ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM
PROBLEM TO BE SOLVED: To provide an ethylenic polymer having excellent moldability and easy openability, a thermoplastic resin composition containing the ethylenic polymer, a molded article and a film produced therefrom and a laminate film containing the film. SOLUTION: The ethylenic polymer satisfi...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | SUZUKI MASAO TANIFUJI DAISUKE SATO YASUO BANDO HIDEKI SEKIOKA HIROYU |
description | PROBLEM TO BE SOLVED: To provide an ethylenic polymer having excellent moldability and easy openability, a thermoplastic resin composition containing the ethylenic polymer, a molded article and a film produced therefrom and a laminate film containing the film. SOLUTION: The ethylenic polymer satisfies the following requirements (I) to (V) at the same time. (I) The ratio [MMe+Et/Mall] of the content [MMe+Et(mol%)] of the methyl branches and the ethyl branches determined by13C-NMR to the content [Mall(mol%)] of all branches determined by13C-NMR is 0.30-1.00; (II) the MFR (190°C, 2.16 kg-load) is 0.1-100 g/10 min; (III) the density is 875-970 kg/m3; (IV) the ratio [MT/η*(g/p)] of the melt tension (MT(g), 190°C) to the shear viscosity [η*(P), 200°C, 1.0 rad/sec] is 1.50×10-4to 9.00×10-4; and (V) the zero shear viscosity [η0(P), 200°C] and the weight-average molecular weight (Mw) determined by a GPC-viscosity detector method satisfy the relationship of 0.01×10-13×Mw3.4≤η0≤4.50×10-13×Mw3.4. COPYRIGHT: (C)2009,JPO&INPIT |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2009173798A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2009173798A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2009173798A3</originalsourceid><addsrcrecordid>eNqNjLEKwjAURbM4iPoPD2eFaoe2Y0hebSTJC2kcOpUicRIt1MW_twE3F6d7ORzOkr0xNJ1GqwQ40p1Bv4PQoDfkNG_DjD22yoIg46hVQVH6NnBllT0lFX4KwK0EQ1qiBO7nhkZwnuRFzCDFsfZk1mxxG-5T3Hx3xbY1BtHs4_js4zQO1_iIr_7sjllWHYq8qEqe_yV9AK1tO2M</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM</title><source>esp@cenet</source><creator>SUZUKI MASAO ; TANIFUJI DAISUKE ; SATO YASUO ; BANDO HIDEKI ; SEKIOKA HIROYU</creator><creatorcontrib>SUZUKI MASAO ; TANIFUJI DAISUKE ; SATO YASUO ; BANDO HIDEKI ; SEKIOKA HIROYU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide an ethylenic polymer having excellent moldability and easy openability, a thermoplastic resin composition containing the ethylenic polymer, a molded article and a film produced therefrom and a laminate film containing the film. SOLUTION: The ethylenic polymer satisfies the following requirements (I) to (V) at the same time. (I) The ratio [MMe+Et/Mall] of the content [MMe+Et(mol%)] of the methyl branches and the ethyl branches determined by13C-NMR to the content [Mall(mol%)] of all branches determined by13C-NMR is 0.30-1.00; (II) the MFR (190°C, 2.16 kg-load) is 0.1-100 g/10 min; (III) the density is 875-970 kg/m3; (IV) the ratio [MT/η*(g/p)] of the melt tension (MT(g), 190°C) to the shear viscosity [η*(P), 200°C, 1.0 rad/sec] is 1.50×10-4to 9.00×10-4; and (V) the zero shear viscosity [η0(P), 200°C] and the weight-average molecular weight (Mw) determined by a GPC-viscosity detector method satisfy the relationship of 0.01×10-13×Mw3.4≤η0≤4.50×10-13×Mw3.4. COPYRIGHT: (C)2009,JPO&INPIT</description><language>eng</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090806&DB=EPODOC&CC=JP&NR=2009173798A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090806&DB=EPODOC&CC=JP&NR=2009173798A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SUZUKI MASAO</creatorcontrib><creatorcontrib>TANIFUJI DAISUKE</creatorcontrib><creatorcontrib>SATO YASUO</creatorcontrib><creatorcontrib>BANDO HIDEKI</creatorcontrib><creatorcontrib>SEKIOKA HIROYU</creatorcontrib><title>ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM</title><description>PROBLEM TO BE SOLVED: To provide an ethylenic polymer having excellent moldability and easy openability, a thermoplastic resin