Improvements in or relating to polysulphides
A polysulphide is prepared by reacting a solution of a primary, secondary or tertiary amine free from hetero atoms other than nitrogen or an alkaloid with sulphur at a pressure of 3-60 atmospheres and a temperature of 100-300 DEG C. The reaction may be carried out in the presence of barium sulphide,...