PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE
A method of manufacturing spherical alumina comprising preparing a basic aluminum chloride solution having an aluminum concentration in the range of from 7 wt.% to 12 wt.% and a weight ratio of aluminum to chloride in the range of from 0.3 to 0.8 by reacting gibbsite with an aqueous hydrochloric aci...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | ita |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MASARU TATSUSHIMA TOSHIO HASHIMOTO SHIZUO TAKUMI |
description | A method of manufacturing spherical alumina comprising preparing a basic aluminum chloride solution having an aluminum concentration in the range of from 7 wt.% to 12 wt.% and a weight ratio of aluminum to chloride in the range of from 0.3 to 0.8 by reacting gibbsite with an aqueous hydrochloric acid solution at an elevated temperature, preparing an alumina hydrosol having an aluminum concentration in the range of from 9 wt.% to 15 wt.% and a weight ratio of aluminum to chloride in the range of from 0.8 to 1.5 by reacting the thus prepared solution with metallic aluminum at an elevated temperature, commingling this hydrosol with a gelling agent, dispersing the resulting mixture in the form of droplets in a suspending medium thereby to form hydrogel particles, ageing the thus obtained particles in said suspending medium and then an aqueous ammonia, washing with water, drying and calcining. The thus obtained spherical alumina is substantially free from sodium in spite of employing gibbsite as raw material. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_IT1121490B</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>IT1121490B</sourcerecordid><originalsourceid>FETCH-epo_espacenet_IT1121490B3</originalsourceid><addsrcrecordid>eNrjZLAPCPJ3dnXx9HX1C_FXCHANUgAKuIQGBbkqOPr4hPp6-jkqBLu5Bvl7ujj6uCoACR8FT5cgxyB3Tx8fzxBXHgbWtMSc4lReKM3NIO_mGuLsoZtakB-fWlyQmJyal1oS7xliaGhkaGJp4GRMWAUA-7ApzQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE</title><source>esp@cenet</source><creator>MASARU TATSUSHIMA ; TOSHIO HASHIMOTO ; SHIZUO TAKUMI</creator><creatorcontrib>MASARU TATSUSHIMA ; TOSHIO HASHIMOTO ; SHIZUO TAKUMI</creatorcontrib><description>A method of manufacturing spherical alumina comprising preparing a basic aluminum chloride solution having an aluminum concentration in the range of from 7 wt.% to 12 wt.% and a weight ratio of aluminum to chloride in the range of from 0.3 to 0.8 by reacting gibbsite with an aqueous hydrochloric acid solution at an elevated temperature, preparing an alumina hydrosol having an aluminum concentration in the range of from 9 wt.% to 15 wt.% and a weight ratio of aluminum to chloride in the range of from 0.8 to 1.5 by reacting the thus prepared solution with metallic aluminum at an elevated temperature, commingling this hydrosol with a gelling agent, dispersing the resulting mixture in the form of droplets in a suspending medium thereby to form hydrogel particles, ageing the thus obtained particles in said suspending medium and then an aqueous ammonia, washing with water, drying and calcining. The thus obtained spherical alumina is substantially free from sodium in spite of employing gibbsite as raw material.</description><edition>4</edition><language>ita</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; CONCRETE ; INORGANIC CHEMISTRY ; LIME, MAGNESIA ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; REFRACTORIES ; SLAG ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF NATURAL STONE</subject><creationdate>1986</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19860402&DB=EPODOC&CC=IT&NR=1121490B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19860402&DB=EPODOC&CC=IT&NR=1121490B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MASARU TATSUSHIMA</creatorcontrib><creatorcontrib>TOSHIO HASHIMOTO</creatorcontrib><creatorcontrib>SHIZUO TAKUMI</creatorcontrib><title>PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE</title><description>A method of manufacturing spherical alumina comprising preparing a basic aluminum chloride solution having an aluminum concentration in the range of from 7 wt.% to 12 wt.% and a weight ratio of aluminum to chloride in the range of from 0.3 to 0.8 by reacting gibbsite with an aqueous hydrochloric acid solution at an elevated temperature, preparing an alumina hydrosol having an aluminum concentration in the range of from 9 wt.% to 15 wt.% and a weight ratio of aluminum to chloride in the range of from 0.8 to 1.5 by reacting the thus prepared solution with metallic aluminum at an elevated temperature, commingling this hydrosol with a gelling agent, dispersing the resulting mixture in the form of droplets in a suspending medium thereby to form hydrogel particles, ageing the thus obtained particles in said suspending medium and then an aqueous ammonia, washing with water, drying and calcining. The thus obtained spherical alumina is substantially free from sodium in spite of employing gibbsite as raw material.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>CONCRETE</subject><subject>INORGANIC CHEMISTRY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1986</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAPCPJ3dnXx9HX1C_FXCHANUgAKuIQGBbkqOPr4hPp6-jkqBLu5Bvl7ujj6uCoACR8FT5cgxyB3Tx8fzxBXHgbWtMSc4lReKM3NIO_mGuLsoZtakB-fWlyQmJyal1oS7xliaGhkaGJp4GRMWAUA-7ApzQ</recordid><startdate>19860402</startdate><enddate>19860402</enddate><creator>MASARU TATSUSHIMA</creator><creator>TOSHIO HASHIMOTO</creator><creator>SHIZUO TAKUMI</creator><scope>EVB</scope></search><sort><creationdate>19860402</creationdate><title>PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE</title><author>MASARU TATSUSHIMA ; TOSHIO HASHIMOTO ; SHIZUO TAKUMI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_IT1121490B3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ita</language><creationdate>1986</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>CONCRETE</topic><topic>INORGANIC CHEMISTRY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>MASARU TATSUSHIMA</creatorcontrib><creatorcontrib>TOSHIO HASHIMOTO</creatorcontrib><creatorcontrib>SHIZUO TAKUMI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MASARU TATSUSHIMA</au><au>TOSHIO HASHIMOTO</au><au>SHIZUO TAKUMI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE</title><date>1986-04-02</date><risdate>1986</risdate><abstract>A method of manufacturing spherical alumina comprising preparing a basic aluminum chloride solution having an aluminum concentration in the range of from 7 wt.% to 12 wt.% and a weight ratio of aluminum to chloride in the range of from 0.3 to 0.8 by reacting gibbsite with an aqueous hydrochloric acid solution at an elevated temperature, preparing an alumina hydrosol having an aluminum concentration in the range of from 9 wt.% to 15 wt.% and a weight ratio of aluminum to chloride in the range of from 0.8 to 1.5 by reacting the thus prepared solution with metallic aluminum at an elevated temperature, commingling this hydrosol with a gelling agent, dispersing the resulting mixture in the form of droplets in a suspending medium thereby to form hydrogel particles, ageing the thus obtained particles in said suspending medium and then an aqueous ammonia, washing with water, drying and calcining. The thus obtained spherical alumina is substantially free from sodium in spite of employing gibbsite as raw material.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | ita |
recordid | cdi_epo_espacenet_IT1121490B |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS CONCRETE INORGANIC CHEMISTRY LIME, MAGNESIA METALLURGY PERFORMING OPERATIONS PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL REFRACTORIES SLAG THEIR RELEVANT APPARATUS TRANSPORTING TREATMENT OF NATURAL STONE |
title | PROCEDIMENTO PER PRODURRE ALLUMINA SFEROIDALE DALL IDRARGILLITE |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-19T18%3A12%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MASARU%20TATSUSHIMA&rft.date=1986-04-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EIT1121490B%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |