BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME

PROBLEM TO BE SOLVED: To provide a method for manufacturing a base material having, on its surface, a fluorine-containing polymer thin film which is excellent in adhesion with the base material, scratch resistance, mold-release resistance and an antifouling property, and has a fluorine-containing al...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAMITSUJI SHINYA, MINAMIDATE JUN, UENO KATSUYA, WATANABE KUNIO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAMITSUJI SHINYA
MINAMIDATE JUN
UENO KATSUYA
WATANABE KUNIO
description PROBLEM TO BE SOLVED: To provide a method for manufacturing a base material having, on its surface, a fluorine-containing polymer thin film which is excellent in adhesion with the base material, scratch resistance, mold-release resistance and an antifouling property, and has a fluorine-containing aliphatic ring structure. SOLUTION: In the method for manufacturing the base material having the fluorine-containing polymer thin film on its surface, following processes [1] to [4] are carried out in order of [1] to [4], wherein [1] is a process of treating the base material surface with a silane coupling agent having a polar functional group, [2] is a process of coating the base material surface with the fluorine-containing polymer which has a reactive functional group having reactivity with the polar functional group and has the fluorine-containing aliphatic ring structure in its main chain, [3] is a process of heat-treating the base material and [4] is a process of washing the base material surface with a fluorine-containing solvent. COPYRIGHT: (C)2010,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2010131569A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2010131569A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2010131569A3</originalsourceid><addsrcrecordid>eNqNjEEKwjAQAHvxIOofFu-F1qLgcW03JpJsSroVPNUi8SRaqP9HCz7A08AwzDy5HrAhcCgUDFrQeDZ8BGVbHwxTWnoWNDy52tuLowCiDYMy1gFyBY5E-wqUD98JtwpLacOUiyZo0NEymd37xxhXPy6StSIpdRqHVxfHob_FZ3x3p3qT5Vle5NvdHou_og_SaDOu</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME</title><source>esp@cenet</source><creator>TAMITSUJI SHINYA ; MINAMIDATE JUN ; UENO KATSUYA ; WATANABE KUNIO</creator><creatorcontrib>TAMITSUJI SHINYA ; MINAMIDATE JUN ; UENO KATSUYA ; WATANABE KUNIO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a base material having, on its surface, a fluorine-containing polymer thin film which is excellent in adhesion with the base material, scratch resistance, mold-release resistance and an antifouling property, and has a fluorine-containing aliphatic ring structure. SOLUTION: In the method for manufacturing the base material having the fluorine-containing polymer thin film on its surface, following processes [1] to [4] are carried out in order of [1] to [4], wherein [1] is a process of treating the base material surface with a silane coupling agent having a polar functional group, [2] is a process of coating the base material surface with the fluorine-containing polymer which has a reactive functional group having reactivity with the polar functional group and has the fluorine-containing aliphatic ring structure in its main chain, [3] is a process of heat-treating the base material and [4] is a process of washing the base material surface with a fluorine-containing solvent. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><language>eng</language><subject>ADHESIVES ; APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL ; CHEMICAL PAINT OR INK REMOVERS ; CHEMISTRY ; COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS ; CORRECTING FLUIDS ; DYES ; FILLING PASTES ; INKS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; PASTES OR SOLIDS FOR COLOURING OR PRINTING ; PERFORMING OPERATIONS ; POLISHES ; PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL ; SPRAYING OR ATOMISING IN GENERAL ; TRANSPORTING ; USE OF MATERIALS THEREFOR ; WOODSTAINS</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100617&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010131569A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100617&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010131569A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAMITSUJI SHINYA</creatorcontrib><creatorcontrib>MINAMIDATE JUN</creatorcontrib><creatorcontrib>UENO KATSUYA</creatorcontrib><creatorcontrib>WATANABE KUNIO</creatorcontrib><title>BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing a base material having, on its surface, a fluorine-containing polymer thin film which is excellent in adhesion with the base material, scratch resistance, mold-release resistance and an antifouling property, and has a fluorine-containing aliphatic ring structure. SOLUTION: In the method for manufacturing the base material having the fluorine-containing polymer thin film on its surface, following processes [1] to [4] are carried out in order of [1] to [4], wherein [1] is a process of treating the base material surface with a silane coupling agent having a polar functional group, [2] is a process of coating the base material surface with the fluorine-containing polymer which has a reactive functional group having reactivity with the polar functional group and has the fluorine-containing aliphatic ring structure in its main chain, [3] is a process of heat-treating the base material and [4] is a process of washing the base material surface with a fluorine-containing solvent. