Continuous casting of light alloy
In the continuous casting of a light alloy, the melt is poured into the mould at 10-150 deg.C above the liquidus temp. of the alloy and subjected to ultrasound of intensity 2-60 W/sq.cm., distributed throughout the cross-section of the melt in the mould by an ultrasonic source immersed to a depth of...