NICKEL MATERIAL AND REFINING METHOD THEREOF
PROBLEM TO BE SOLVED: To provide a nickel material excellent in hot workability, and a method for stably producing the nickel material. SOLUTION: The nickel material has a chemical composition including, by mass, 0.0050-0.0150% Mg, 0.0001-0.0010% S, 0.020-0.100% Al, at least one element chosen from...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HOSOI TAKEO |
description | PROBLEM TO BE SOLVED: To provide a nickel material excellent in hot workability, and a method for stably producing the nickel material. SOLUTION: The nickel material has a chemical composition including, by mass, 0.0050-0.0150% Mg, 0.0001-0.0010% S, 0.020-0.100% Al, at least one element chosen from the group consisting of ≤0.05% Ti, ≤0.30% Mn, ≤0.40% Fe, ≤0.0030% B and ≤0.02% C and the balance being Ni and impurities, wherein the ΔS parameter (S-0.3×Mg) is within the range of -0.0011% to -0.0030%. The chemical composition can be stably obtained by carrying out ladle refining using a slag, in which the slag basicity (T. CaO/Al2O3) is ≤2.6 and the MgO concentration is equal to or larger than 4.0 mass% but smaller than 12.0 mass%, provided that the components are adjusted so as to achieve an oxygen activity ao, which is represented by formula (1)(not indicated in a figure), of 0.70-1.30. COPYRIGHT: (C)2009,JPO&INPIT |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2009024241A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2009024241A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2009024241A3</originalsourceid><addsrcrecordid>eNrjZND283T2dvVR8HUMcQ3ydPRRcPRzUQhydfP08_RzV_B1DfHwd1EI8XANcvV342FgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGlgZGJkYmho7GRCkCAJ_SJQ4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>NICKEL MATERIAL AND REFINING METHOD THEREOF</title><source>esp@cenet</source><creator>HOSOI TAKEO</creator><creatorcontrib>HOSOI TAKEO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a nickel material excellent in hot workability, and a method for stably producing the nickel material. SOLUTION: The nickel material has a chemical composition including, by mass, 0.0050-0.0150% Mg, 0.0001-0.0010% S, 0.020-0.100% Al, at least one element chosen from the group consisting of ≤0.05% Ti, ≤0.30% Mn, ≤0.40% Fe, ≤0.0030% B and ≤0.02% C and the balance being Ni and impurities, wherein the ΔS parameter (S-0.3×Mg) is within the range of -0.0011% to -0.0030%. The chemical composition can be stably obtained by carrying out ladle refining using a slag, in which the slag basicity (T. CaO/Al2O3) is ≤2.6 and the MgO concentration is equal to or larger than 4.0 mass% but smaller than 12.0 mass%, provided that the components are adjusted so as to achieve an oxygen activity ao, which is represented by formula (1)(not indicated in a figure), of 0.70-1.30. COPYRIGHT: (C)2009,JPO&INPIT</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090205&DB=EPODOC&CC=JP&NR=2009024241A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090205&DB=EPODOC&CC=JP&NR=2009024241A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HOSOI TAKEO</creatorcontrib><title>NICKEL MATERIAL AND REFINING METHOD THEREOF</title><description>PROBLEM TO BE SOLVED: To provide a nickel material excellent in hot workability, and a method for stably producing the nickel material. SOLUTION: The nickel material has a chemical composition including, by mass, 0.0050-0.0150% Mg, 0.0001-0.0010% S, 0.020-0.100% Al, at least one element chosen from the group consisting of ≤0.05% Ti, ≤0.30% Mn, ≤0.40% Fe, ≤0.0030% B and ≤0.02% C and the balance being Ni and impurities, wherein the ΔS parameter (S-0.3×Mg) is within the range of -0.0011% to -0.0030%. The chemical composition can be stably obtained by carrying out ladle refining using a slag, in which the slag basicity (T. CaO/Al2O3) is ≤2.6 and the MgO concentration is equal to or larger than 4.0 mass% but smaller than 12.0 mass%, provided that the components are adjusted so as to achieve an oxygen activity ao, which is represented by formula (1)(not indicated in a figure), of 0.70-1.30. COPYRIGHT: (C)2009,JPO&INPIT</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND283T2dvVR8HUMcQ3ydPRRcPRzUQhydfP08_RzV_B1DfHwd1EI8XANcvV342FgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGlgZGJkYmho7GRCkCAJ_SJQ4</recordid><startdate>20090205</startdate><enddate>20090205</enddate><creator>HOSOI TAKEO</creator><scope>EVB</scope></search><sort><creationdate>20090205</creationdate><title>NICKEL MATERIAL AND REFINING METHOD THEREOF</title><author>HOSOI TAKEO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2009024241A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2009</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>HOSOI TAKEO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HOSOI TAKEO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>NICKEL MATERIAL AND REFINING METHOD THEREOF</title><date>2009-02-05</date><risdate>2009</risdate><abstract>PROBLEM TO BE SOLVED: To provide a nickel material excellent in hot workability, and a method for stably producing the nickel material. SOLUTION: The nickel material has a chemical composition including, by mass, 0.0050-0.0150% Mg, 0.0001-0.0010% S, 0.020-0.100% Al, at least one element chosen from the group consisting of ≤0.05% Ti, ≤0.30% Mn, ≤0.40% Fe, ≤0.0030% B and ≤0.02% C and the balance being Ni and impurities, wherein the ΔS parameter (S-0.3×Mg) is within the range of -0.0011% to -0.0030%. The chemical composition can be stably obtained by carrying out ladle refining using a slag, in which the slag basicity (T. CaO/Al2O3) is ≤2.6 and the MgO concentration is equal to or larger than 4.0 mass% but smaller than 12.0 mass%, provided that the components are adjusted so as to achieve an oxygen activity ao, which is represented by formula (1)(not indicated in a figure), of 0.70-1.30. COPYRIGHT: (C)2009,JPO&INPIT</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2009024241A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | NICKEL MATERIAL AND REFINING METHOD THEREOF |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T02%3A48%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HOSOI%20TAKEO&rft.date=2009-02-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2009024241A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |