PRODUCING METHOD FOR POLYESTER
PROBLEM TO BE SOLVED: To produce a polyester, in which bubbles and a fish eye are difficult to be generated in moldings and crystallization controlling properties of the moldings are good and transparency is excellent and also dirt of a mold at time of molding is difficult to be generated. SOLUTION:...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MATSUI YOSHINAO YOSHIDA KOJI YAMAUCHI ITSUKI |
description | PROBLEM TO BE SOLVED: To produce a polyester, in which bubbles and a fish eye are difficult to be generated in moldings and crystallization controlling properties of the moldings are good and transparency is excellent and also dirt of a mold at time of molding is difficult to be generated. SOLUTION: In the method for producing a polyester, in which the polyester obtained by melt polymerization is discharged in a strand shape from a die head, cooled and solidified and thereafter cut into a chip state, the polyester is cut into the chip state in the conditions satisfying formula (1). 0.02 |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2001246622A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2001246622A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2001246622A3</originalsourceid><addsrcrecordid>eNrjZJALCPJ3CXX29HNX8HUN8fB3UXDzD1II8PeJdA0OcQ3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaGRiZmZkZGjsZEKQIAA3Yh5Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCING METHOD FOR POLYESTER</title><source>esp@cenet</source><creator>MATSUI YOSHINAO ; YOSHIDA KOJI ; YAMAUCHI ITSUKI</creator><creatorcontrib>MATSUI YOSHINAO ; YOSHIDA KOJI ; YAMAUCHI ITSUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To produce a polyester, in which bubbles and a fish eye are difficult to be generated in moldings and crystallization controlling properties of the moldings are good and transparency is excellent and also dirt of a mold at time of molding is difficult to be generated. SOLUTION: In the method for producing a polyester, in which the polyester obtained by melt polymerization is discharged in a strand shape from a die head, cooled and solidified and thereafter cut into a chip state, the polyester is cut into the chip state in the conditions satisfying formula (1). 0.02<=(V1/S1)×t1×ΔT<=0.35...(1) Wherein, Tg, Text and T respectively show glass transition temperature ( deg.C) of the polyester, temperature Text ( deg.C) in the case of discharging the polyester from a die head to a strand state and temperature ( deg.C) of cooling water. Further, V1, S1 and T1 respectively show cooling water amount (cm3/sec) per unit time in a process until a strand is cut in the chip state, surface area (cm2/sec) of the strand brought into contact with cooling water and time (sec) in which cooling water is brought into contact with the strand.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; MAKING GRANULES OR PREFORMS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010911&DB=EPODOC&CC=JP&NR=2001246622A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010911&DB=EPODOC&CC=JP&NR=2001246622A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MATSUI YOSHINAO</creatorcontrib><creatorcontrib>YOSHIDA KOJI</creatorcontrib><creatorcontrib>YAMAUCHI ITSUKI</creatorcontrib><title>PRODUCING METHOD FOR POLYESTER</title><description>PROBLEM TO BE SOLVED: To produce a polyester, in which bubbles and a fish eye are difficult to be generated in moldings and crystallization controlling properties of the moldings are good and transparency is excellent and also dirt of a mold at time of molding is difficult to be generated. SOLUTION: In the method for producing a polyester, in which the polyester obtained by melt polymerization is discharged in a strand shape from a die head, cooled and solidified and thereafter cut into a chip state, the polyester is cut into the chip state in the conditions satisfying formula (1). 0.02<=(V1/S1)×t1×ΔT<=0.35...(1) Wherein, Tg, Text and T respectively show glass transition temperature ( deg.C) of the polyester, temperature Text ( deg.C) in the case of discharging the polyester from a die head to a strand state and temperature ( deg.C) of cooling water. Further, V1, S1 and T1 respectively show cooling water amount (cm3/sec) per unit time in a process until a strand is cut in the chip state, surface area (cm2/sec) of the strand brought into contact with cooling water and time (sec) in which cooling water is brought into contact with the strand.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJALCPJ3CXX29HNX8HUN8fB3UXDzD1II8PeJdA0OcQ3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaGRiZmZkZGjsZEKQIAA3Yh5Q</recordid><startdate>20010911</startdate><enddate>20010911</enddate><creator>MATSUI YOSHINAO</creator><creator>YOSHIDA KOJI</creator><creator>YAMAUCHI ITSUKI</creator><scope>EVB</scope></search><sort><creationdate>20010911</creationdate><title>PRODUCING METHOD FOR POLYESTER</title><author>MATSUI YOSHINAO ; YOSHIDA KOJI ; YAMAUCHI ITSUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2001246622A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2001</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>MATSUI YOSHINAO</creatorcontrib><creatorcontrib>YOSHIDA KOJI</creatorcontrib><creatorcontrib>YAMAUCHI ITSUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MATSUI YOSHINAO</au><au>YOSHIDA KOJI</au><au>YAMAUCHI ITSUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCING METHOD FOR POLYESTER</title><date>2001-09-11</date><risdate>2001</risdate><abstract>PROBLEM TO BE SOLVED: To produce a polyester, in which bubbles and a fish eye are difficult to be generated in moldings and crystallization controlling properties of the moldings are good and transparency is excellent and also dirt of a mold at time of molding is difficult to be generated. SOLUTION: In the method for producing a polyester, in which the polyester obtained by melt polymerization is discharged in a strand shape from a die head, cooled and solidified and thereafter cut into a chip state, the polyester is cut into the chip state in the conditions satisfying formula (1). 0.02<=(V1/S1)×t1×ΔT<=0.35...(1) Wherein, Tg, Text and T respectively show glass transition temperature ( deg.C) of the polyester, temperature Text ( deg.C) in the case of discharging the polyester from a die head to a strand state and temperature ( deg.C) of cooling water. Further, V1, S1 and T1 respectively show cooling water amount (cm3/sec) per unit time in a process until a strand is cut in the chip state, surface area (cm2/sec) of the strand brought into contact with cooling water and time (sec) in which cooling water is brought into contact with the strand.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2001246622A |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS MAKING GRANULES OR PREFORMS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PERFORMING OPERATIONS PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS THEIR PREPARATION OR CHEMICAL WORKING-UP TRANSPORTING WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | PRODUCING METHOD FOR POLYESTER |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T04%3A13%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MATSUI%20YOSHINAO&rft.date=2001-09-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2001246622A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |