAGa4Jpg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT</title><source>esp@cenet</source><creator>YONEZAWA TOSHIO ; IKEO YOSAKU ; HASUMI TAKASHI ; KINOSHITA MITSUO ; TAMAKI SHINJI ; INOUE KAZUMASA ; SAITO KAZUHIDE ; KURODA MOE ; WACHI MASAHIRO ; MITSUI TATEO</creator><creatorcontrib>YONEZAWA TOSHIO ; IKEO YOSAKU ; HASUMI TAKASHI ; KINOSHITA MITSUO ; TAMAKI SHINJI ; INOUE KAZUMASA ; SAITO KAZUHIDE ; KURODA MOE ; WACHI MASAHIRO ; MITSUI TATEO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a concrete composition, while suppressing the exhaust amount of carbon dioxide, which can secure satisfactory applicability in a state where the reduction in the fluidity and the reduction in an air amount with the lapse of time in the prepared concrete composition are suppressed, further can suppress the drying shrinkage of the obtained hardened body, and can make the required strength appear in the obtained hardened body as well. SOLUTION: The concrete composition at least comprises cement, water, fine aggregate, coarse aggregate and an admixture. As the cement, the following blast-furnace cement is used, also, the ratio of the water/the blast-furnace cement is regulated to 20 to 60%, and further, per 100 pts.mass of the blast-furnace cement, as at least a part of the admixture, a specified cement dispersant, a specified drying shrinkage reducer and a specified setting accelerator are comprised by prescribed amounts. The blast-furnace cement comprises blast-furnace slag fine powder having fineness of 3,000 to 13,000 cm2/g and portland cement, and also, the blast-furnace slag fine powder is comprised by 60 to 80 mass% and the portland cement is comprised by 20 to 40 mass% (total 100 mass%). COPYRIGHT: (C)2011,JPO&INPIT</description><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE ; TREATMENT OF NATURAL STONE</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20101224&DB=EPODOC&CC=JP&NR=2010285292A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20101224&DB=EPODOC&CC=JP&NR=2010285292A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YONEZAWA TOSHIO</creatorcontrib><creatorcontrib>IKEO YOSAKU</creatorcontrib><creatorcontrib>HASUMI TAKASHI</creatorcontrib><creatorcontrib>KINOSHITA MITSUO</creatorcontrib><creatorcontrib>TAMAKI SHINJI</creatorcontrib><creatorcontrib>INOUE KAZUMASA</creatorcontrib><creatorcontrib>SAITO KAZUHIDE</creatorcontrib><creatorcontrib>KURODA MOE</creatorcontrib><creatorcontrib>WACHI MASAHIRO</creatorcontrib><creatorcontrib>MITSUI TATEO</creatorcontrib><title>CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT</title><description>PROBLEM TO BE SOLVED: To provide a concrete composition, while suppressing the exhaust amount of carbon dioxide, which can secure satisfactory applicability in a state where the reduction in the fluidity and the reduction in an air amount with the lapse of time in the prepared concrete composition are suppressed, further can suppress the drying shrinkage of the obtained hardened body, and can make the required strength appear in the obtained hardened body as well. SOLUTION: The concrete composition at least comprises cement, water, fine aggregate, coarse aggregate and an admixture. As the cement, the following blast-furnace cement is used, also, the ratio of the water/the blast-furnace cement is regulated to 20 to 60%, and further, per 100 pts.mass of the blast-furnace cement, as at least a part of the admixture, a specified cement dispersant, a specified drying shrinkage reducer and a specified setting accelerator are comprised by prescribed amounts. The blast-furnace cement comprises blast-furnace slag fine powder having fineness of 3,000 to 13,000 cm2/g and portland cement, and also, the blast-furnace slag fine powder is comprised by 60 to 80 mass% and the portland cement is comprised by 20 to 40 mass% (total 100 mass%). COPYRIGHT: (C)2011,JPO&INPIT</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNB39vdzDnINcVVw9vcN8A_2DPH091MIDfb0c1dw8nEMDtF1Cw3yc3QGyrv6uvqF8DCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwNDAyMLUyNLI0djohQBAGa4Jpg</recordid><startdate>20101224</startdate><enddate>20101224</enddate><creator>YONEZAWA TOSHIO</creator><creator>IKEO YOSAKU</creator><creator>HASUMI TAKASHI</creator><creator>KINOSHITA MITSUO</creator><creator>TAMAKI SHINJI</creator><creator>INOUE KAZUMASA</creator><creator>SAITO KAZUHIDE</creator><creator>KURODA MOE</creator><creator>WACHI MASAHIRO</creator><creator>MITSUI TATEO</creator><scope>EVB</scope></search><sort><creationdate>20101224</creationdate><title>CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT</title><author>YONEZAWA TOSHIO ; IKEO YOSAKU ; HASUMI TAKASHI ; KINOSHITA MITSUO ; TAMAKI SHINJI ; INOUE KAZUMASA ; SAITO KAZUHIDE ; KURODA MOE ; WACHI MASAHIRO ; MITSUI TATEO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2010285292A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2010</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>YONEZAWA TOSHIO</creatorcontrib><creatorcontrib>IKEO YOSAKU</creatorcontrib><creatorcontrib>HASUMI TAKASHI</creatorcontrib><creatorcontrib>KINOSHITA MITSUO</creatorcontrib><creatorcontrib>TAMAKI SHINJI</creatorcontrib><creatorcontrib>INOUE KAZUMASA</creatorcontrib><creatorcontrib>SAITO KAZUHIDE</creatorcontrib><creatorcontrib>KURODA MOE</creatorcontrib><creatorcontrib>WACHI MASAHIRO</creatorcontrib><creatorcontrib>MITSUI TATEO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YONEZAWA TOSHIO</au><au>IKEO YOSAKU</au><au>HASUMI TAKASHI</au><au>KINOSHITA MITSUO</au><au>TAMAKI SHINJI</au><au>INOUE KAZUMASA</au><au>SAITO KAZUHIDE</au><au>KURODA MOE</au><au>WACHI MASAHIRO</au><au>MITSUI TATEO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT</title><date>2010-12-24</date><risdate>2010</risdate><abstract>PROBLEM TO BE SOLVED: To provide a concrete composition, while suppressing the exhaust amount of carbon dioxide, which can secure satisfactory applicability in a state where the reduction in the fluidity and the reduction in an air amount with the lapse of time in the prepared concrete composition are suppressed, further can suppress the drying shrinkage of the obtained hardened body, and can make the required strength appear in the obtained hardened body as well. SOLUTION: The concrete composition at least comprises cement, water, fine aggregate, coarse aggregate and an admixture. As the cement, the following blast-furnace cement is used, also, the ratio of the water/the blast-furnace cement is regulated to 20 to 60%, and further, per 100 pts.mass of the blast-furnace cement, as at least a part of the admixture, a specified cement dispersant, a specified drying shrinkage reducer and a specified setting accelerator are comprised by prescribed amounts. The blast-furnace cement comprises blast-furnace slag fine powder having fineness of 3,000 to 13,000 cm2/g and portland cement, and also, the blast-furnace slag fine powder is comprised by 60 to 80 mass% and the portland cement is comprised by 20 to 40 mass% (total 100 mass%). COPYRIGHT: (C)2011,JPO&INPIT</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2010285292A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATERTREATMENT OR WASTE MANAGEMENT COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE TREATMENT OF NATURAL STONE |
title | CONCRETE COMPOSITION USING BLAST-FURNACE CEMENT |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-29T02%3A14%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YONEZAWA%20TOSHIO&rft.date=2010-12-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2010285292A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |