METHOD FOR CONTINUOUSLY CASTING STEEL

PROBLEM TO BE SOLVED: To provide a method for continuously casting steel by which the sticking of alumina etc., on the inner surface of an immersion nozzle is reliably prevented and a cast slab having good surface quality can be obtained. SOLUTION: In the method for continuously casting extra-low ca...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KATO TORU, MUTO AKIFUMI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KATO TORU
MUTO AKIFUMI
description PROBLEM TO BE SOLVED: To provide a method for continuously casting steel by which the sticking of alumina etc., on the inner surface of an immersion nozzle is reliably prevented and a cast slab having good surface quality can be obtained. SOLUTION: In the method for continuously casting extra-low carbon steel, at least part of the inner surface of the immersion nozzle for supplying the molten steel from a tundish into a mold is constituted of a refractory containing alumina and graphite as the main components. While supplying the electric power from the immersion nozzle into the molten steel stream in the inner part, the continuous casting is performed. The potential difference between the immersion nozzle and the ground is made to be 0.5 to 5.0 V. COPYRIGHT: (C)2005,JPO&NCIPI
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2005169477A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2005169477A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2005169477A3</originalsourceid><addsrcrecordid>eNrjZFD1dQ3x8HdRcPMPUnD29wvx9Av1Dw32iVRwdgwGctwVgkNcXX14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgYGpoZmlibm5ozFRigD7-iP8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CONTINUOUSLY CASTING STEEL</title><source>esp@cenet</source><creator>KATO TORU ; MUTO AKIFUMI</creator><creatorcontrib>KATO TORU ; MUTO AKIFUMI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for continuously casting steel by which the sticking of alumina etc., on the inner surface of an immersion nozzle is reliably prevented and a cast slab having good surface quality can be obtained. SOLUTION: In the method for continuously casting extra-low carbon steel, at least part of the inner surface of the immersion nozzle for supplying the molten steel from a tundish into a mold is constituted of a refractory containing alumina and graphite as the main components. While supplying the electric power from the immersion nozzle into the molten steel stream in the inner part, the continuous casting is performed. The potential difference between the immersion nozzle and the ground is made to be 0.5 to 5.0 V. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><edition>7</edition><language>eng</language><subject>ARTIFICIAL STONE ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; REFRACTORIES ; SLAG ; TRANSPORTING ; TREATMENT OF NATURAL STONE</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050630&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005169477A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050630&amp;DB=EPODOC&amp;CC=JP&amp;NR=2005169477A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KATO TORU</creatorcontrib><creatorcontrib>MUTO AKIFUMI</creatorcontrib><title>METHOD FOR CONTINUOUSLY CASTING STEEL</title><description>PROBLEM TO BE SOLVED: To provide a method for continuously casting steel by which the sticking of alumina etc., on the inner surface of an immersion nozzle is reliably prevented and a cast slab having good surface quality can be obtained. SOLUTION: In the method for continuously casting extra-low carbon steel, at least part of the inner surface of the immersion nozzle for supplying the molten steel from a tundish into a mold is constituted of a refractory containing alumina and graphite as the main components. While supplying the electric power from the immersion nozzle into the molten steel stream in the inner part, the continuous casting is performed. The potential difference between the immersion nozzle and the ground is made to be 0.5 to 5.0 V. COPYRIGHT: (C)2005,JPO&amp;NCIPI</description><subject>ARTIFICIAL STONE</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD1dQ3x8HdRcPMPUnD29wvx9Av1Dw32iVRwdgwGctwVgkNcXX14GFjTEnOKU3mhNDeDkptriLOHbmpBfnxqcUFicmpeakm8V4CRgYGpoZmlibm5ozFRigD7-iP8</recordid><startdate>20050630</startdate><enddate>20050630</enddate><creator>KATO TORU</creator><creator>MUTO AKIFUMI</creator><scope>EVB</scope></search><sort><creationdate>20050630</creationdate><title>METHOD FOR CONTINUOUSLY CASTING STEEL</title><author>KATO TORU ; MUTO AKIFUMI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2005169477A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>ARTIFICIAL STONE</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>KATO TORU</creatorcontrib><creatorcontrib>MUTO AKIFUMI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KATO TORU</au><au>MUTO AKIFUMI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CONTINUOUSLY CASTING STEEL</title><date>2005-06-30</date><risdate>2005</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for continuously casting steel by which the sticking of alumina etc., on the inner surface of an immersion nozzle is reliably prevented and a cast slab having good surface quality can be obtained. SOLUTION: In the method for continuously casting extra-low carbon steel, at least part of the inner surface of the immersion nozzle for supplying the molten steel from a tundish into a mold is constituted of a refractory containing alumina and graphite as the main components. While supplying the electric power from the immersion nozzle into the molten steel stream in the inner part, the continuous casting is performed. The potential difference between the immersion nozzle and the ground is made to be 0.5 to 5.0 V. COPYRIGHT: (C)2005,JPO&amp;NCIPI</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2005169477A
source esp@cenet
subjects ARTIFICIAL STONE
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
REFRACTORIES
SLAG
TRANSPORTING
TREATMENT OF NATURAL STONE
title METHOD FOR CONTINUOUSLY CASTING STEEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T09%3A26%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KATO%20TORU&rft.date=2005-06-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2005169477A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true