SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME

PROBLEM TO BE SOLVED: To use a large filling amount of sodium salt of a solidified body and make it insoluble in water by adding the compound of elements selected from alkali earth metal, transition metal, metalloid or the like to a vitrification base material, and forming to heat and melt them. SOL...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: INOBE MITSUYOSHI, MIYAKE TAKASHI, KAWASE YOSHIKATSU, MATSUBARA RYUICHI, SHIOJI NORIO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator INOBE MITSUYOSHI
MIYAKE TAKASHI
KAWASE YOSHIKATSU
MATSUBARA RYUICHI
SHIOJI NORIO
description PROBLEM TO BE SOLVED: To use a large filling amount of sodium salt of a solidified body and make it insoluble in water by adding the compound of elements selected from alkali earth metal, transition metal, metalloid or the like to a vitrification base material, and forming to heat and melt them. SOLUTION: In a preprocessing process, radioactive waste liquid containing sodium compound is dried to become powder, and in a storing process, the powder is stored in a storage tank. In a first mixing process, the dried powder is weighed to supply the powder of SiO2 so as to be mixed at a constant rate. In a second mixing process, about 2-22 mol.% of one oxide out of CaO, B2O3, Al2O3, Fe2O3, TiO2 or the like is added to the mixed powder, and sodium oxide in a vitrified and solidified body is made about 26-35 wt.% to be mixed and agitated. In a heating melting process, the heating and melting temperature of a furnace is set at 850-1100 deg.C, and a mixture is put into a crucible to be heated or continuously heated in a cylindrical furnace. In a cooling and solidifying process, it is preferably forcedly cooled at about 500-600 deg.C by furnace outside air cooling, fan air cooling, water cooling or the like.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2001027694A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2001027694A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2001027694A3</originalsourceid><addsrcrecordid>eNrjZAgJ9vfxdPF083R1UXDyd4lU8HdTCHJ08fR3dA7xDHNVcPb3c3H1CwbKhjsGh7gqBIc6BYc4-jm7Kjj6uSj4OvqFugFVhga5gjSGeAAVOPq68jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDQwMjczNLE0djohQBAGl_MEA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME</title><source>esp@cenet</source><creator>INOBE MITSUYOSHI ; MIYAKE TAKASHI ; KAWASE YOSHIKATSU ; MATSUBARA RYUICHI ; SHIOJI NORIO</creator><creatorcontrib>INOBE MITSUYOSHI ; MIYAKE TAKASHI ; KAWASE YOSHIKATSU ; MATSUBARA RYUICHI ; SHIOJI NORIO</creatorcontrib><description>PROBLEM TO BE SOLVED: To use a large filling amount of sodium salt of a solidified body and make it insoluble in water by adding the compound of elements selected from alkali earth metal, transition metal, metalloid or the like to a vitrification base material, and forming to heat and melt them. SOLUTION: In a preprocessing process, radioactive waste liquid containing sodium compound is dried to become powder, and in a storing process, the powder is stored in a storage tank. In a first mixing process, the dried powder is weighed to supply the powder of SiO2 so as to be mixed at a constant rate. In a second mixing process, about 2-22 mol.% of one oxide out of CaO, B2O3, Al2O3, Fe2O3, TiO2 or the like is added to the mixed powder, and sodium oxide in a vitrified and solidified body is made about 26-35 wt.% to be mixed and agitated. In a heating melting process, the heating and melting temperature of a furnace is set at 850-1100 deg.C, and a mixture is put into a crucible to be heated or continuously heated in a cylindrical furnace. In a cooling and solidifying process, it is preferably forcedly cooled at about 500-600 deg.C by furnace outside air cooling, fan air cooling, water cooling or the like.</description><edition>7</edition><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; DECONTAMINATION ARRANGEMENTS THEREFOR ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; NUCLEAR ENGINEERING ; NUCLEAR PHYSICS ; PHYSICS ; PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULARRADIATION OR PARTICLE BOMBARDMENT ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS ; TREATING RADIOACTIVELY CONTAMINATED MATERIAL</subject><creationdate>2001</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010130&amp;DB=EPODOC&amp;CC=JP&amp;NR=2001027694A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20010130&amp;DB=EPODOC&amp;CC=JP&amp;NR=2001027694A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>INOBE MITSUYOSHI</creatorcontrib><creatorcontrib>MIYAKE TAKASHI</creatorcontrib><creatorcontrib>KAWASE YOSHIKATSU</creatorcontrib><creatorcontrib>MATSUBARA RYUICHI</creatorcontrib><creatorcontrib>SHIOJI NORIO</creatorcontrib><title>SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME</title><description>PROBLEM TO BE SOLVED: To use a large filling amount of sodium salt of a solidified body and make it insoluble in water by adding the compound of elements selected from alkali earth metal, transition metal, metalloid or the like to a vitrification base material, and forming to heat and melt them. SOLUTION: In a preprocessing process, radioactive waste liquid containing sodium compound is dried to become powder, and in a storing process, the powder is stored in a storage tank. In a first mixing process, the dried powder is weighed to supply the powder of SiO2 so as to be mixed at a constant rate. In a second mixing process, about 2-22 mol.