composition containing the ethylenic polymer, a molded article and a film produced therefrom and a laminate film containing the film. SOLUTION: The ethylenic polymer satisfies the following requirements (I) to (V) at the same time. (I) The ratio [MMe+Et/Mall] of the content [MMe+Et(mol%)] of the methyl branches and the ethyl branches determined by13C-NMR to the content [Mall(mol%)] of all branches determined by13C-NMR is 0.30-1.00; (II) the MFR (190°C, 2.16 kg-load) is 0.1-100 g/10 min; (III) the density is 875-970 kg/m3; (IV) the ratio [MT/η*(g/p)] of the melt tension (MT(g), 190°C) to the shear viscosity [η*(P), 200°C, 1.0 rad/sec] is 1.50×10-4to 9.00×10-4; and (V) the zero shear viscosity [η0(P), 200°C] and the weight-average molecular weight (Mw) determined by a GPC-viscosity detector method satisfy the relationship of 0.01×10-13×Mw3.4≤η0≤4.50×10-13×Mw3.4. COPYRIGHT: (C)2009,JPO&INPIT</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEKwjAURbM4iPoPD2eFaoe2Y0hebSTJC2kcOpUicRIt1MW_twE3F6d7ORzOkr0xNJ1GqwQ40p1Bv4PQoDfkNG_DjD22yoIg46hVQVH6NnBllT0lFX4KwK0EQ1qiBO7nhkZwnuRFzCDFsfZk1mxxG-5T3Hx3xbY1BtHs4_js4zQO1_iIr_7sjllWHYq8qEqe_yV9AK1tO2M</recordid><startdate>20090806</startdate><enddate>20090806</enddate><creator>SUZUKI MASAO</creator><creator>TANIFUJI DAISUKE</creator><creator>SATO YASUO</creator><creator>BANDO HIDEKI</creator><creator>SEKIOKA HIROYU</creator><scope>EVB</scope></search><sort><creationdate>20090806</creationdate><title>ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM</title><author>SUZUKI MASAO ; TANIFUJI DAISUKE ; SATO YASUO ; BANDO HIDEKI ; SEKIOKA HIROYU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2009173798A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2009</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>SUZUKI MASAO</creatorcontrib><creatorcontrib>TANIFUJI DAISUKE</creatorcontrib><creatorcontrib>SATO YASUO</creatorcontrib><creatorcontrib>BANDO HIDEKI</creatorcontrib><creatorcontrib>SEKIOKA HIROYU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SUZUKI MASAO</au><au>TANIFUJI DAISUKE</au><au>SATO YASUO</au><au>BANDO HIDEKI</au><au>SEKIOKA HIROYU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM</title><date>2009-08-06</date><risdate>2009</risdate><abstract>PROBLEM TO BE SOLVED: To provide an ethylenic polymer having excellent moldability and easy openability, a thermoplastic resin composition containing the ethylenic polymer, a molded article and a film produced therefrom and a laminate film containing the film. SOLUTION: The ethylenic polymer satisfies the following requirements (I) to (V) at the same time. (I) The ratio [MMe+Et/Mall] of the content [MMe+Et(mol%)] of the methyl branches and the ethyl branches determined by13C-NMR to the content [Mall(mol%)] of all branches determined by13C-NMR is 0.30-1.00; (II) the MFR (190°C, 2.16 kg-load) is 0.1-100 g/10 min; (III) the density is 875-970 kg/m3; (IV) the ratio [MT/η*(g/p)] of the melt tension (MT(g), 190°C) to the shear viscosity [η*(P), 200°C, 1.0 rad/sec] is 1.50×10-4to 9.00×10-4; and (V) the zero shear viscosity [η0(P), 200°C] and the weight-average molecular weight (Mw) determined by a GPC-viscosity detector method satisfy the relationship of 0.01×10-13×Mw3.4≤η0≤4.50×10-13×Mw3.4. COPYRIGHT: (C)2009,JPO&INPIT</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2009173798A |
source | esp@cenet |
subjects | AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G CHEMISTRY COMPOSITIONS BASED THEREON GENERAL PROCESSES OF COMPOUNDING MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP WORKING-UP |
title | ETHYLENIC POLYMER, THERMOPLASTIC RESIN COMPOSITION CONTAINING THE ETHYLENIC POLYMER AND MOLDED ARTICLE PRODUCED THEREFROM |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T13%3A21%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SUZUKI%20MASAO&rft.date=2009-08-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2009173798A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |