KNITTED CLOTH

PROBLEM TO BE SOLVED: To solve the problems wherein a chalk mark appears and reduces the surface appearance quality when a knitted cloth easily causing the chalk mark is subjected to a resin finishing with inorganic particles having functionality. SOLUTION: The usually observed chalk mark is reduced...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SEKI MASAO, OKAJIMA KATSUYA, HASEYAMA AYA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SEKI MASAO
OKAJIMA KATSUYA
HASEYAMA AYA
description PROBLEM TO BE SOLVED: To solve the problems wherein a chalk mark appears and reduces the surface appearance quality when a knitted cloth easily causing the chalk mark is subjected to a resin finishing with inorganic particles having functionality. SOLUTION: The usually observed chalk mark is reduced by attaching the inorganic particles and an acrylic resin having a silicone segment to the knitted fabric having ≥100 total of a warp density and a weft density. COPYRIGHT: (C)2006,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2006070378A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2006070378A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2006070378A3</originalsourceid><addsrcrecordid>eNrjZOD19vMMCXF1UXD28Q_x4GFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGZgbmBsbmFo7GRCkCAOJeHRc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>KNITTED CLOTH</title><source>esp@cenet</source><creator>SEKI MASAO ; OKAJIMA KATSUYA ; HASEYAMA AYA</creator><creatorcontrib>SEKI MASAO ; OKAJIMA KATSUYA ; HASEYAMA AYA</creatorcontrib><description>PROBLEM TO BE SOLVED: To solve the problems wherein a chalk mark appears and reduces the surface appearance quality when a knitted cloth easily causing the chalk mark is subjected to a resin finishing with inorganic particles having functionality. SOLUTION: The usually observed chalk mark is reduced by attaching the inorganic particles and an acrylic resin having a silicone segment to the knitted fabric having ≥100 total of a warp density and a weft density. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><language>eng</language><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060316&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006070378A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060316&amp;DB=EPODOC&amp;CC=JP&amp;NR=2006070378A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SEKI MASAO</creatorcontrib><creatorcontrib>OKAJIMA KATSUYA</creatorcontrib><creatorcontrib>HASEYAMA AYA</creatorcontrib><title>KNITTED CLOTH</title><description>PROBLEM TO BE SOLVED: To solve the problems wherein a chalk mark appears and reduces the surface appearance quality when a knitted cloth easily causing the chalk mark is subjected to a resin finishing with inorganic particles having functionality. SOLUTION: The usually observed chalk mark is reduced by attaching the inorganic particles and an acrylic resin having a silicone segment to the knitted fabric having ≥100 total of a warp density and a weft density. COPYRIGHT: (C)2006,JPO&amp;NCIPI</description><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOD19vMMCXF1UXD28Q_x4GFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgYGZgbmBsbmFo7GRCkCAOJeHRc</recordid><startdate>20060316</startdate><enddate>20060316</enddate><creator>SEKI MASAO</creator><creator>OKAJIMA KATSUYA</creator><creator>HASEYAMA AYA</creator><scope>EVB</scope></search><sort><creationdate>20060316</creationdate><title>KNITTED CLOTH</title><author>SEKI MASAO ; OKAJIMA KATSUYA ; HASEYAMA AYA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2006070378A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2006</creationdate><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><toplevel>online_resources</toplevel><creatorcontrib>SEKI MASAO</creatorcontrib><creatorcontrib>OKAJIMA KATSUYA</creatorcontrib><creatorcontrib>HASEYAMA AYA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SEKI MASAO</au><au>OKAJIMA KATSUYA</au><au>HASEYAMA AYA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>KNITTED CLOTH</title><date>2006-03-16</date><risdate>2006</risdate><abstract>PROBLEM TO BE SOLVED: To solve the problems wherein a chalk mark appears and reduces the surface appearance quality when a knitted cloth easily causing the chalk mark is subjected to a resin finishing with inorganic particles having functionality. SOLUTION: The usually observed chalk mark is reduced by attaching the inorganic particles and an acrylic resin having a silicone segment to the knitted fabric having ≥100 total of a warp density and a weft density. COPYRIGHT: (C)2006,JPO&amp;NCIPI</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2006070378A
source esp@cenet
subjects FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR
LAUNDERING
TEXTILES
TREATMENT OF TEXTILES OR THE LIKE
TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS
title KNITTED CLOTH
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T21%3A26%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SEKI%20MASAO&rft.date=2006-03-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2006070378A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true