RESIN COMPOSITION

PROBLEM TO BE SOLVED: To prepare a resin composition where the variation in surface electric resistance is stably controlled so as to exist in a specific range by including a specific poly(ether/aromatic ketone) and specific carbon fibers in a specific content ratio. SOLUTION: This resin composition...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SATO TAKASHI, YANAGIHARA KAYAKO, YOSHIMURA MASAJI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SATO TAKASHI
YANAGIHARA KAYAKO
YOSHIMURA MASAJI
description PROBLEM TO BE SOLVED: To prepare a resin composition where the variation in surface electric resistance is stably controlled so as to exist in a specific range by including a specific poly(ether/aromatic ketone) and specific carbon fibers in a specific content ratio. SOLUTION: This resin composition is prepared by including (A) 90-60 wt.% poly(ether/aromatic ketone) having repeating units of the formula and (B) 10-40 wt.% carbon fibers subjected to electric resistance augmentation treatment, and having 3-25 μm average fiber diameter and 50-70,000 μm average fiber length. When the resin composition is molded into a molded article, the variation in the surface electric resistance of the molded article preferably is controlled stably so as to exist between 106 Ω and 1012 Ω. The ingredient B preferably has 10-2 Ω-103 Ω volume resistivity value, which enables trouble due to short circuit to be prevented, enables the adhesion of dust or the like in use to sufficiently be controlled and enables the resin composition to be widely used in the field where antistaticity is required.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2000191901A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2000191901A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2000191901A3</originalsourceid><addsrcrecordid>eNrjZBAMcg329FNw9vcN8A_2DPH09-NhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBgaGloaWBoaOxkQpAgBn5R5P</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>RESIN COMPOSITION</title><source>esp@cenet</source><creator>SATO TAKASHI ; YANAGIHARA KAYAKO ; YOSHIMURA MASAJI</creator><creatorcontrib>SATO TAKASHI ; YANAGIHARA KAYAKO ; YOSHIMURA MASAJI</creatorcontrib><description>PROBLEM TO BE SOLVED: To prepare a resin composition where the variation in surface electric resistance is stably controlled so as to exist in a specific range by including a specific poly(ether/aromatic ketone) and specific carbon fibers in a specific content ratio. SOLUTION: This resin composition is prepared by including (A) 90-60 wt.% poly(ether/aromatic ketone) having repeating units of the formula and (B) 10-40 wt.% carbon fibers subjected to electric resistance augmentation treatment, and having 3-25 μm average fiber diameter and 50-70,000 μm average fiber length. When the resin composition is molded into a molded article, the variation in the surface electric resistance of the molded article preferably is controlled stably so as to exist between 106 Ω and 1012 Ω. The ingredient B preferably has 10-2 Ω-103 Ω volume resistivity value, which enables trouble due to short circuit to be prevented, enables the adhesion of dust or the like in use to sufficiently be controlled and enables the resin composition to be widely used in the field where antistaticity is required.</description><edition>7</edition><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; METALLURGY ; MILLING ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2000</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20000711&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000191901A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20000711&amp;DB=EPODOC&amp;CC=JP&amp;NR=2000191901A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SATO TAKASHI</creatorcontrib><creatorcontrib>YANAGIHARA KAYAKO</creatorcontrib><creatorcontrib>YOSHIMURA MASAJI</creatorcontrib><title>RESIN COMPOSITION</title><description>PROBLEM TO BE SOLVED: To prepare a resin composition where the variation in surface electric resistance is stably controlled so as to exist in a specific range by including a specific poly(ether/aromatic ketone) and specific carbon fibers in a specific content ratio. SOLUTION: This resin composition is prepared by including (A) 90-60 wt.% poly(ether/aromatic ketone) having repeating units of the formula and (B) 10-40 wt.% carbon fibers subjected to electric resistance augmentation treatment, and having 3-25 μm average fiber diameter and 50-70,000 μm average fiber length. When the resin composition is molded into a molded article, the variation in the surface electric resistance of the molded article preferably is controlled stably so as to exist between 106 Ω and 1012 Ω. The ingredient B preferably has 10-2 Ω-103 Ω volume resistivity value, which enables trouble due to short circuit to be prevented, enables the adhesion of dust or the like in use to sufficiently be controlled and enables the resin composition to be widely used in the field where antistaticity is required.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>METALLURGY</subject><subject>MILLING</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2000</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBAMcg329FNw9vcN8A_2DPH09-NhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBgaGloaWBoaOxkQpAgBn5R5P</recordid><startdate>20000711</startdate><enddate>20000711</enddate><creator>SATO TAKASHI</creator><creator>YANAGIHARA KAYAKO</creator><creator>YOSHIMURA MASAJI</creator><scope>EVB</scope></search><sort><creationdate>20000711</creationdate><title>RESIN COMPOSITION</title><author>SATO TAKASHI ; YANAGIHARA KAYAKO ; YOSHIMURA MASAJI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2000191901A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2000</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>METALLURGY</topic><topic>MILLING</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>SATO TAKASHI</creatorcontrib><creatorcontrib>YANAGIHARA KAYAKO</creatorcontrib><creatorcontrib>YOSHIMURA MASAJI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SATO TAKASHI</au><au>YANAGIHARA KAYAKO</au><au>YOSHIMURA MASAJI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>RESIN COMPOSITION</title><date>2000-07-11</date><risdate>2000</risdate><abstract>PROBLEM TO BE SOLVED: To prepare a resin composition where the variation in surface electric resistance is stably controlled so as to exist in a specific range by including a specific poly(ether/aromatic ketone) and specific carbon fibers in a specific content ratio. SOLUTION: This resin composition is prepared by including (A) 90-60 wt.% poly(ether/aromatic ketone) having repeating units of the formula and (B) 10-40 wt.% carbon fibers subjected to electric resistance augmentation treatment, and having 3-25 μm average fiber diameter and 50-70,000 μm average fiber length. When the resin composition is molded into a molded article, the variation in the surface electric resistance of the molded article preferably is controlled stably so as to exist between 106 Ω and 1012 Ω. The ingredient B preferably has 10-2 Ω-103 Ω volume resistivity value, which enables trouble due to short circuit to be prevented, enables the adhesion of dust or the like in use to sufficiently be controlled and enables the resin composition to be widely used in the field where antistaticity is required.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2000191901A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
METALLURGY
MILLING
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title RESIN COMPOSITION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T21%3A58%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SATO%20TAKASHI&rft.date=2000-07-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2000191901A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true