SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME

PROBLEM TO BE SOLVED: To improve the working characteristics of the slab by controlling the maxi mum value of the crystal grain size in the depth equal from the surface of the cast slab to the one equal to or below the specified times of the average crystal grain size in the depth. SOLUTION: The max...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUSUNOKI SHINTARO, MOROHOSHI TAKASHI, SEZE AKIFUMI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUSUNOKI SHINTARO
MOROHOSHI TAKASHI
SEZE AKIFUMI
description PROBLEM TO BE SOLVED: To improve the working characteristics of the slab by controlling the maxi mum value of the crystal grain size in the depth equal from the surface of the cast slab to the one equal to or below the specified times of the average crystal grain size in the depth. SOLUTION: The maximum value of the crystal grain size is controlled to the one equal to or below the three times the average crystal grain size in the depth thereof, where >=60% of the cross-section in the thickness direction of the slab can be formed of equi-axed crystals. Moreover, the whole cross section in the thickness direction of the slab can be formed of crystal grains composed of equi-axed crystals. The slab may be incorporated with the oxide of Mg formed by adding Mg or an Mg alloy to molten steel. The slab, in which the maximum value of the crystal grain size in the depth equal from the surface has been controlled to the one equal to or below the three times the average crystal grain size in the depth, is heated at 1100 to 1350 deg.C and is thereafter subjected to working such as rolling. Since the slab having a structure of uniform crystal grains is used in this way, the cracking resistance at the time of working such as rolling is high, and (r) value expressing drawing characteristics, or the like, can be improved.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2000328173A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2000328173A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2000328173A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAQANAsDqL-w-FeiM2g6yU9TTQmkhzUTqVInEQL9f9xEWent7y5iNmjBroa8p4CgwvQxnRy4QDGYkLDlFxmZwBDA5mJPETN6AI1oLtfZkuQ8UxLMbsPj6msvi7Eek9sbFXGV1-mcbiVZ3n3x0stpVT1brNVqP5KH318Lt4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME</title><source>esp@cenet</source><creator>KUSUNOKI SHINTARO ; MOROHOSHI TAKASHI ; SEZE AKIFUMI</creator><creatorcontrib>KUSUNOKI SHINTARO ; MOROHOSHI TAKASHI ; SEZE AKIFUMI</creatorcontrib><description>PROBLEM TO BE SOLVED: To improve the working characteristics of the slab by controlling the maxi mum value of the crystal grain size in the depth equal from the surface of the cast slab to the one equal to or below the specified times of the average crystal grain size in the depth. SOLUTION: The maximum value of the crystal grain size is controlled to the one equal to or below the three times the average crystal grain size in the depth thereof, where &gt;=60% of the cross-section in the thickness direction of the slab can be formed of equi-axed crystals. Moreover, the whole cross section in the thickness direction of the slab can be formed of crystal grains composed of equi-axed crystals. The slab may be incorporated with the oxide of Mg formed by adding Mg or an Mg alloy to molten steel. The slab, in which the maximum value of the crystal grain size in the depth equal from the surface has been controlled to the one equal to or below the three times the average crystal grain size in the depth, is heated at 1100 to 1350 deg.C and is thereafter subjected to working such as rolling. Since the slab having a structure of uniform crystal grains is used in this way, the cracking resistance at the time of working such as rolling is high, and (r) value expressing drawing characteristics, or the like, can be improved.</description><edition>7</edition><language>eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2000</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20001128&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000328173A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20001128&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000328173A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUSUNOKI SHINTARO</creatorcontrib><creatorcontrib>MOROHOSHI TAKASHI</creatorcontrib><creatorcontrib>SEZE AKIFUMI</creatorcontrib><title>SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME</title><description>PROBLEM TO BE SOLVED: To improve the working characteristics of the slab by controlling the maxi mum value of the crystal grain size in the depth equal from the surface of the cast slab to the one equal to or below the specified times of the average crystal grain size in the depth. SOLUTION: The maximum value of the crystal grain size is controlled to the one equal to or below the three times the average crystal grain size in the depth thereof, where &gt;=60% of the cross-section in the thickness direction of the slab can be formed of equi-axed crystals. Moreover, the whole cross section in the thickness direction of the slab can be formed of crystal grains composed of equi-axed crystals. The slab may be incorporated with the oxide of Mg formed by adding Mg or an Mg alloy to molten steel. The slab, in which the maximum value of the crystal grain size in the depth equal from the surface has been controlled to the one equal to or below the three times the average crystal grain size in the depth, is heated at 1100 to 1350 deg.C and is thereafter subjected to working such as rolling. Since the slab having a structure of uniform crystal grains is used in this way, the cracking resistance at the time of working such as rolling is high, and (r) value expressing drawing characteristics, or the like, can be improved.</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2000</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQANAsDqL-w-FeiM2g6yU9TTQmkhzUTqVInEQL9f9xEWent7y5iNmjBroa8p4CgwvQxnRy4QDGYkLDlFxmZwBDA5mJPETN6AI1oLtfZkuQ8UxLMbsPj6msvi7Eek9sbFXGV1-mcbiVZ3n3x0stpVT1brNVqP5KH318Lt4</recordid><startdate>20001128</startdate><enddate>20001128</enddate><creator>KUSUNOKI SHINTARO</creator><creator>MOROHOSHI TAKASHI</creator><creator>SEZE AKIFUMI</creator><scope>EVB</scope></search><sort><creationdate>20001128</creationdate><title>SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME</title><author>KUSUNOKI SHINTARO ; MOROHOSHI TAKASHI ; SEZE AKIFUMI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2000328173A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2000</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KUSUNOKI SHINTARO</creatorcontrib><creatorcontrib>MOROHOSHI TAKASHI</creatorcontrib><creatorcontrib>SEZE AKIFUMI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUSUNOKI SHINTARO</au><au>MOROHOSHI TAKASHI</au><au>SEZE AKIFUMI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME</title><date>2000-11-28</date><risdate>2000</risdate><abstract>PROBLEM TO BE SOLVED: To improve the working characteristics of the slab by controlling the maxi mum value of the crystal grain size in the depth equal from the surface of the cast slab to the one equal to or below the specified times of the average crystal grain size in the depth. SOLUTION: The maximum value of the crystal grain size is controlled to the one equal to or below the three times the average crystal grain size in the depth thereof, where &gt;=60% of the cross-section in the thickness direction of the slab can be formed of equi-axed crystals. Moreover, the whole cross section in the thickness direction of the slab can be formed of crystal grains composed of equi-axed crystals. The slab may be incorporated with the oxide of Mg formed by adding Mg or an Mg alloy to molten steel. The slab, in which the maximum value of the crystal grain size in the depth equal from the surface has been controlled to the one equal to or below the three times the average crystal grain size in the depth, is heated at 1100 to 1350 deg.C and is thereafter subjected to working such as rolling. Since the slab having a structure of uniform crystal grains is used in this way, the cracking resistance at the time of working such as rolling is high, and (r) value expressing drawing characteristics, or the like, can be improved.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2000328173A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title SLAB EXCELLENT IN WORKING CHARACTERISTIC AND STEEL OBTAINED BY WORKING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T11%3A41%3A47IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUSUNOKI%20SHINTARO&rft.date=2000-11-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2000328173A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true