METHOD FOR ANODIZING ALUMINUM MEMBER

PROBLEM TO BE SOLVED: To provide a method for anodizing an aluminum member in which a formation rate of an anodized film is accelerated so that an anodization step can be carried out on-line and synchronized with other steps. SOLUTION: The method for anodizing the aluminum member includes the steps...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KOJIMA TOSHIYA, IO KENJI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KOJIMA TOSHIYA
IO KENJI
description PROBLEM TO BE SOLVED: To provide a method for anodizing an aluminum member in which a formation rate of an anodized film is accelerated so that an anodization step can be carried out on-line and synchronized with other steps. SOLUTION: The method for anodizing the aluminum member includes the steps of: immersing the aluminum member being the object to be treated in a treatment bath; sending a DC current to the treatment bath at an early stage until the bath voltage reaches a predetermined value (I); and sending a DC current with a superimposed AC current, in which a high-frequency current is superimposed on the DC current, to the treatment bath after the bath voltage reaches the predetermined value (II). The current density of the DC current is 50-120 A/dm2and the frequency of the high-frequency current is 5,000-15,000 Hz. COPYRIGHT: (C)2010,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2009235539A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2009235539A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2009235539A3</originalsourceid><addsrcrecordid>eNrjZFDxdQ3x8HdRcPMPUnD083fxjPL0c1dw9An19fQL9VXwdfV1cg3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaWRsampsaWjsZEKQIAv4Ejdg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR ANODIZING ALUMINUM MEMBER</title><source>esp@cenet</source><creator>KOJIMA TOSHIYA ; IO KENJI</creator><creatorcontrib>KOJIMA TOSHIYA ; IO KENJI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for anodizing an aluminum member in which a formation rate of an anodized film is accelerated so that an anodization step can be carried out on-line and synchronized with other steps. SOLUTION: The method for anodizing the aluminum member includes the steps of: immersing the aluminum member being the object to be treated in a treatment bath; sending a DC current to the treatment bath at an early stage until the bath voltage reaches a predetermined value (I); and sending a DC current with a superimposed AC current, in which a high-frequency current is superimposed on the DC current, to the treatment bath after the bath voltage reaches the predetermined value (II). The current density of the DC current is 50-120 A/dm2and the frequency of the high-frequency current is 5,000-15,000 Hz. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><language>eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091015&amp;DB=EPODOC&amp;CC=JP&amp;NR=2009235539A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091015&amp;DB=EPODOC&amp;CC=JP&amp;NR=2009235539A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KOJIMA TOSHIYA</creatorcontrib><creatorcontrib>IO KENJI</creatorcontrib><title>METHOD FOR ANODIZING ALUMINUM MEMBER</title><description>PROBLEM TO BE SOLVED: To provide a method for anodizing an aluminum member in which a formation rate of an anodized film is accelerated so that an anodization step can be carried out on-line and synchronized with other steps. SOLUTION: The method for anodizing the aluminum member includes the steps of: immersing the aluminum member being the object to be treated in a treatment bath; sending a DC current to the treatment bath at an early stage until the bath voltage reaches a predetermined value (I); and sending a DC current with a superimposed AC current, in which a high-frequency current is superimposed on the DC current, to the treatment bath after the bath voltage reaches the predetermined value (II). The current density of the DC current is 50-120 A/dm2and the frequency of the high-frequency current is 5,000-15,000 Hz. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDxdQ3x8HdRcPMPUnD083fxjPL0c1dw9An19fQL9VXwdfV1cg3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaWRsampsaWjsZEKQIAv4Ejdg</recordid><startdate>20091015</startdate><enddate>20091015</enddate><creator>KOJIMA TOSHIYA</creator><creator>IO KENJI</creator><scope>EVB</scope></search><sort><creationdate>20091015</creationdate><title>METHOD FOR ANODIZING ALUMINUM MEMBER</title><author>KOJIMA TOSHIYA ; IO KENJI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2009235539A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2009</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><toplevel>online_resources</toplevel><creatorcontrib>KOJIMA TOSHIYA</creatorcontrib><creatorcontrib>IO KENJI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KOJIMA TOSHIYA</au><au>IO KENJI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR ANODIZING ALUMINUM MEMBER</title><date>2009-10-15</date><risdate>2009</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for anodizing an aluminum member in which a formation rate of an anodized film is accelerated so that an anodization step can be carried out on-line and synchronized with other steps. SOLUTION: The method for anodizing the aluminum member includes the steps of: immersing the aluminum member being the object to be treated in a treatment bath; sending a DC current to the treatment bath at an early stage until the bath voltage reaches a predetermined value (I); and sending a DC current with a superimposed AC current, in which a high-frequency current is superimposed on the DC current, to the treatment bath after the bath voltage reaches the predetermined value (II). The current density of the DC current is 50-120 A/dm2and the frequency of the high-frequency current is 5,000-15,000 Hz. COPYRIGHT: (C)2010,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2009235539A
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROFORMING
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS
title METHOD FOR ANODIZING ALUMINUM MEMBER
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-16T03%3A12%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KOJIMA%20TOSHIYA&rft.date=2009-10-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2009235539A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true