METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL
PROBLEM TO BE SOLVED: To provide a method for producing an Al-Mg based alloy material which has improved extrudability and forgeability, particularly, in extrudability. SOLUTION: A cast material of an Al-Si based alloy having a composition containing 3 to 18% Si, 1 to 5% Cu and 0.2 to 3% Mg, and fur...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OKUBO YOSHIMASA |
description | PROBLEM TO BE SOLVED: To provide a method for producing an Al-Mg based alloy material which has improved extrudability and forgeability, particularly, in extrudability. SOLUTION: A cast material of an Al-Si based alloy having a composition containing 3 to 18% Si, 1 to 5% Cu and 0.2 to 3% Mg, and further containing one or more kinds selected from |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2002212692A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2002212692A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2002212692A3</originalsourceid><addsrcrecordid>eNrjZND3dQ3x8HdRcPMPUggI8ncJdfb0c1dwzNENzlRwcgx2dVFw9PHxj1TwdQxxDfJ09OFhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBkZGhkZmlkaOxkQpAgBKOyZW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL</title><source>esp@cenet</source><creator>OKUBO YOSHIMASA</creator><creatorcontrib>OKUBO YOSHIMASA</creatorcontrib><description><![CDATA[PROBLEM TO BE SOLVED: To provide a method for producing an Al-Mg based alloy material which has improved extrudability and forgeability, particularly, in extrudability. SOLUTION: A cast material of an Al-Si based alloy having a composition containing 3 to 18% Si, 1 to 5% Cu and 0.2 to 3% Mg, and further containing one or more kinds selected from <0.5% Mn, <0.5% Fe,<0.5% Cr, <0.5% Zr, <=0.1% Ti and <=0.05% B, and the balance Al with impurities is subjected to homogenizing treatment consisting of first heat treatment in which it is held to >450 to <510 deg.C for 2 to <24 hr and second heat treatment in which it is held in the temperature range of 300 to 390 deg.C for 3 to 24 hr.]]></description><edition>7</edition><language>eng</language><subject>ALLOYS ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2002</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20020731&DB=EPODOC&CC=JP&NR=2002212692A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20020731&DB=EPODOC&CC=JP&NR=2002212692A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OKUBO YOSHIMASA</creatorcontrib><title>METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL</title><description><![CDATA[PROBLEM TO BE SOLVED: To provide a method for producing an Al-Mg based alloy material which has improved extrudability and forgeability, particularly, in extrudability. SOLUTION: A cast material of an Al-Si based alloy having a composition containing 3 to 18% Si, 1 to 5% Cu and 0.2 to 3% Mg, and further containing one or more kinds selected from <0.5% Mn, <0.5% Fe,<0.5% Cr, <0.5% Zr, <=0.1% Ti and <=0.05% B, and the balance Al with impurities is subjected to homogenizing treatment consisting of first heat treatment in which it is held to >450 to <510 deg.C for 2 to <24 hr and second heat treatment in which it is held in the temperature range of 300 to 390 deg.C for 3 to 24 hr.]]></description><subject>ALLOYS</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2002</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND3dQ3x8HdRcPMPUggI8ncJdfb0c1dwzNENzlRwcgx2dVFw9PHxj1TwdQxxDfJ09OFhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBkZGhkZmlkaOxkQpAgBKOyZW</recordid><startdate>20020731</startdate><enddate>20020731</enddate><creator>OKUBO YOSHIMASA</creator><scope>EVB</scope></search><sort><creationdate>20020731</creationdate><title>METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL</title><author>OKUBO YOSHIMASA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2002212692A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2002</creationdate><topic>ALLOYS</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>OKUBO YOSHIMASA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OKUBO YOSHIMASA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL</title><date>2002-07-31</date><risdate>2002</risdate><abstract><![CDATA[PROBLEM TO BE SOLVED: To provide a method for producing an Al-Mg based alloy material which has improved extrudability and forgeability, particularly, in extrudability. SOLUTION: A cast material of an Al-Si based alloy having a composition containing 3 to 18% Si, 1 to 5% Cu and 0.2 to 3% Mg, and further containing one or more kinds selected from <0.5% Mn, <0.5% Fe,<0.5% Cr, <0.5% Zr, <=0.1% Ti and <=0.05% B, and the balance Al with impurities is subjected to homogenizing treatment consisting of first heat treatment in which it is held to >450 to <510 deg.C for 2 to <24 hr and second heat treatment in which it is held in the temperature range of 300 to 390 deg.C for 3 to 24 hr.]]></abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2002212692A |
source | esp@cenet |
subjects | ALLOYS CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | METHOD FOR PRODUCING Al-Si BASED ALLOY MATERIAL |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T22%3A00%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OKUBO%20YOSHIMASA&rft.date=2002-07-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2002212692A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |