METHOD FOR PROCESSING BAUXITES

A method for processing bauxites according to the Bayer technology, with an increased yield in Al2O3 and with decreased caustic soda losses, starting particularly from goethite bauxites of boehmite and/or diaspore type and carrying out the digestion at 180 DEG C to 300 DEG C using an aluminate liquo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: VAROS I, SIKLOSI P, OZVALD Z, TOTH P, SIGMOND G, PINTER T, BUJDOSO E, SOLYMAR K, FEHER I, ZAMBO J, LENGYEL L, ORBAN M, WENTZELY K, LAZAR F, MATYASI J, FERENCZI T
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator VAROS I
SIKLOSI P
OZVALD Z
TOTH P
SIGMOND G
PINTER T
BUJDOSO E
SOLYMAR K
FEHER I
ZAMBO J
LENGYEL L
ORBAN M
WENTZELY K
LAZAR F
MATYASI J
FERENCZI T
description A method for processing bauxites according to the Bayer technology, with an increased yield in Al2O3 and with decreased caustic soda losses, starting particularly from goethite bauxites of boehmite and/or diaspore type and carrying out the digestion at 180 DEG C to 300 DEG C using an aluminate liquor containing Na2Ocaustic in a concentration of 80 to 300 g./l. The digestion is carried out in the presence of a calcium compound in an amount corresponding to 2 to 6 % of CaO calculated for the dry weight of bauxite and of a sulfate salt in an amount corresponding to 1.0 to 7.0 g./l. of sulfate ion concentration, whereby the goethite content of the bauxite is converted into hematite. The process provides advantageous conditions for the complete dissolution of the boehmite and diaspore content of bauxite in the vicinity of the equilibrium molar ratio, and enables to recover efficiently the caustic soda losses in the Bayer process itself, requiring no supplementary operation.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_IN139499B</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>IN139499B</sourcerecordid><originalsourceid>FETCH-epo_espacenet_IN139499B3</originalsourceid><addsrcrecordid>eNrjZJDzdQ3x8HdRcPMPUggI8nd2DQ729HNXcHIMjfAMcQ3mYWBNS8wpTuWF0twMcm6uIc4euqkF-fGpxQWJyal5qSXxnn6GxpYmlpZOxgQVAAABkCBd</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PROCESSING BAUXITES</title><source>esp@cenet</source><creator>VAROS I ; SIKLOSI P ; OZVALD Z ; TOTH P ; SIGMOND G ; PINTER T ; BUJDOSO E ; SOLYMAR K ; FEHER I ; ZAMBO J ; LENGYEL L ; ORBAN M ; WENTZELY K ; LAZAR F ; MATYASI J ; FERENCZI T</creator><creatorcontrib>VAROS I ; SIKLOSI P ; OZVALD Z ; TOTH P ; SIGMOND G ; PINTER T ; BUJDOSO E ; SOLYMAR K ; FEHER I ; ZAMBO J ; LENGYEL L ; ORBAN M ; WENTZELY K ; LAZAR F ; MATYASI J ; FERENCZI T</creatorcontrib><description>A method for processing bauxites according to the Bayer technology, with an increased yield in Al2O3 and with decreased caustic soda losses, starting particularly from goethite bauxites of boehmite and/or diaspore type and carrying out the digestion at 180 DEG C to 300 DEG C using an aluminate liquor containing Na2Ocaustic in a concentration of 80 to 300 g./l. The digestion is carried out in the presence of a calcium compound in an amount corresponding to 2 to 6 % of CaO calculated for the dry weight of bauxite and of a sulfate salt in an amount corresponding to 1.0 to 7.0 g./l. of sulfate ion concentration, whereby the goethite content of the bauxite is converted into hematite. The process provides advantageous conditions for the complete dissolution of the boehmite and diaspore content of bauxite in the vicinity of the equilibrium molar ratio, and enables to recover efficiently the caustic soda losses in the Bayer process itself, requiring no supplementary operation.</description><edition>2</edition><language>eng</language><subject>CHEMISTRY ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>1976</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19760626&amp;DB=EPODOC&amp;CC=IN&amp;NR=139499B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19760626&amp;DB=EPODOC&amp;CC=IN&amp;NR=139499B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>VAROS I</creatorcontrib><creatorcontrib>SIKLOSI P</creatorcontrib><creatorcontrib>OZVALD Z</creatorcontrib><creatorcontrib>TOTH P</creatorcontrib><creatorcontrib>SIGMOND G</creatorcontrib><creatorcontrib>PINTER T</creatorcontrib><creatorcontrib>BUJDOSO E</creatorcontrib><creatorcontrib>SOLYMAR K</creatorcontrib><creatorcontrib>FEHER I</creatorcontrib><creatorcontrib>ZAMBO J</creatorcontrib><creatorcontrib>LENGYEL L</creatorcontrib><creatorcontrib>ORBAN M</creatorcontrib><creatorcontrib>WENTZELY K</creatorcontrib><creatorcontrib>LAZAR F</creatorcontrib><creatorcontrib>MATYASI J</creatorcontrib><creatorcontrib>FERENCZI T</creatorcontrib><title>METHOD FOR PROCESSING BAUXITES</title><description>A method for processing bauxites according to the Bayer technology, with an increased yield in Al2O3 and with decreased caustic soda losses, starting particularly from goethite bauxites of boehmite and/or diaspore type and carrying out the digestion at 180 DEG C to 300 DEG C using an aluminate liquor containing Na2Ocaustic in a concentration of 80 to 300 g./l. The digestion is carried out in the presence of a calcium compound in an amount corresponding to 2 to 6 % of CaO calculated for the dry weight of bauxite and of a sulfate salt in an amount corresponding to 1.0 to 7.0 g./l. of sulfate ion concentration, whereby the goethite content of the bauxite is converted into hematite. The process provides advantageous conditions for the complete dissolution of the boehmite and diaspore content of bauxite in the vicinity of the equilibrium molar ratio, and enables to recover efficiently the caustic soda losses in the Bayer process itself, requiring no supplementary operation.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1976</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJDzdQ3x8HdRcPMPUggI8nd2DQ729HNXcHIMjfAMcQ3mYWBNS8wpTuWF0twMcm6uIc4euqkF-fGpxQWJyal5qSXxnn6GxpYmlpZOxgQVAAABkCBd</recordid><startdate>19760626</startdate><enddate>19760626</enddate><creator>VAROS I</creator><creator>SIKLOSI P</creator><creator>OZVALD Z</creator><creator>TOTH P</creator><creator>SIGMOND G</creator><creator>PINTER T</creator><creator>BUJDOSO E</creator><creator>SOLYMAR K</creator><creator>FEHER I</creator><creator>ZAMBO J</creator><creator>LENGYEL L</creator><creator>ORBAN M</creator><creator>WENTZELY K</creator><creator>LAZAR F</creator><creator>MATYASI J</creator><creator>FERENCZI T</creator><scope>EVB</scope></search><sort><creationdate>19760626</creationdate><title>METHOD FOR PROCESSING BAUXITES</title><author>VAROS I ; SIKLOSI P ; OZVALD Z ; TOTH P ; SIGMOND G ; PINTER T ; BUJDOSO E ; SOLYMAR K ; FEHER I ; ZAMBO J ; LENGYEL L ; ORBAN M ; WENTZELY K ; LAZAR F ; MATYASI J ; FERENCZI T</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_IN139499B3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1976</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>VAROS I</creatorcontrib><creatorcontrib>SIKLOSI P</creatorcontrib><creatorcontrib>OZVALD Z</creatorcontrib><creatorcontrib>TOTH P</creatorcontrib><creatorcontrib>SIGMOND G</creatorcontrib><creatorcontrib>PINTER T</creatorcontrib><creatorcontrib>BUJDOSO E</creatorcontrib><creatorcontrib>SOLYMAR K</creatorcontrib><creatorcontrib>FEHER I</creatorcontrib><creatorcontrib>ZAMBO J</creatorcontrib><creatorcontrib>LENGYEL L</creatorcontrib><creatorcontrib>ORBAN M</creatorcontrib><creatorcontrib>WENTZELY K</creatorcontrib><creatorcontrib>LAZAR F</creatorcontrib><creatorcontrib>MATYASI J</creatorcontrib><creatorcontrib>FERENCZI T</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>VAROS I</au><au>SIKLOSI P</au><au>OZVALD Z</au><au>TOTH P</au><au>SIGMOND G</au><au>PINTER T</au><au>BUJDOSO E</au><au>SOLYMAR K</au><au>FEHER I</au><au>ZAMBO J</au><au>LENGYEL L</au><au>ORBAN M</au><au>WENTZELY K</au><au>LAZAR F</au><au>MATYASI J</au><au>FERENCZI T</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PROCESSING BAUXITES</title><date>1976-06-26</date><risdate>1976</risdate><abstract>A method for processing bauxites according to the Bayer technology, with an increased yield in Al2O3 and with decreased caustic soda losses, starting particularly from goethite bauxites of boehmite and/or diaspore type and carrying out the digestion at 180 DEG C to 300 DEG C using an aluminate liquor containing Na2Ocaustic in a concentration of 80 to 300 g./l. The digestion is carried out in the presence of a calcium compound in an amount corresponding to 2 to 6 % of CaO calculated for the dry weight of bauxite and of a sulfate salt in an amount corresponding to 1.0 to 7.0 g./l. of sulfate ion concentration, whereby the goethite content of the bauxite is converted into hematite. The process provides advantageous conditions for the complete dissolution of the boehmite and diaspore content of bauxite in the vicinity of the equilibrium molar ratio, and enables to recover efficiently the caustic soda losses in the Bayer process itself, requiring no supplementary operation.</abstract><edition>2</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_IN139499B
source esp@cenet
subjects CHEMISTRY
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
METALLURGY
title METHOD FOR PROCESSING BAUXITES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T14%3A55%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=VAROS%20I&rft.date=1976-06-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EIN139499B%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true