% of one oxide out of CaO, B2O3, Al2O3, Fe2O3, TiO2 or the like is added to the mixed powder, and sodium oxide in a vitrified and solidified body is made about 26-35 wt.% to be mixed and agitated. In a heating melting process, the heating and melting temperature of a furnace is set at 850-1100 deg.C, and a mixture is put into a crucible to be heated or continuously heated in a cylindrical furnace. In a cooling and solidifying process, it is preferably forcedly cooled at about 500-600 deg.C by furnace outside air cooling, fan air cooling, water cooling or the like.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>DECONTAMINATION ARRANGEMENTS THEREFOR</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>NUCLEAR ENGINEERING</subject><subject>NUCLEAR PHYSICS</subject><subject>PHYSICS</subject><subject>PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULARRADIATION OR PARTICLE BOMBARDMENT</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><subject>TREATING RADIOACTIVELY CONTAMINATED MATERIAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2001</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAgJ9vfxdPF083R1UXDyd4lU8HdTCHJ08fR3dA7xDHNVcPb3c3H1CwbKhjsGh7gqBIc6BYc4-jm7Kjj6uSj4OvqFugFVhga5gjSGeAAVOPq68jCwpiXmFKfyQmluBiU31xBnD93Ugvz41OKCxOTUvNSSeK8AIwMDQwMjczNLE0djohQBAGl_MEA</recordid><startdate>20010130</startdate><enddate>20010130</enddate><creator>INOBE MITSUYOSHI</creator><creator>MIYAKE TAKASHI</creator><creator>KAWASE YOSHIKATSU</creator><creator>MATSUBARA RYUICHI</creator><creator>SHIOJI NORIO</creator><scope>EVB</scope></search><sort><creationdate>20010130</creationdate><title>SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME</title><author>INOBE MITSUYOSHI ; MIYAKE TAKASHI ; KAWASE YOSHIKATSU ; MATSUBARA RYUICHI ; SHIOJI NORIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2001027694A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2001</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>DECONTAMINATION ARRANGEMENTS THEREFOR</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>NUCLEAR ENGINEERING</topic><topic>NUCLEAR PHYSICS</topic><topic>PHYSICS</topic><topic>PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULARRADIATION OR PARTICLE BOMBARDMENT</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><topic>TREATING RADIOACTIVELY CONTAMINATED MATERIAL</topic><toplevel>online_resources</toplevel><creatorcontrib>INOBE MITSUYOSHI</creatorcontrib><creatorcontrib>MIYAKE TAKASHI</creatorcontrib><creatorcontrib>KAWASE YOSHIKATSU</creatorcontrib><creatorcontrib>MATSUBARA RYUICHI</creatorcontrib><creatorcontrib>SHIOJI NORIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>INOBE MITSUYOSHI</au><au>MIYAKE TAKASHI</au><au>KAWASE YOSHIKATSU</au><au>MATSUBARA RYUICHI</au><au>SHIOJI NORIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME</title><date>2001-01-30</date><risdate>2001</risdate><abstract>PROBLEM TO BE SOLVED: To use a large filling amount of sodium salt of a solidified body and make it insoluble in water by adding the compound of elements selected from alkali earth metal, transition metal, metalloid or the like to a vitrification base material, and forming to heat and melt them. SOLUTION: In a preprocessing process, radioactive waste liquid containing sodium compound is dried to become powder, and in a storing process, the powder is stored in a storage tank. In a first mixing process, the dried powder is weighed to supply the powder of SiO2 so as to be mixed at a constant rate. In a second mixing process, about 2-22 mol.% of one oxide out of CaO, B2O3, Al2O3, Fe2O3, TiO2 or the like is added to the mixed powder, and sodium oxide in a vitrified and solidified body is made about 26-35 wt.% to be mixed and agitated. In a heating melting process, the heating and melting temperature of a furnace is set at 850-1100 deg.C, and a mixture is put into a crucible to be heated or continuously heated in a cylindrical furnace. In a cooling and solidifying process, it is preferably forcedly cooled at about 500-600 deg.C by furnace outside air cooling, fan air cooling, water cooling or the like.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2001027694A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
DECONTAMINATION ARRANGEMENTS THEREFOR
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
NUCLEAR ENGINEERING
NUCLEAR PHYSICS
PHYSICS
PROTECTION AGAINST X-RADIATION, GAMMA RADIATION, CORPUSCULARRADIATION OR PARTICLE BOMBARDMENT
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
TREATING RADIOACTIVELY CONTAMINATED MATERIAL
title SOLIDIFIED BODY OF RADIOACTIVE CONDENSED WASTE SUBSTANCE AND MANUFACTURE OF THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T13%3A36%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=INOBE%20MITSUYOSHI&rft.date=2001-01-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2001027694A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true