CONTINUOUS CASTING METHOD OF STEEL
PROBLEM TO BE SOLVED: To provide the continuous casting method of steel, with which, when molten steel 6 is continuously cast using a continuous casting machine 1 provided with a light rolling reduction zone composed of two or more pairs of rolls 4A, 4B for applying rolling reduction force to a slab...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | KUSUMOTO MUNENORI OSUMI AKIRA ODA HIDEKAZU ITAKURA TAKASHI |
description | PROBLEM TO BE SOLVED: To provide the continuous casting method of steel, with which, when molten steel 6 is continuously cast using a continuous casting machine 1 provided with a light rolling reduction zone composed of two or more pairs of rolls 4A, 4B for applying rolling reduction force to a slab 7, and when a boundary between a dummy bar head 15 and the bottommost slab 7A passes through the slight rolling reduction zone 11, variation in the molten metal surface 10 of the molten steel in a mold 3 and bulging of the slab 7 in the vicinity of the boundary caused by the discharging resistance owing to the narrowing in the intervals of the rolls can be jointly prevented. SOLUTION: When the outflow of hydraulic oil from a hydraulic cylinder 16 for applying rolling reduction force to the slab 7 by the rolls 4A, 4B reaches a fixed value or above, rolling reduction force is applied to the slab 7 by the rolls 4A, 4B. COPYRIGHT: (C)2009,JPO&INPIT |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2008290113A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2008290113A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2008290113A3</originalsourceid><addsrcrecordid>eNrjZFBy9vcL8fQL9Q8NVnB2DAYy3RV8XUM8_F0U_N0UgkNcXX14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgYGFkaWBoaGxozFRigCEeyLk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CONTINUOUS CASTING METHOD OF STEEL</title><source>esp@cenet</source><creator>KUSUMOTO MUNENORI ; OSUMI AKIRA ; ODA HIDEKAZU ; ITAKURA TAKASHI</creator><creatorcontrib>KUSUMOTO MUNENORI ; OSUMI AKIRA ; ODA HIDEKAZU ; ITAKURA TAKASHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide the continuous casting method of steel, with which, when molten steel 6 is continuously cast using a continuous casting machine 1 provided with a light rolling reduction zone composed of two or more pairs of rolls 4A, 4B for applying rolling reduction force to a slab 7, and when a boundary between a dummy bar head 15 and the bottommost slab 7A passes through the slight rolling reduction zone 11, variation in the molten metal surface 10 of the molten steel in a mold 3 and bulging of the slab 7 in the vicinity of the boundary caused by the discharging resistance owing to the narrowing in the intervals of the rolls can be jointly prevented. SOLUTION: When the outflow of hydraulic oil from a hydraulic cylinder 16 for applying rolling reduction force to the slab 7 by the rolls 4A, 4B reaches a fixed value or above, rolling reduction force is applied to the slab 7 by the rolls 4A, 4B. COPYRIGHT: (C)2009,JPO&INPIT</description><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20081204&DB=EPODOC&CC=JP&NR=2008290113A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20081204&DB=EPODOC&CC=JP&NR=2008290113A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUSUMOTO MUNENORI</creatorcontrib><creatorcontrib>OSUMI AKIRA</creatorcontrib><creatorcontrib>ODA HIDEKAZU</creatorcontrib><creatorcontrib>ITAKURA TAKASHI</creatorcontrib><title>CONTINUOUS CASTING METHOD OF STEEL</title><description>PROBLEM TO BE SOLVED: To provide the continuous casting method of steel, with which, when molten steel 6 is continuously cast using a continuous casting machine 1 provided with a light rolling reduction zone composed of two or more pairs of rolls 4A, 4B for applying rolling reduction force to a slab 7, and when a boundary between a dummy bar head 15 and the bottommost slab 7A passes through the slight rolling reduction zone 11, variation in the molten metal surface 10 of the molten steel in a mold 3 and bulging of the slab 7 in the vicinity of the boundary caused by the discharging resistance owing to the narrowing in the intervals of the rolls can be jointly prevented. SOLUTION: When the outflow of hydraulic oil from a hydraulic cylinder 16 for applying rolling reduction force to the slab 7 by the rolls 4A, 4B reaches a fixed value or above, rolling reduction force is applied to the slab 7 by the rolls 4A, 4B. COPYRIGHT: (C)2009,JPO&INPIT</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFBy9vcL8fQL9Q8NVnB2DAYy3RV8XUM8_F0U_N0UgkNcXX14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgYGFkaWBoaGxozFRigCEeyLk</recordid><startdate>20081204</startdate><enddate>20081204</enddate><creator>KUSUMOTO MUNENORI</creator><creator>OSUMI AKIRA</creator><creator>ODA HIDEKAZU</creator><creator>ITAKURA TAKASHI</creator><scope>EVB</scope></search><sort><creationdate>20081204</creationdate><title>CONTINUOUS CASTING METHOD OF STEEL</title><author>KUSUMOTO MUNENORI ; OSUMI AKIRA ; ODA HIDEKAZU ; ITAKURA TAKASHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2008290113A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2008</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KUSUMOTO MUNENORI</creatorcontrib><creatorcontrib>OSUMI AKIRA</creatorcontrib><creatorcontrib>ODA HIDEKAZU</creatorcontrib><creatorcontrib>ITAKURA TAKASHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUSUMOTO MUNENORI</au><au>OSUMI AKIRA</au><au>ODA HIDEKAZU</au><au>ITAKURA TAKASHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CONTINUOUS CASTING METHOD OF STEEL</title><date>2008-12-04</date><risdate>2008</risdate><abstract>PROBLEM TO BE SOLVED: To provide the continuous casting method of steel, with which, when molten steel 6 is continuously cast using a continuous casting machine 1 provided with a light rolling reduction zone composed of two or more pairs of rolls 4A, 4B for applying rolling reduction force to a slab 7, and when a boundary between a dummy bar head 15 and the bottommost slab 7A passes through the slight rolling reduction zone 11, variation in the molten metal surface 10 of the molten steel in a mold 3 and bulging of the slab 7 in the vicinity of the boundary caused by the discharging resistance owing to the narrowing in the intervals of the rolls can be jointly prevented. SOLUTION: When the outflow of hydraulic oil from a hydraulic cylinder 16 for applying rolling reduction force to the slab 7 by the rolls 4A, 4B reaches a fixed value or above, rolling reduction force is applied to the slab 7 by the rolls 4A, 4B. COPYRIGHT: (C)2009,JPO&INPIT</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2008290113A |
source | esp@cenet |
subjects | CASTING CASTING OF METALS CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES PERFORMING OPERATIONS POWDER METALLURGY TRANSPORTING |
title | CONTINUOUS CASTING METHOD OF STEEL |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T07%3A14%3A33IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUSUMOTO%20MUNENORI&rft.date=2008-12-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2008290113A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |