METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE

PROBLEM TO BE SOLVED: To provide technology for forming a coating of a self-fluxing alloy having a high surface hardness on the inner circumferential surface of a cylindrical member body. SOLUTION: After horizontally placing cylindrical member body 1, a self-fluxing alloy powder in an amount corresp...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKEYA AKIHIRO, TADA FUMIAKI, WATANABE YASUO, YATABE KENJI, NISHIBABA KAZUNORI, SOJI YOSHINOBU, TANABE MICHIO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAKEYA AKIHIRO
TADA FUMIAKI
WATANABE YASUO
YATABE KENJI
NISHIBABA KAZUNORI
SOJI YOSHINOBU
TANABE MICHIO
description PROBLEM TO BE SOLVED: To provide technology for forming a coating of a self-fluxing alloy having a high surface hardness on the inner circumferential surface of a cylindrical member body. SOLUTION: After horizontally placing cylindrical member body 1, a self-fluxing alloy powder in an amount corresponding to a thickness of coating is disposed on the inside of the cylindrical member equally in its axial direction. Then, the cylindrical member body 1 is rotated at high speed to form a powder layer with a uniform thickness on the inner circumferential surface. After that, the cylindrical member body 1 is heated to melt the powder therein and to form a molten metal layer, which is later cooled and solidified to form a coating a coating on the inner surface. When the self-fluxing alloy is melted and solidified, an atmospheric pressure of 0.3-3 MPa is applied on the surface of the molten metal layer located on the inner circumferential surface of the cylindrical member body 1 and the rotation speed of the cylindrical member body is controlled so as to generate a centrifugal force of not less than 10G on the inner circumferential surface, so that the surface harness of the coating on the inner surface can be increased, while preventing the occurrence of pinholes. COPYRIGHT: (C)2006,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2006075906A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2006075906A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2006075906A3</originalsourceid><addsrcrecordid>eNrjZHD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcI708fRzCfJ0dvRR8HX1dXINUgj3DPFQcPZ3DHF1UfD08wOKBIcGAXW48jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDMwNzU0sDM0djohQBANtVLHk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE</title><source>esp@cenet</source><creator>TAKEYA AKIHIRO ; TADA FUMIAKI ; WATANABE YASUO ; YATABE KENJI ; NISHIBABA KAZUNORI ; SOJI YOSHINOBU ; TANABE MICHIO</creator><creatorcontrib>TAKEYA AKIHIRO ; TADA FUMIAKI ; WATANABE YASUO ; YATABE KENJI ; NISHIBABA KAZUNORI ; SOJI YOSHINOBU ; TANABE MICHIO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide technology for forming a coating of a self-fluxing alloy having a high surface hardness on the inner circumferential surface of a cylindrical member body. SOLUTION: After horizontally placing cylindrical member body 1, a self-fluxing alloy powder in an amount corresponding to a thickness of coating is disposed on the inside of the cylindrical member equally in its axial direction. Then, the cylindrical member body 1 is rotated at high speed to form a powder layer with a uniform thickness on the inner circumferential surface. After that, the cylindrical member body 1 is heated to melt the powder therein and to form a molten metal layer, which is later cooled and solidified to form a coating a coating on the inner surface. When the self-fluxing alloy is melted and solidified, an atmospheric pressure of 0.3-3 MPa is applied on the surface of the molten metal layer located on the inner circumferential surface of the cylindrical member body 1 and the rotation speed of the cylindrical member body is controlled so as to generate a centrifugal force of not less than 10G on the inner circumferential surface, so that the surface harness of the coating on the inner surface can be increased, while preventing the occurrence of pinholes. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><language>eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060323&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006075906A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060323&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006075906A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKEYA AKIHIRO</creatorcontrib><creatorcontrib>TADA FUMIAKI</creatorcontrib><creatorcontrib>WATANABE YASUO</creatorcontrib><creatorcontrib>YATABE KENJI</creatorcontrib><creatorcontrib>NISHIBABA KAZUNORI</creatorcontrib><creatorcontrib>SOJI YOSHINOBU</creatorcontrib><creatorcontrib>TANABE MICHIO</creatorcontrib><title>METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE</title><description>PROBLEM TO BE SOLVED: To provide technology for forming a coating of a self-fluxing alloy having a high surface hardness on the inner circumferential surface of a cylindrical member body. SOLUTION: After horizontally placing cylindrical member body 1, a self-fluxing alloy powder in an amount corresponding to a thickness of coating is disposed on the inside of the cylindrical member equally in its axial direction. Then, the cylindrical member body 1 is rotated at high speed to form a powder layer with a uniform thickness on the inner circumferential surface. After that, the cylindrical member body 1 is heated to melt the powder therein and to form a molten metal layer, which is later cooled and solidified to form a coating a coating on the inner surface. When the self-fluxing alloy is melted and solidified, an atmospheric pressure of 0.3-3 MPa is applied on the surface of the molten metal layer located on the inner circumferential surface of the cylindrical member body 1 and the rotation speed of the cylindrical member body is controlled so as to generate a centrifugal force of not less than 10G on the inner circumferential surface, so that the surface harness of the coating on the inner surface can be increased, while preventing the occurrence of pinholes. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcI708fRzCfJ0dvRR8HX1dXINUgj3DPFQcPZ3DHF1UfD08wOKBIcGAXW48jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDMwNzU0sDM0djohQBANtVLHk</recordid><startdate>20060323</startdate><enddate>20060323</enddate><creator>TAKEYA AKIHIRO</creator><creator>TADA FUMIAKI</creator><creator>WATANABE YASUO</creator><creator>YATABE KENJI</creator><creator>NISHIBABA KAZUNORI</creator><creator>SOJI YOSHINOBU</creator><creator>TANABE MICHIO</creator><scope>EVB</scope></search><sort><creationdate>20060323</creationdate><title>METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE</title><author>TAKEYA AKIHIRO ; TADA FUMIAKI ; WATANABE YASUO ; YATABE KENJI ; NISHIBABA KAZUNORI ; SOJI YOSHINOBU ; TANABE MICHIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2006075906A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2006</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKEYA AKIHIRO</creatorcontrib><creatorcontrib>TADA FUMIAKI</creatorcontrib><creatorcontrib>WATANABE YASUO</creatorcontrib><creatorcontrib>YATABE KENJI</creatorcontrib><creatorcontrib>NISHIBABA KAZUNORI</creatorcontrib><creatorcontrib>SOJI YOSHINOBU</creatorcontrib><creatorcontrib>TANABE MICHIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKEYA AKIHIRO</au><au>TADA FUMIAKI</au><au>WATANABE YASUO</au><au>YATABE KENJI</au><au>NISHIBABA KAZUNORI</au><au>SOJI YOSHINOBU</au><au>TANABE MICHIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE</title><date>2006-03-23</date><risdate>2006</risdate><abstract>PROBLEM TO BE SOLVED: To provide technology for forming a coating of a self-fluxing alloy having a high surface hardness on the inner circumferential surface of a cylindrical member body. SOLUTION: After horizontally placing cylindrical member body 1, a self-fluxing alloy powder in an amount corresponding to a thickness of coating is disposed on the inside of the cylindrical member equally in its axial direction. Then, the cylindrical member body 1 is rotated at high speed to form a powder layer with a uniform thickness on the inner circumferential surface. After that, the cylindrical member body 1 is heated to melt the powder therein and to form a molten metal layer, which is later cooled and solidified to form a coating a coating on the inner surface. When the self-fluxing alloy is melted and solidified, an atmospheric pressure of 0.3-3 MPa is applied on the surface of the molten metal layer located on the inner circumferential surface of the cylindrical member body 1 and the rotation speed of the cylindrical member body is controlled so as to generate a centrifugal force of not less than 10G on the inner circumferential surface, so that the surface harness of the coating on the inner surface can be increased, while preventing the occurrence of pinholes. COPYRIGHT: (C)2006,JPO&amp;NCIPI</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2006075906A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title METHOD FOR MANUFACTURING CYLINDRICAL MEMBER WITH COATED INNER SURFACE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-12T21%3A45%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKEYA%20AKIHIRO&rft.date=2006-03-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2006075906A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true