TUNDISH FOR CONTINUOUS CASTING

PROBLEM TO BE SOLVED: To increase the separation-removal function of inclusions in a molten steel while improving the yield of the steel. SOLUTION: On the bottom face 13 of a tundish 1, a flat part 30 forming a flat shape at least in the lower part of an injection nozzle 20 is formed. The corner par...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKEZAKI KAZUMASA, FUJI TAKEHIKO, SHIGEMATSU KIYOSHI, FUCHIGAMI KATSUHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAKEZAKI KAZUMASA
FUJI TAKEHIKO
SHIGEMATSU KIYOSHI
FUCHIGAMI KATSUHIRO
description PROBLEM TO BE SOLVED: To increase the separation-removal function of inclusions in a molten steel while improving the yield of the steel. SOLUTION: On the bottom face 13 of a tundish 1, a flat part 30 forming a flat shape at least in the lower part of an injection nozzle 20 is formed. The corner parts between the flat part 30 and the long-side walls 10, 10 have curved parts 31, 31 curved so as to be projected to the external side. The flat part 30 and the curved part 31 are formed along the long-side walls 10 of the tundish 1, and the minimum curvature radius R(m) of the curved part 31 satisfies inequality: 0.1≤R≤(W-D)/2 [wherein W denotes a distance (m) between the intersections P, P between the tangent L1of the long-side wall 10 in the position of the maximum molten metal surface M1within the tundish 1 and the extension L2of the flat part 30; and D denotes the inside diameter (m) of the injection nozzle 20]. COPYRIGHT: (C)2011,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2010274321A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2010274321A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2010274321A3</originalsourceid><addsrcrecordid>eNrjZJALCfVz8Qz2UHDzD1Jw9vcL8fQL9Q8NVnB2DAYy3XkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBoYGRuYmxkaGjMVGKAAhyIes</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>TUNDISH FOR CONTINUOUS CASTING</title><source>esp@cenet</source><creator>TAKEZAKI KAZUMASA ; FUJI TAKEHIKO ; SHIGEMATSU KIYOSHI ; FUCHIGAMI KATSUHIRO</creator><creatorcontrib>TAKEZAKI KAZUMASA ; FUJI TAKEHIKO ; SHIGEMATSU KIYOSHI ; FUCHIGAMI KATSUHIRO</creatorcontrib><description>PROBLEM TO BE SOLVED: To increase the separation-removal function of inclusions in a molten steel while improving the yield of the steel. SOLUTION: On the bottom face 13 of a tundish 1, a flat part 30 forming a flat shape at least in the lower part of an injection nozzle 20 is formed. The corner parts between the flat part 30 and the long-side walls 10, 10 have curved parts 31, 31 curved so as to be projected to the external side. The flat part 30 and the curved part 31 are formed along the long-side walls 10 of the tundish 1, and the minimum curvature radius R(m) of the curved part 31 satisfies inequality: 0.1≤R≤(W-D)/2 [wherein W denotes a distance (m) between the intersections P, P between the tangent L1of the long-side wall 10 in the position of the maximum molten metal surface M1within the tundish 1 and the extension L2of the flat part 30; and D denotes the inside diameter (m) of the injection nozzle 20]. COPYRIGHT: (C)2011,JPO&amp;INPIT</description><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20101209&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010274321A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20101209&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010274321A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKEZAKI KAZUMASA</creatorcontrib><creatorcontrib>FUJI TAKEHIKO</creatorcontrib><creatorcontrib>SHIGEMATSU KIYOSHI</creatorcontrib><creatorcontrib>FUCHIGAMI KATSUHIRO</creatorcontrib><title>TUNDISH FOR CONTINUOUS CASTING</title><description>PROBLEM TO BE SOLVED: To increase the separation-removal function of inclusions in a molten steel while improving the yield of the steel. SOLUTION: On the bottom face 13 of a tundish 1, a flat part 30 forming a flat shape at least in the lower part of an injection nozzle 20 is formed. The corner parts between the flat part 30 and the long-side walls 10, 10 have curved parts 31, 31 curved so as to be projected to the external side. The flat part 30 and the curved part 31 are formed along the long-side walls 10 of the tundish 1, and the minimum curvature radius R(m) of the curved part 31 satisfies inequality: 0.1≤R≤(W-D)/2 [wherein W denotes a distance (m) between the intersections P, P between the tangent L1of the long-side wall 10 in the position of the maximum molten metal surface M1within the tundish 1 and the extension L2of the flat part 30; and D denotes the inside diameter (m) of the injection nozzle 20]. COPYRIGHT: (C)2011,JPO&amp;INPIT</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJALCfVz8Qz2UHDzD1Jw9vcL8fQL9Q8NVnB2DAYy3XkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBoYGRuYmxkaGjMVGKAAhyIes</recordid><startdate>20101209</startdate><enddate>20101209</enddate><creator>TAKEZAKI KAZUMASA</creator><creator>FUJI TAKEHIKO</creator><creator>SHIGEMATSU KIYOSHI</creator><creator>FUCHIGAMI KATSUHIRO</creator><scope>EVB</scope></search><sort><creationdate>20101209</creationdate><title>TUNDISH FOR CONTINUOUS CASTING</title><author>TAKEZAKI KAZUMASA ; FUJI TAKEHIKO ; SHIGEMATSU KIYOSHI ; FUCHIGAMI KATSUHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2010274321A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2010</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKEZAKI KAZUMASA</creatorcontrib><creatorcontrib>FUJI TAKEHIKO</creatorcontrib><creatorcontrib>SHIGEMATSU KIYOSHI</creatorcontrib><creatorcontrib>FUCHIGAMI KATSUHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKEZAKI KAZUMASA</au><au>FUJI TAKEHIKO</au><au>SHIGEMATSU KIYOSHI</au><au>FUCHIGAMI KATSUHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>TUNDISH FOR CONTINUOUS CASTING</title><date>2010-12-09</date><risdate>2010</risdate><abstract>PROBLEM TO BE SOLVED: To increase the separation-removal function of inclusions in a molten steel while improving the yield of the steel. SOLUTION: On the bottom face 13 of a tundish 1, a flat part 30 forming a flat shape at least in the lower part of an injection nozzle 20 is formed. The corner parts between the flat part 30 and the long-side walls 10, 10 have curved parts 31, 31 curved so as to be projected to the external side. The flat part 30 and the curved part 31 are formed along the long-side walls 10 of the tundish 1, and the minimum curvature radius R(m) of the curved part 31 satisfies inequality: 0.1≤R≤(W-D)/2 [wherein W denotes a distance (m) between the intersections P, P between the tangent L1of the long-side wall 10 in the position of the maximum molten metal surface M1within the tundish 1 and the extension L2of the flat part 30; and D denotes the inside diameter (m) of the injection nozzle 20]. COPYRIGHT: (C)2011,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2010274321A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title TUNDISH FOR CONTINUOUS CASTING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-12T08%3A32%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKEZAKI%20KAZUMASA&rft.date=2010-12-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2010274321A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true