CEMENT ADMIXTURE, FIBER REINFORCED CEMENT MATERIAL, FIBER REINFORCED CEMENT MEMBER, AND METHOD FOR MANUFACTURING FIBER REINFORCED CEMENT MEMBER
PROBLEM TO BE SOLVED: To provide a cement member having strength sufficient for practicable use and has durability by using casting waste sand as a mixing raw material. SOLUTION: The cement admixture contains casting sand of 95 to 100wt% in particles below a grain size 150 μm, ≤50 μm in 50% volume c...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a cement member having strength sufficient for practicable use and has durability by using casting waste sand as a mixing raw material. SOLUTION: The cement admixture contains casting sand of 95 to 100wt% in particles below a grain size 150 μm, ≤50 μm in 50% volume cumulative particle diameter, ≥60wt% in the ratio of siliceous component in terms of SiO2, and ≤5.5wt% ignition loss. The fiber reinforced cement material containing (a) 3 to 30wt% cement admixture, (b) 20 to 40wt% cement, (c) 20 to 45wt% siliceous raw material, (d) 0 to 45wt% filler, and (e) 3 to 15wt% fibrous material. The method for manufacturing the fiber reinforced cement member includes a process of obtaining (1) the hydraulic composition by kneading the fiber reinforced cement material, the cement material, and water, (2) a process of forming a molding by molding the hydraulic composition, and (3) a process of hydrothermally curing the molding. COPYRIGHT: (C)2006,JPO&NCIPI |
---|