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><subject>ADHESIVES</subject><subject>APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL</subject><subject>CHEMICAL PAINT OR INK REMOVERS</subject><subject>CHEMISTRY</subject><subject>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</subject><subject>CORRECTING FLUIDS</subject><subject>DYES</subject><subject>FILLING PASTES</subject><subject>INKS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>PASTES OR SOLIDS FOR COLOURING OR PRINTING</subject><subject>PERFORMING OPERATIONS</subject><subject>POLISHES</subject><subject>PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL</subject><subject>SPRAYING OR ATOMISING IN GENERAL</subject><subject>TRANSPORTING</subject><subject>USE OF MATERIALS THEREFOR</subject><subject>WOODSTAINS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAQAHvxIOofFu-F1qLgcW03JpJsSroVPNUi8SRaqP9HCz7A08AwzDy5HrAhcCgUDFrQeDZ8BGVbHwxTWnoWNDy52tuLowCiDYMy1gFyBY5E-wqUD98JtwpLacOUiyZo0NEymd37xxhXPy6StSIpdRqHVxfHob_FZ3x3p3qT5Vle5NvdHou_og_SaDOu</recordid><startdate>20100617</startdate><enddate>20100617</enddate><creator>TAMITSUJI SHINYA</creator><creator>MINAMIDATE JUN</creator><creator>UENO KATSUYA</creator><creator>WATANABE KUNIO</creator><scope>EVB</scope></search><sort><creationdate>20100617</creationdate><title>BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME</title><author>TAMITSUJI SHINYA ; MINAMIDATE JUN ; UENO KATSUYA ; WATANABE KUNIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2010131569A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2010</creationdate><topic>ADHESIVES</topic><topic>APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL</topic><topic>CHEMICAL PAINT OR INK REMOVERS</topic><topic>CHEMISTRY</topic><topic>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</topic><topic>CORRECTING FLUIDS</topic><topic>DYES</topic><topic>FILLING PASTES</topic><topic>INKS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>PASTES OR SOLIDS FOR COLOURING OR PRINTING</topic><topic>PERFORMING OPERATIONS</topic><topic>POLISHES</topic><topic>PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL</topic><topic>SPRAYING OR ATOMISING IN GENERAL</topic><topic>TRANSPORTING</topic><topic>USE OF MATERIALS THEREFOR</topic><topic>WOODSTAINS</topic><toplevel>online_resources</toplevel><creatorcontrib>TAMITSUJI SHINYA</creatorcontrib><creatorcontrib>MINAMIDATE JUN</creatorcontrib><creatorcontrib>UENO KATSUYA</creatorcontrib><creatorcontrib>WATANABE KUNIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAMITSUJI SHINYA</au><au>MINAMIDATE JUN</au><au>UENO KATSUYA</au><au>WATANABE KUNIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME</title><date>2010-06-17</date><risdate>2010</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing a base material having, on its surface, a fluorine-containing polymer thin film which is excellent in adhesion with the base material, scratch resistance, mold-release resistance and an antifouling property, and has a fluorine-containing aliphatic ring structure. SOLUTION: In the method for manufacturing the base material having the fluorine-containing polymer thin film on its surface, following processes [1] to [4] are carried out in order of [1] to [4], wherein [1] is a process of treating the base material surface with a silane coupling agent having a polar functional group, [2] is a process of coating the base material surface with the fluorine-containing polymer which has a reactive functional group having reactivity with the polar functional group and has the fluorine-containing aliphatic ring structure in its main chain, [3] is a process of heat-treating the base material and [4] is a process of washing the base material surface with a fluorine-containing solvent. COPYRIGHT: (C)2010,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2010131569A
source esp@cenet
subjects ADHESIVES
APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
CHEMICAL PAINT OR INK REMOVERS
CHEMISTRY
COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS
CORRECTING FLUIDS
DYES
FILLING PASTES
INKS
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
PAINTS
PASTES OR SOLIDS FOR COLOURING OR PRINTING
PERFORMING OPERATIONS
POLISHES
PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL
SPRAYING OR ATOMISING IN GENERAL
TRANSPORTING
USE OF MATERIALS THEREFOR
WOODSTAINS
title BASE MATERIAL HAVING FLUORINE-CONTAINING POLYMER THIN FILM AND METHOD FOR MANUFACTURING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T21%3A01%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAMITSUJI%20SHINYA&rft.date=2010-06-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2010131569A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true