METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE
PROBLEM TO BE SOLVED: To provide a metal member forming method, a metal member, and a metal member forming device for achieving the forming property and higher strength of the metal member. SOLUTION: The cylindrical metal member 1 having a hollow chamber 10 and a forming die 3 having a forming die f...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WATANABE HARUO IZEKI HAKUSHIN |
description | PROBLEM TO BE SOLVED: To provide a metal member forming method, a metal member, and a metal member forming device for achieving the forming property and higher strength of the metal member. SOLUTION: The cylindrical metal member 1 having a hollow chamber 10 and a forming die 3 having a forming die face 31 are used. The metal member 1 is heated to a quench-strengthening temperature zone (e.g. A1 transformation temperature or above). By increasing the internal pressure of the gas in the hollow chamber 10 of the heated metal member 1, a wall 1a of the metal member 1 is swollen (plastically deformed), and the swollen wall 1a of the metal member 1 is brought into close contact with the forming die face 31 of the forming die 3 to perform the forming and the quench-strengthening. The wall 1a of the metal member 1 is hardened, and the strength of the metal member 1 is increased thereby. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2003154415A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2003154415A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2003154415A3</originalsourceid><addsrcrecordid>eNrjZPDydQ1x9FHwdfV1cg1ScPMP8vX0cwdyQzz8XXQUkCV1FBz9XBSwKndxDfN0duVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBsaGpiYmhqaOxkQpAgBhni0Y</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE</title><source>esp@cenet</source><creator>WATANABE HARUO ; IZEKI HAKUSHIN</creator><creatorcontrib>WATANABE HARUO ; IZEKI HAKUSHIN</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a metal member forming method, a metal member, and a metal member forming device for achieving the forming property and higher strength of the metal member. SOLUTION: The cylindrical metal member 1 having a hollow chamber 10 and a forming die 3 having a forming die face 31 are used. The metal member 1 is heated to a quench-strengthening temperature zone (e.g. A1 transformation temperature or above). By increasing the internal pressure of the gas in the hollow chamber 10 of the heated metal member 1, a wall 1a of the metal member 1 is swollen (plastically deformed), and the swollen wall 1a of the metal member 1 is brought into close contact with the forming die face 31 of the forming die 3 to perform the forming and the quench-strengthening. The wall 1a of the metal member 1 is hardened, and the strength of the metal member 1 is increased thereby.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING ; WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20030527&DB=EPODOC&CC=JP&NR=2003154415A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25568,76551</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20030527&DB=EPODOC&CC=JP&NR=2003154415A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WATANABE HARUO</creatorcontrib><creatorcontrib>IZEKI HAKUSHIN</creatorcontrib><title>METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE</title><description>PROBLEM TO BE SOLVED: To provide a metal member forming method, a metal member, and a metal member forming device for achieving the forming property and higher strength of the metal member. SOLUTION: The cylindrical metal member 1 having a hollow chamber 10 and a forming die 3 having a forming die face 31 are used. The metal member 1 is heated to a quench-strengthening temperature zone (e.g. A1 transformation temperature or above). By increasing the internal pressure of the gas in the hollow chamber 10 of the heated metal member 1, a wall 1a of the metal member 1 is swollen (plastically deformed), and the swollen wall 1a of the metal member 1 is brought into close contact with the forming die face 31 of the forming die 3 to perform the forming and the quench-strengthening. The wall 1a of the metal member 1 is hardened, and the strength of the metal member 1 is increased thereby.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><subject>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDydQ1x9FHwdfV1cg1ScPMP8vX0cwdyQzz8XXQUkCV1FBz9XBSwKndxDfN0duVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBsaGpiYmhqaOxkQpAgBhni0Y</recordid><startdate>20030527</startdate><enddate>20030527</enddate><creator>WATANABE HARUO</creator><creator>IZEKI HAKUSHIN</creator><scope>EVB</scope></search><sort><creationdate>20030527</creationdate><title>METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE</title><author>WATANABE HARUO ; IZEKI HAKUSHIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2003154415A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><topic>WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WATANABE HARUO</creatorcontrib><creatorcontrib>IZEKI HAKUSHIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WATANABE HARUO</au><au>IZEKI HAKUSHIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE</title><date>2003-05-27</date><risdate>2003</risdate><abstract>PROBLEM TO BE SOLVED: To provide a metal member forming method, a metal member, and a metal member forming device for achieving the forming property and higher strength of the metal member. SOLUTION: The cylindrical metal member 1 having a hollow chamber 10 and a forming die 3 having a forming die face 31 are used. The metal member 1 is heated to a quench-strengthening temperature zone (e.g. A1 transformation temperature or above). By increasing the internal pressure of the gas in the hollow chamber 10 of the heated metal member 1, a wall 1a of the metal member 1 is swollen (plastically deformed), and the swollen wall 1a of the metal member 1 is brought into close contact with the forming die face 31 of the forming die 3 to perform the forming and the quench-strengthening. The wall 1a of the metal member 1 is hardened, and the strength of the metal member 1 is increased thereby.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2003154415A |
source | esp@cenet |
subjects | CHEMISTRY GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS PERFORMING OPERATIONS PUNCHING METAL TRANSPORTING WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS ORPROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL |
title | METAL MEMBER FORMING METHOD, METAL MEMBER, AND METAL MEMBER FORMING DEVICE |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T03%3A32%3A38IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WATANABE%20HARUO&rft.date=2003-05-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2003154415A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |