SEAMLESS STEEL PIPE FOR HOLLOW SPRING

A seamless steel pipe for a hollow spring includes C: 0.2 to 0.7 mass%, Si: 0.5 to 3 mass%, Mn: 0.1 to 2 mass%, Cr: 3 mass% or less (excluding 0 mass%), Al: 0.1 mass% or less (excluding 0 mass%), P: 0.02 mass% or less (excluding 0 mass%), S: 0.02 mass% or less (excluding 0 mass%) and N: 0.02 mass% o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAMURA, Eiichi, HATANO, Hitoshi, TOYOTAKE, Kotaro, KOCHI, Takuya
Format: Patent
Sprache:eng ; hun
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAMURA, Eiichi
HATANO, Hitoshi
TOYOTAKE, Kotaro
KOCHI, Takuya
description A seamless steel pipe for a hollow spring includes C: 0.2 to 0.7 mass%, Si: 0.5 to 3 mass%, Mn: 0.1 to 2 mass%, Cr: 3 mass% or less (excluding 0 mass%), Al: 0.1 mass% or less (excluding 0 mass%), P: 0.02 mass% or less (excluding 0 mass%), S: 0.02 mass% or less (excluding 0 mass%) and N: 0.02 mass% or less (excluding 0 mass%). A residual austenite content in an inner surface layer part of the steel pipe is 5 vol.% or less. An average grain size of a ferrite-pearlite structure in the inner surface layer part of the steel pipe is 18µm or less. A number density of a carbide having a circle equivalent diameter of 500 nm or more and being present in the inner surface layer part of the steel pipe is 1.8×10 -2 particles/µm 2 or less.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_HUE036303TT2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>HUE036303TT2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_HUE036303TT23</originalsourceid><addsrcrecordid>eNrjZFANdnX09XENDlYIDnF19VEI8AxwVXDzD1Lw8Pfx8Q9XCA4I8vRz52FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8R6hrgbGZsYGxiEhRsbEqAEArRMj1Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SEAMLESS STEEL PIPE FOR HOLLOW SPRING</title><source>esp@cenet</source><creator>TAMURA, Eiichi ; HATANO, Hitoshi ; TOYOTAKE, Kotaro ; KOCHI, Takuya</creator><creatorcontrib>TAMURA, Eiichi ; HATANO, Hitoshi ; TOYOTAKE, Kotaro ; KOCHI, Takuya</creatorcontrib><description>A seamless steel pipe for a hollow spring includes C: 0.2 to 0.7 mass%, Si: 0.5 to 3 mass%, Mn: 0.1 to 2 mass%, Cr: 3 mass% or less (excluding 0 mass%), Al: 0.1 mass% or less (excluding 0 mass%), P: 0.02 mass% or less (excluding 0 mass%), S: 0.02 mass% or less (excluding 0 mass%) and N: 0.02 mass% or less (excluding 0 mass%). A residual austenite content in an inner surface layer part of the steel pipe is 5 vol.% or less. An average grain size of a ferrite-pearlite structure in the inner surface layer part of the steel pipe is 18µm or less. A number density of a carbide having a circle equivalent diameter of 500 nm or more and being present in the inner surface layer part of the steel pipe is 1.8×10 -2 particles/µm 2 or less.</description><language>eng ; hun</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION ; TECHNICAL SUBJECTS COVERED BY FORMER USPC ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180628&amp;DB=EPODOC&amp;CC=HU&amp;NR=E036303T2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180628&amp;DB=EPODOC&amp;CC=HU&amp;NR=E036303T2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAMURA, Eiichi</creatorcontrib><creatorcontrib>HATANO, Hitoshi</creatorcontrib><creatorcontrib>TOYOTAKE, Kotaro</creatorcontrib><creatorcontrib>KOCHI, Takuya</creatorcontrib><title>SEAMLESS STEEL PIPE FOR HOLLOW SPRING</title><description>A seamless steel pipe for a hollow spring includes C: 0.2 to 0.7 mass%, Si: 0.5 to 3 mass%, Mn: 0.1 to 2 mass%, Cr: 3 mass% or less (excluding 0 mass%), Al: 0.1 mass% or less (excluding 0 mass%), P: 0.02 mass% or less (excluding 0 mass%), S: 0.02 mass% or less (excluding 0 mass%) and N: 0.02 mass% or less (excluding 0 mass%). A residual austenite content in an inner surface layer part of the steel pipe is 5 vol.% or less. An average grain size of a ferrite-pearlite structure in the inner surface layer part of the steel pipe is 18µm or less. A number density of a carbide having a circle equivalent diameter of 500 nm or more and being present in the inner surface layer part of the steel pipe is 1.8×10 -2 particles/µm 2 or less.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFANdnX09XENDlYIDnF19VEI8AxwVXDzD1Lw8Pfx8Q9XCA4I8vRz52FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8R6hrgbGZsYGxiEhRsbEqAEArRMj1Q</recordid><startdate>20180628</startdate><enddate>20180628</enddate><creator>TAMURA, Eiichi</creator><creator>HATANO, Hitoshi</creator><creator>TOYOTAKE, Kotaro</creator><creator>KOCHI, Takuya</creator><scope>EVB</scope></search><sort><creationdate>20180628</creationdate><title>SEAMLESS STEEL PIPE FOR HOLLOW SPRING</title><author>TAMURA, Eiichi ; HATANO, Hitoshi ; TOYOTAKE, Kotaro ; KOCHI, Takuya</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_HUE036303TT23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; hun</language><creationdate>2018</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>TAMURA, Eiichi</creatorcontrib><creatorcontrib>HATANO, Hitoshi</creatorcontrib><creatorcontrib>TOYOTAKE, Kotaro</creatorcontrib><creatorcontrib>KOCHI, Takuya</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAMURA, Eiichi</au><au>HATANO, Hitoshi</au><au>TOYOTAKE, Kotaro</au><au>KOCHI, Takuya</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SEAMLESS STEEL PIPE FOR HOLLOW SPRING</title><date>2018-06-28</date><risdate>2018</risdate><abstract>A seamless steel pipe for a hollow spring includes C: 0.2 to 0.7 mass%, Si: 0.5 to 3 mass%, Mn: 0.1 to 2 mass%, Cr: 3 mass% or less (excluding 0 mass%), Al: 0.1 mass% or less (excluding 0 mass%), P: 0.02 mass% or less (excluding 0 mass%), S: 0.02 mass% or less (excluding 0 mass%) and N: 0.02 mass% or less (excluding 0 mass%). A residual austenite content in an inner surface layer part of the steel pipe is 5 vol.% or less. An average grain size of a ferrite-pearlite structure in the inner surface layer part of the steel pipe is 18µm or less. A number density of a carbide having a circle equivalent diameter of 500 nm or more and being present in the inner surface layer part of the steel pipe is 1.8×10 -2 particles/µm 2 or less.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; hun
recordid cdi_epo_espacenet_HUE036303TT2
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
TECHNICAL SUBJECTS COVERED BY FORMER USPC
TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title SEAMLESS STEEL PIPE FOR HOLLOW SPRING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T14%3A07%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAMURA,%20Eiichi&rft.date=2018-06-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EHUE036303TT2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true