CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD

PROBLEM TO BE SOLVED: To provide a low expansion crystallized glass of a milk white color or white color having excellent light diffusion characteristics, a crystallized glass member and their manufacturing method. SOLUTION: The crystallized glass contains each component of 50-62% SiO2, 22-26% Al2O3...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: NAMIKAWA HIROYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NAMIKAWA HIROYUKI
description PROBLEM TO BE SOLVED: To provide a low expansion crystallized glass of a milk white color or white color having excellent light diffusion characteristics, a crystallized glass member and their manufacturing method. SOLUTION: The crystallized glass contains each component of 50-62% SiO2, 22-26% Al2O3, 3-5% Li2O by mass%, an average crystal particle diameter of a crystalline phase is more than 100 nm and an average line expansion coefficient is ≤30×10-7/°C in a temperature range of 0 to 50°C. The manufacturing method contains a process for melting a glass raw material, a process for forming the molten glass, a process for gradually cooling the formed glass, a process for subjecting a first heat treatment for 0.1-200 hr at 650-750°C after gradual cooling and a second heat treatment for 0.1-50 hr at 800-1,000°C after the first heat treatment. COPYRIGHT: (C)2006,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2006232661A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2006232661A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2006232661A3</originalsourceid><addsrcrecordid>eNrjZNB3DooMDnH08fGMcnVRcPdxDA5WcPRzUfAMCVbwdfQLdXN0DgkN8vRzV_B1DfHwd-FhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBmZGxkZmZoaOxkQpAgBjkyaO</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD</title><source>esp@cenet</source><creator>NAMIKAWA HIROYUKI</creator><creatorcontrib>NAMIKAWA HIROYUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a low expansion crystallized glass of a milk white color or white color having excellent light diffusion characteristics, a crystallized glass member and their manufacturing method. SOLUTION: The crystallized glass contains each component of 50-62% SiO2, 22-26% Al2O3, 3-5% Li2O by mass%, an average crystal particle diameter of a crystalline phase is more than 100 nm and an average line expansion coefficient is ≤30×10-7/°C in a temperature range of 0 to 50°C. The manufacturing method contains a process for melting a glass raw material, a process for forming the molten glass, a process for gradually cooling the formed glass, a process for subjecting a first heat treatment for 0.1-200 hr at 650-750°C after gradual cooling and a second heat treatment for 0.1-50 hr at 800-1,000°C after the first heat treatment. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PHYSICS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060907&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006232661A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060907&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006232661A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NAMIKAWA HIROYUKI</creatorcontrib><title>CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD</title><description>PROBLEM TO BE SOLVED: To provide a low expansion crystallized glass of a milk white color or white color having excellent light diffusion characteristics, a crystallized glass member and their manufacturing method. SOLUTION: The crystallized glass contains each component of 50-62% SiO2, 22-26% Al2O3, 3-5% Li2O by mass%, an average crystal particle diameter of a crystalline phase is more than 100 nm and an average line expansion coefficient is ≤30×10-7/°C in a temperature range of 0 to 50°C. The manufacturing method contains a process for melting a glass raw material, a process for forming the molten glass, a process for gradually cooling the formed glass, a process for subjecting a first heat treatment for 0.1-200 hr at 650-750°C after gradual cooling and a second heat treatment for 0.1-50 hr at 800-1,000°C after the first heat treatment. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNB3DooMDnH08fGMcnVRcPdxDA5WcPRzUfAMCVbwdfQLdXN0DgkN8vRzV_B1DfHwd-FhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBmZGxkZmZoaOxkQpAgBjkyaO</recordid><startdate>20060907</startdate><enddate>20060907</enddate><creator>NAMIKAWA HIROYUKI</creator><scope>EVB</scope></search><sort><creationdate>20060907</creationdate><title>CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD</title><author>NAMIKAWA HIROYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2006232661A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2006</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>NAMIKAWA HIROYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NAMIKAWA HIROYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD</title><date>2006-09-07</date><risdate>2006</risdate><abstract>PROBLEM TO BE SOLVED: To provide a low expansion crystallized glass of a milk white color or white color having excellent light diffusion characteristics, a crystallized glass member and their manufacturing method. SOLUTION: The crystallized glass contains each component of 50-62% SiO2, 22-26% Al2O3, 3-5% Li2O by mass%, an average crystal particle diameter of a crystalline phase is more than 100 nm and an average line expansion coefficient is ≤30×10-7/°C in a temperature range of 0 to 50°C. The manufacturing method contains a process for melting a glass raw material, a process for forming the molten glass, a process for gradually cooling the formed glass, a process for subjecting a first heat treatment for 0.1-200 hr at 650-750°C after gradual cooling and a second heat treatment for 0.1-50 hr at 800-1,000°C after the first heat treatment. COPYRIGHT: (C)2006,JPO&amp;NCIPI</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2006232661A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
PHYSICS
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title CRYSTALLIZED GLASS AND ITS MANUFACTURING METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T21%3A16%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NAMIKAWA%20HIROYUKI&rft.date=2006-09-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2006232661A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true