PAPER CONTAINER
PROBLEM TO BE SOLVED: To prevent cracks from being generated at the time of the box-making, and improve the preservation property for a content by laminating an inorganic oxide membrane layer of a specified film thickness as a barrier layer of a laminated material in such a manner that the inorganic...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | TAKE YOSHIAKI KANO MITSURU |
description | PROBLEM TO BE SOLVED: To prevent cracks from being generated at the time of the box-making, and improve the preservation property for a content by laminating an inorganic oxide membrane layer of a specified film thickness as a barrier layer of a laminated material in such a manner that the inorganic oxide membrane layer may be located at approx. the center of the thickness of the laminated material, in a paper container which is formed into a box shape by bending a blank sheet comprising the laminated material. SOLUTION: This paper container is formed into a box-shape by bending ruled lines 1 of a blank sheet comprising a laminated material 100, wherein paperboards 120 and 170 are used as base materials, and an inorganic oxide membrane layer 140 is made a barrier layer. In such a paper container, the inorganic oxide membrane layer 140 as the barrier layer of the laminated material 100 is laminated in a manner to be located at approx. the center of the thickness of the laminated material 100. For the inorganic oxide membrane layer 140, at least on one surface of a drawn polyethylene terephthalate film layer from among the laminate constituting materials, a silicon oxide or the like is deposit-formed, and the deposited film thickness is 100 to 3,000 . Also, the paper container is formed in such a manner that the inorganic oxide membrane layer 140 at a corner section 12 when the laminated material 100 is bent at an approx. right angle on the ruled line, may be bent inward at an obtuse angle. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2001031073A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2001031073A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2001031073A3</originalsourceid><addsrcrecordid>eNrjZOAPcAxwDVJw9vcLcfT0cw3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaGBsaGBubGjsZEKQIAGb8dhw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PAPER CONTAINER</title><source>esp@cenet</source><creator>TAKE YOSHIAKI ; KANO MITSURU</creator><creatorcontrib>TAKE YOSHIAKI ; KANO MITSURU</creatorcontrib><description>PROBLEM TO BE SOLVED: To prevent cracks from being generated at the time of the box-making, and improve the preservation property for a content by laminating an inorganic oxide membrane layer of a specified film thickness as a barrier layer of a laminated material in such a manner that the inorganic oxide membrane layer may be located at approx. the center of the thickness of the laminated material, in a paper container which is formed into a box shape by bending a blank sheet comprising the laminated material. SOLUTION: This paper container is formed into a box-shape by bending ruled lines 1 of a blank sheet comprising a laminated material 100, wherein paperboards 120 and 170 are used as base materials, and an inorganic oxide membrane layer 140 is made a barrier layer. In such a paper container, the inorganic oxide membrane layer 140 as the barrier layer of the laminated material 100 is laminated in a manner to be located at approx. the center of the thickness of the laminated material 100. For the inorganic oxide membrane layer 140, at least on one surface of a drawn polyethylene terephthalate film layer from among the laminate constituting materials, a silicon oxide or the like is deposit-formed, and the deposited film thickness is 100 to 3,000 . Also, the paper container is formed in such a manner that the inorganic oxide membrane layer 140 at a corner section 12 when the laminated material 100 is bent at an approx. right angle on the ruled line, may be bent inward at an obtuse angle.</description><edition>7</edition><language>eng</language><subject>ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR ; CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS,e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES,DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS ; CONVEYING ; HANDLING THIN OR FILAMENTARY MATERIAL ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; PACKAGES ; PACKAGING ELEMENTS ; PACKING ; PERFORMING OPERATIONS ; STORING ; TRANSPORTING</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010206&DB=EPODOC&CC=JP&NR=2001031073A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010206&DB=EPODOC&CC=JP&NR=2001031073A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKE YOSHIAKI</creatorcontrib><creatorcontrib>KANO MITSURU</creatorcontrib><title>PAPER CONTAINER</title><description>PROBLEM TO BE SOLVED: To prevent cracks from being generated at the time of the box-making, and improve the preservation property for a content by laminating an inorganic oxide membrane layer of a specified film thickness as a barrier layer of a laminated material in such a manner that the inorganic oxide membrane layer may be located at approx. the center of the thickness of the laminated material, in a paper container which is formed into a box shape by bending a blank sheet comprising the laminated material. SOLUTION: This paper container is formed into a box-shape by bending ruled lines 1 of a blank sheet comprising a laminated material 100, wherein paperboards 120 and 170 are used as base materials, and an inorganic oxide membrane layer 140 is made a barrier layer. In such a paper container, the inorganic oxide membrane layer 140 as the barrier layer of the laminated material 100 is laminated in a manner to be located at approx. the center of the thickness of the laminated material 100. For the inorganic oxide membrane layer 140, at least on one surface of a drawn polyethylene terephthalate film layer from among the laminate constituting materials, a silicon oxide or the like is deposit-formed, and the deposited film thickness is 100 to 3,000 . Also, the paper container is formed in such a manner that the inorganic oxide membrane layer 140 at a corner section 12 when the laminated material 100 is bent at an approx. right angle on the ruled line, may be bent inward at an obtuse angle.</description><subject>ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR</subject><subject>CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS,e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES,DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS</subject><subject>CONVEYING</subject><subject>HANDLING THIN OR FILAMENTARY MATERIAL</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>PACKAGES</subject><subject>PACKAGING ELEMENTS</subject><subject>PACKING</subject><subject>PERFORMING OPERATIONS</subject><subject>STORING</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOAPcAxwDVJw9vcLcfT0cw3iYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaGBsaGBubGjsZEKQIAGb8dhw</recordid><startdate>20010206</startdate><enddate>20010206</enddate><creator>TAKE YOSHIAKI</creator><creator>KANO MITSURU</creator><scope>EVB</scope></search><sort><creationdate>20010206</creationdate><title>PAPER CONTAINER</title><author>TAKE YOSHIAKI ; KANO MITSURU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2001031073A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2001</creationdate><topic>ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR</topic><topic>CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS,e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES,DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS</topic><topic>CONVEYING</topic><topic>HANDLING THIN OR FILAMENTARY MATERIAL</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>PACKAGES</topic><topic>PACKAGING ELEMENTS</topic><topic>PACKING</topic><topic>PERFORMING OPERATIONS</topic><topic>STORING</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKE YOSHIAKI</creatorcontrib><creatorcontrib>KANO MITSURU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKE YOSHIAKI</au><au>KANO MITSURU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PAPER CONTAINER</title><date>2001-02-06</date><risdate>2001</risdate><abstract>PROBLEM TO BE SOLVED: To prevent cracks from being generated at the time of the box-making, and improve the preservation property for a content by laminating an inorganic oxide membrane layer of a specified film thickness as a barrier layer of a laminated material in such a manner that the inorganic oxide membrane layer may be located at approx. the center of the thickness of the laminated material, in a paper container which is formed into a box shape by bending a blank sheet comprising the laminated material. SOLUTION: This paper container is formed into a box-shape by bending ruled lines 1 of a blank sheet comprising a laminated material 100, wherein paperboards 120 and 170 are used as base materials, and an inorganic oxide membrane layer 140 is made a barrier layer. In such a paper container, the inorganic oxide membrane layer 140 as the barrier layer of the laminated material 100 is laminated in a manner to be located at approx. the center of the thickness of the laminated material 100. For the inorganic oxide membrane layer 140, at least on one surface of a drawn polyethylene terephthalate film layer from among the laminate constituting materials, a silicon oxide or the like is deposit-formed, and the deposited film thickness is 100 to 3,000 . Also, the paper container is formed in such a manner that the inorganic oxide membrane layer 140 at a corner section 12 when the laminated material 100 is bent at an approx. right angle on the ruled line, may be bent inward at an obtuse angle.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2001031073A |
source | esp@cenet |
subjects | ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS,e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES,DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS CONVEYING HANDLING THIN OR FILAMENTARY MATERIAL LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM PACKAGES PACKAGING ELEMENTS PACKING PERFORMING OPERATIONS STORING TRANSPORTING |
title | PAPER CONTAINER |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T07%3A17%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKE%20YOSHIAKI&rft.date=2001-02-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2001031073A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |